Topics
|
|
|
We.4.5.1
|
INSTRUMENTS, TOOLS AND METHODS TO CHECK RAILS IN THEIR TRACK FOR DEFECTS ALONG THE SURFACE AND IMMEDIATELY BELOW IT
Junger, M., Rohmann, Frankenthal
(Germany)
Radde, P., Rohmann, Frankenthal
(Germany)
|
without manuscript
|
|
We.4.5.2
|
FAAST:FAST AUTOMATED ANGLE SCAN TECHNIQUE
Coperet, P., Socomate International, Crecy La Chapelle (France)
|
Manuscript
|
|
We.4.5.3
|
Advantage of a combined Ultrasonic and Eddy Current Examination for Railway Inspection Trains
Thomas, H.-M., BAM Berlin
(Germany)
Heckel, T., BAM Berlin
(Germany)
Hanspach, G., Berlin
(Germany)
|
Manuscript
|
|
We.4.5.4
|
GUIDED WAVE ULTRASONIC FLAW DETECTION IN RAILS. APPLICATION EXPERIENCE
Samokrutov, A.A., Association "Spektr-Group", Moscow (Russia) Shevaldykin, V.G., Association "Spektr-Group", Moscow (Russia) Gurvich, A.K., PGUPS, St. Petersburg (Russia)
|
Manuscript
|
|
Th.1.4.1
|
APPLICATION OF NEW FRONT-END ELECTRONICS FOR NON-DESTRUCTIVE TESTING OF RAILROAD WHEEL SETS
Kappes, W., Fraunhofer IZfP, Saarbrücken
(Germany)
Bähr, W., Fraunhofer IZFP, Saarbrücken
(Germany)
Kröning, M., Fraunhofer IZFP, Saarbrücken
(Germany)
Rockstroh, B., Fraunhofer IZFP, Saarbrücken
(Germany)
Rodner, C., Fraunhofer IZFP, Saarbrücken
(Germany)
Goetz, J., Fraunhofer Technologie-Entwicklungsgruppe, Stuttgart
(Germany)
Nemec, D., Fraunhofer Technologie-Entwicklungsgruppe, Stuttgart
(Germany)
|
Manuscript
|
|
Th.1.4.2
|
Non-destructive evaluation of residual stresses in railway solid wheels by non-contact EMAT probe
Gori, M., CESI, S.p.A., Milano (Italy)
|
Manuscript
|
|
Th.1.4.3
|
IMPACT ON RELIABILITY AND PRODUCTIVITY OF WHEEL SET INSPECTION BY ADVANCED AUTOMATED NDE SYSTEMS
Engl, G., intelligeNDT Systems & Services, Erlangen
(Germany)
Oelschlägel, T., DB Brandenburg
(Germany)
Hintze, H., Deutsche Bahn, Brandenburg-Kirchmöser
(Germany)
Meier, R., intelligeNDT Systems & Services, Erlangen
(Germany)
Ritter, J., intelligeNDT Systems & Services, Erlangen
(Germany)
|
without manuscript
|
|
Th.1.4.4
|
NDT Of Railwelds During The Construction Of The Rapid Transportation System in Kaohsiung
Chen, P.-K., China Steel Corporation, Kaohsiung (Taiwan)
|
Manuscript
|
|
Th.4.5.1
|
Railroad Ballast Fouling Detection Using Ground Penetrating Radar – A New Approach Based on Scattering from Voids
Rudy, J., Geophysical Survey Systems, North Salem (USA) Roberts, R., Geophysical Survey Systems, North Salem (USA) Boyle, J., Sperry Rail Service, Danbury, CT (USA) Al-Qadi, I., University of Illinois at Urbana-Champaign, Urbana, IL (USA) Tutumluer, E., University of Illinois at Urbana-Champaign, Urbana, IL (USA)
|
Manuscript
|
|
Th.4.5.2
|
ADVANCES IN ON-TRAIN INSPECTION OF HIGH-SPEED TRAIN WHEELS BY THE NEW GENERATION OF UFPE SYSTEMS
Engl, G., intelligeNDT Systems & Services, Erlangen
(Germany)
Ettlich, R., Deutsche Bahn, Brandenburg-Kirchmöser
(Germany)
Hintze, H., Deutsche Bahn, Brandenburg-Kirchmöser
(Germany)
Rückelt, B., intelligeNDT Systems & Services, Erlangen
(Germany)
Zeilinger, R., intelligeNDT Systems & Services, Erlangen
(Germany)
|
without manuscript
|
|
Th.4.5.3
|
New ultrasound testing systems for the production testing of rail wheels
Rockstroh, B., Fraunhofer IZFP, Saarbrücken
(Germany)
Dath, R., Bochumer Verein Verkehrstechnik, Bochum
(Germany)
Bessert, S., Fraunhofer IZFP, Saarbrücken
(Germany)
Kappes, W., Fraunhofer IZfP, Saarbrücken
(Germany)
Kröning, M., Fraunhofer IZFP, Saarbrücken
(Germany)
Schäfer, W., Fraunhofer IZfP, Saarbrücken
(Germany)
Walte, F., Fraunhofer IZFP, Saarbrücken
(Germany)
Minich, F., Fraunhofer Technologie-Entwicklungsgruppe, Stuttgart
(Germany)
Motnacher, J., Fraunhofer Technologie-Entwicklungsgruppe, Stuttgart
(Germany)
Kamardin, V., Nizhnij Tagil Kombinat NTMK (Russia) Kushnarev, A., Nizhnij Tagil Kombinat NTMK (Russia) Üblacker, B., Radsatzfabrik Ilsenburg GmbH , Ilsenburg
(Germany)
Smorodinski, Y., Russian Academy of Sciences, Ekaterinenburg (Russia)
|
Manuscript
|
|
Th.4.5.4
|
ANALYSIS AND REVIEW OF NDT INSTRUMENTS USED FOR RAILS INSPECTION AT RUSSIAN RAILWAY ROADS
Gordely, V.I., Scientific-industrial enterprise "VIGOR", Moscow (Russia)
|
Manuscript
|
|
Fr.1.3.1
|
Automatic in service train axle inspection systems
Garcia Ares, E., INTERLAB IEC, Madrid (Spain) Buitrago Carrillo, A., INTERLAB IEC, Madrid (Spain) Crespo Giménez, N., INTERLAB IEC, Madrid (Spain) Fernández Plaza, J.A., INTERLAB IEC, Madrid (Spain) Garcia Alonso, J.L., INTERLAB IEC, Madrid (Spain) Ramírez Cervigón, M.A., Renfe Integria (Spain) Sánchez Aznar, F., Renfe Integria (Spain)
|
Manuscript
|
|
Fr.1.3.2
|
INVESTIGATION OF INSPECTION PERFORMANCE ON CRACKED RAILWAY AXLES
Rudlin, J., TWI, Cambridge (United Kingdom) Muhammed, A., TWI, Cambridge (United Kingdom) Schneider, C., TWI, Cambridge (United Kingdom)
|
Manuscript
|
|
Fr.1.3.3
|
Phased array rotation scanner probe system for ultrasonic testing of sleeve shafts
Boehm, R., BAM Berlin
(Germany)
Spruch, W., Büro f. Techn. Diagnostik, Brandenburg-Plaue
(Germany)
|
Manuscript
|
|
Fr.1.3.4
|
Numerical Modelling of Ultrasonic NDT of a Wheel Shaft of a ICE Train
Marklein, R., Universität Kassel
(Germany)
Plankert, W., DB AG FTZ, Brandenburg
(Germany)
Hintze, H., Deutsche Bahn, Brandenburg-Kirchmöser
(Germany)
Chinta, P.K., Universität Kassel
(Germany)
|
Manuscript
|
|
P178
|
A new eddy current instrument in a rail grinding train
Pohl, R., BAM Berlin
(Germany)
Krull, R., Deutsche Bahn, Brandenburg-Kirchmöser
(Germany)
Meierhofer, R., SPENO International SA (Switzerland)
|
Manuscript
|
|
P179
|
HOW TO PROVIDE HIGHER RELIABILITY OF VEHICLES AT THE SLOVENIAN RAILWAYS BY MEANS OF NON-DESTRUCTIVE METHODS
Jemec, V., High school Domzale (Slovenia) Grum, J., SSNDT, University of Ljubljana (Slovenia)
|
Manuscript
|
|