Up: Bond strength measurement in
Previous: Conclusion
References
- 1
- C. V. Cagle, Handbook of adhesive bonding (McGraw Hill,
New York, 1972), pp 421-430.
- 2
- Claus, R.O. and Kline, R.A., Adhesive bondline interrogation
using Stoneley wave methods, J. Appl. Phys. 50 (1979) 8066-8069.
- 3
- Cielo, P., Thermoelastic testing of stratified materials,
International Advances in Nondestructive Testing 11 (1985)
175-217.
- 4
- Bar-Cohen, Y. and Chimenti, D.E., NDE of composite
laminates by leaky lamb waves, Review of Progress in Quantitative NDE
5B (1985) 1199-1206.
- 5
- Rokhlin, S.I., Wang, W., Wang, Y.J. and Hamill, J.L., NDE
of adhesive bonds and bondlines track, Proceedings of the 1989 ASNT Fall
Conference (1989) 41-50.
- 6
- Rokhlin, S.I. and Marom, D., Study of adhesive bonds using
low-frequency obliquely incident ultrasonic waves, J. Acoust. Soc. Am.
80 (1986) 585-590.
- 7
- Nagy, P.B. and Adler, L., Adhesive joint characterization by
leaky guided interface waves, Rev. of Prog. in QNDE 8B (1989)
1417-1424.
- 8
- Pilarski, A., Rose, J.L. and Balasabramaniam, K., On a
plate/surface wave mode selection criteria for ultrasonic evaluation in layered
structures, J. Acoust. Soc. Am. 82 (1987) S21.
- 9
- Singher, L., Segal, Y., Segal, E. and Shamir, J.,
Considerations in bond strength evaluation by ultrasonic guided waves,
J. Acoust. Soc. Am 96 (1994) 2497-2505.
- 10
- Truell, R., Elbaum, C. and Chick, B.B., Ultrasonic
methods in solid state physics (Academic Press, 1969) 9.
- 11
- Singher L., Segal Y. and Shamir J., ``The Interaction of a
Guided Wave with a Non-uniform Adhesion Bond,'' Ultrasonics (1997).
- 12
- Singher L., Segal Y., Segal E. and Shamir J., ``Bond
Strength Measurements by Ultrasonic Guided Waves,'' Ultrasonics (1997).
- 13
- Meeker, T.R. and Meitzler, A.H., Guided wave propagation in
elongated cylinders and plates in: Physical Acoustics, Vol 1A (Ed Mason,
W.P., Academic Press 1964) 111-167.
- 14
- Viktorov, I.A., Rayleigh and Lamb waves (Plenum
Press, New York, 1967).
© Copyright 1. March 1997 Rolf Diederichs, info@ndt.net