Scanning Modes at the Application of
Ultrasonic Phased Array Inspection Systems
H. Wüstenberg, A. Erhard, G. Schenk
Corresponding Author Contact:
Email: Hermann.Wuestenberg@bam.de, Web: http://www.bam.de/g3_viii.html
1. INTRODUCTION
The first applications of phased array probes in NDT tried to imitate the successful medical ultrasonic diagnostic with phased array scanning systems. But due to the many differences between medical diagnostic and industrial applications the phased array concept had to be modified for NDT concerning the probes, the electronic equipment and the software [5 to 14]. Nowadays there are available some manufacturers of NDT phased array equipments and probes. But the application of phased arrays in NDT is also linked to different modes of there use and the corresponding software. A simple takeover e.g. of sector scans and parallel scans from the medical field satisfies only a small number of NDT problems. There are - instead of this - various other scanning modes currently applied [5, 6, 7, 13, 14]. A successful application of phased arrays in NDT requires the intelligent selection of the different soundfield parameters e.g. beam orientation and position, focusing and coupling curvature correction. This includes also the question of the theoretical modelling for the steering parameters as there are: the delay times and amplifications for each element related to the angle and acoustical focusing, the different amplitude correction factors for the distance (DAC or DGS) and the angle and focusing dependent sensitivity variations. The following chapters are describing some of the essentials concerning the software architecture needed for the operation of a phased array system and in connection with that the different scanning modes which up to now have been applied by BAM during 15 years of experience with phased array applications [1, 2, 3, 4].
2. SOUNDBEAM STEERING POSSIBILITIES WITH LINEAR PHASED ARRAYS
The basic possibilities of phased arrays are summarized with the help of Fig. 1,2 and 3. A phased array system is based on a probe divided into small single elements, used as transmitters and/or receivers of ultrasonic waves [1, 12]. The division of a radiating surface in single elements which can be exited with different delay times and sensitivities allows an electronic soundfield steering offering the 3 basic possibilities of Fig.1:
Fig 1: Sound Beam Steering by Phased Array Probes
|
Fig 2: Variation of the Incidence (a) or the Skewing (Y) Angle by Linear Arrays
|
- One can move a beam along the line of a linear array which is the parallel scan of the medical diagnostic.
- More important for NDT is the sector scanning using shear- or longitudinal waves, depending on the angle of incidence and possibly also on wedge angles as demonstrated in Fig. 2.
- A more or less curved distribution of the delaytimes produces a focusing which can also be used to compensate the influence of curved coupling surfaces.
Fig. 2 demonstrates the basic possibilities of wedge equipped probes with a linear phased array [4].
- The angle can be changed only within the plane of incidence,
- One may produce mainly skewing angle variations within the plane perpendicular to the plane of incidence
- By a combining probe type with a rotated linear phased array system one produces skewing- and incidence angle variations.
The typical possibilities of such arrangements are demonstrated in the diagram below in Fig. 2, where the different type of functions describing the dependency of the angle of incidence from the skewing angle are demonstrated. Those probe arrangements have been the basis for a lot of experiences collected during the last years at the BAM together with other industrial partners like Krautkrämer, the German forgemaster VSG and Siemens.
Fig. 3 compares two basic approaches of phased array applications. Instead of using matrix arrays for a 2D steering of the beam one can also use multiple linear array probes with several linear arrays in one probe housing. The decision for such a concept is backed by the better adaptability to the practical circumstances . The arrangement of typical modules within one probe housing is demonstrated in Fig. 3 left-hand side. There is an obvious advantage of smaller number of cables needed for such probes instead of probes with different kinds of mosaic or ring segment arrays. One typical drawback of linear arrays consists in their limitation to 1D focusing. For the second dimension a suitably choosen cylindrical lense is needed, but this is for most of the practical applications not a real restriction /20/.

Fig 3: The Concept of Multiple Phased Array Probes
for the Application of the Phased Array Technique
|
3. SOFTWARE MODULES FOR PHASED ARRAY APPLICATIONS
There are five different areas of software packages which are needed for the planning, the execution and the evaluation phase of a phased array application. Those are:

Fig 4: Top View of a RPV Dome
|

Fig 5: The Spherical Bottom of Boiling Water Reactors
|
Fig 6: Emergency Cooling Inlet Nozzle (inclined)
|
Fig 7: Shear Wave Directivity Pattern in the Plane of Incidence
|
Fig 7a: Modelling the Directivity Patterns of
Linear Phased Array Probes
|
Fig 8: Schematic Arrangement of a Phased Array Equipment
|
- Software to calculate the angles of incidence and skewing, the needed focussing and the distances between probe and defect area and their typical variations along the probe scanning path based on.the geometry datas of an object, e.g. the coupling surface curvatures, the wallthicknesses etc. This is a job for suitable CAD packages. Application examples are the inner nozzle corner inspection and the inspection of the dome or spherical bottom of nuclear reactor pressure vessels /6/. Fig. 4, 5 and 6 are demonstrating the importance of such geometrical calculations. Fig. 4 shows the closure head of a pressurized water reactor with the control rod tube field. An inspection across this field needs steadely changed ultrasonic beam parameters for the skewing- and the incidence angle. The diagram on the left-hand side of this figure shows the distribution of skewing- and incidence angle values which one has to produce during the movement of a probe along one scanning line within the field of the control rod tubes. Those dependencies can easily be realized by the probe system of type b in Fig. 2. A similar situation exists for the spherical bottom of a boiling water reactor, demonstrated in Fig. 5. A much more difficult problem with a complicated geometry is demonstrated in Fig. 6 representing the inclined inlet nozzle for an emergency cooling line emerging into the primary circuit of a pressurized water reactor. The contact technique requires a curvature adapted probe which can only be moved along a scanning line remaining orientated in parallel related to the axis of the main tube. The CAD program has to calculate for each probe position the needed incidence and skewing angles and also the required sound pathes.
- Software to generate the exitation distributions for the elements of an array in
order to generate the different sound field parameters like beam focusing, beam orientation and index point position. Those exitation patterns are essentially defined by the specific delay time and amplification distributions for each element for the transmitting and for the reception case. The character of those patterns can strongly influence the side or grating lobes of the resulting beam e.g. by an amplitude apodizing or by stochastic fluctuations of the delay times. There are basically two ways for the determination of the exitation patterns: One can use an iterative procedure based on a theoretical soundfield modelling and try to check an assumed exitation pattern with the model. For that purpose we are using a software module which calculates the directivity pattern of pulse exited ultrasonic linear arrays in different distances. The inverse problem, that means to input the required beam parameters and to produce at the output the corresponding exitation patterns, can not be solved generally. However, we have derived a set of approximative analytical formula for the probes of Fig.2 with delay pathes or wedges allowing the direct calculation of the delay time distribution- and amplification values for a given case, e.g. with a desired angle of incidence, a desired focusing distance or curvature compensation for both wave modes. /15 to 21/
Those analytical formula are fast enough to be used even during the scanning procedure at pulse repetion rates close to 2 kHz. This may avoid the creation of look up tables for the steering of the phased array equipment during the planning phase of an inspection.
The sound field calculation program calculates the directivity patterns shown in Fig. 7 where different angles of incidence have been realized by a shear wave probe of 3.7 MHz. The grating lopes can be recognized, they are in a good agreement with the grating lopes observed during the practical applications. Fig. 7a shows the case of an array for applications on concrete, an extreme case where we can easely change the gap between the different elements and study its importance. Fig. 7a shows the strong influence of the gap extension for the grating lope amplitude.
Those analytical formula are fast enough to be used even during the scanning procedure at pulse repetion rates close to 2 kHz. This may avoid the creation of look up tables for the steering of the phased array equipment during the planning phase of an inspection.
The sound field calculation program calculates the directivity patterns shown in Fig. 4 where different angles of incidence have been realized by a shear wave probe of 3.7 MHz. The grating lobes can be recognized, they are in a good agreement with the grating lobes observed during the practical applications.
- Software to create look up tables for the steering during an inspection.
- Another important software module is the equipment control software which delivers the delay time and amplification distribution values, time gain control curves etc. to the phased array equipment in order to allow the execution of the desired function during the probe scanning movement. This control software has to cop with the needed fast pulse repetition rate. Typically 1 kHz to 10 kHz pulse repetition rates are possible. Since many phased array applications are limited by late returning echos, e.g. in the case of large turbine shafts, one is forced to use in such cases a pulse repetition rate down to some 40 or 50 Hz. The control software has to carry out the data storage which should be fast enough in order to guarantee that the pulse repetition rate is not limited by the storage procedure. The control software has also to guarantee that all the results are stored in a given structure e.g. characterized by the so called ZEUS data format [22].
- The fifth essential software package is a package for the presentation and evaluation of the results. Here different approaches may be used: from simple time displacement scan (TD-) presentations over C-scan, B-scan to SAFT-reconstructions and echotomography presentations. The different pictures produced by such software packages have to be adapted to the given purpose of specific inspection tasks.
4. SCANNING MODES
The different scanning modes for a phased array equipment can be:
- Free sweeping of the beam e.g. for a sector scan, a parallel scan or even a focus scan for dynamic focusing. Those sweepings can be triggered by the repetition rate frequency with a constant increment between the different shots, that means e.g. a 0.2° step for a sector scan between the different beam angles or also with a variable increment adapting the sector scan or parallel scan to critical areas.
- Angles, focusing, amplification and TGC-curves predetermined by a look up table or calculated during the scanning procedure and triggered by the probe position along the scanning path. This underlines the link between the software modules for geometry and the soundfield modelling.
- The execution of selected and modified inspection functions at specific probe positions according to specific interference conditions, curvatures, expected defects or other specific events, like e.g. a probe approaching to a specific area in a weld, where the internal noise increases and a specific focusing is needed.
The storage of the inspection results (e.g. containing the digitized A-scans, the probe parameters and the probe positions) has for all different scanning modes to guarantee that during the evaluation of the results images can be produced for specific inspection functions, angles or scanning pathes. That means that the data format (e.g. ZEUS format ) must allow the access to A-scans according to different selection criteria.
The execution of the selected inspection functions needs special preparations at the equipment hardware in order to allow a versatile adaptation of the software to the specific sequence of the required inspection functions. Particularly such equipments can be represented by a schematic diagram like shown in the Fig. 8.This figure shows that by the use of a central bus structure such phased array equipments are allowing a very flexible adaptation to different purposes. It should especially be possible for a fast repetition rate that a position dependent triggering of specific function sets can be supported by the intermediate storage of the steering parameter data ( delay time distributions etc. ).
The following examples are describing application cases for the different scanning modes.
5. APPLICATION OF A SCANNING MODE WITH POSITION INDEPENDENT BEAM SWEEPING
6. APPLICATION OF INTELLIGENT SCANNING MODES WITH POSITION AND FUNCTION DEPENDENT STEERING OF THE PHASED ARRAY EQUIPMENT
As shown in Fig. 6 for the inspection of the nozzle inner corner area at an emergency cooling inlet nozzle, fairly large probes must be moved along the scanning path. Since the probe can not be rotated during that movement, it is essential to vary the angles of incidence and skewing electronically. This has been realized by a multi-array probe containing 4 different modules in one probe housing as demonstrated in Fig. 13 top right-hand side. The module 4 of this probe had been used to detect 4 notches within the nozzle inner corner area as demonstrated in Fig. 13 right-hand side bottom. The resulting TD-scan is shown in the same figure left-hand side. One can clearly recognize the indications of the 4 different notches. It is also possible to estimate the different notch depth represented by the echo-amplitude and dynamic behaviour. This application required a careful calculation of look up tables, which had been used during the scanning movement to feed to the phased array equipment at each position an adapted steering data set for the probe soundfield and sensitivity.
Fig 13: Inspection of the Inner Nozzle Corner with a Phased Array Probe
|
Fig 14: Multi-Array-Probes for the Inspection
of the spherical bottom of BWR-Plants
|
Fig 15: Assumed Cracks at the Bottom of BWR-PV
|
A similar procedure for the steering data set had been necessary during the application of a phased system at the inspection of the spherical bottom of boiling water reactors, where during the movement along the scanning path a continuous change of the angles had to be realized. Fig. 14 shows up the control rod holes and assumed defects together with the corresponding probe skewing angles. Fig.15 shows the results of such an inspection. During the movement along pathes between the control rods typical pictures are produced. Combining the inspection results for the control rod ligaments from both sides one produces patterns which can easily be interpreted and evaluated concerning possible anomalies due to the presence of defects.
Another example for an event controled scanning mode is the inspection of axles from railroad wheel sets. Axles without an inner hole are difficult to inspect without dismantling the whole set. The application of phased array probes at different coupling positions as demonstrated in Fig. 16 allows the surveillance of very large areas at the surface of such axles without dismantling them. Fig. 17 shows the results of the phased array scanning where TD-scans have been produced at different angles, thus demonstrating the possibility to detect the different reference defects at the indicated positions. The specific problem for that inspection is shown in Fig. 18 where specific geometric indications from the diskbrakes are demonstrated. Those geometric indications have to be discriminated from defects. This can be enhanced by the adaptation of the increment step during the angular scanning at the angles with typical A-scan patterns linked to diskbrake indications.
Fig 16: Ultrasonic Inspection of Railway Axles with Phased Arrays
|
Fig 17: Detection of Test Notches by a Phased Array Probe
|
Fig 18: TD - Scan at a Railway axle
Probe Position 833 mm
|
The last example is representing the inspection of a girth weld at a pipeline. A typical probe arrangement according to RTD Rotterdam is shown in Fig. 19. In order to reduce the need for a specialized multiple probe arrangement requiring a careful individual adaptation to each wallthickness and tube diameter, a phased array realtime scanner as demonstrated in Fig. 20 can be used. Such a phased array probe, in case of Fig 20 a 64 element probe for 3 Mhz, allows the movement of a beam and the simultaneous angle sweep. Another important feature of such a probe and the connected electronic equipment is the possibility of specific tandem inspection tasks as shown in Fig. 21 and proposed by Fig. 19. Fig. 21 demonstrates the usefulness of the fact that during the emitting phase and the receiving phase totally different delay time distributions can be applied allowing the exitation and reception of shear- or longitudinal waves under specific angles at the same shot. The application of such a technique needs of course a careful check of the zone distribution by modelling and also at testblocks. An example of calculations for the zone distribution based on a model is demonstrated in Fig. 22, where the echo amplitude dependency from the defect inclination can be seen for different index point distances and angles of incidence.
Fig 19: Probe Arrangement for Girth Weld Inspection on Pipelines
|
Fig 20: Weld Inspection Using a Real-Time-Scanner
|
Fig 21: Real - Time - Scanner for Tandem Technique
|
Fig 22: Defect Inclination versus Echoheight
|
7. CONCLUSIONS
The scanning modes of a phased array inspection are linked to the equipment possibilities and the software features.
Five software modules are needed for the planning, execution and evaluation phase:
- Calculation of the geometry data by CAD or similar packages
- Soundfield modelling and/or analytical formula for the beam forming
- Creation of look up tables for the steering during an inspection
- Equipment control software during the execution phase
- Presentation and evaluation of the results
Essentially three scanning modes can be discriminated:
- Free sweeping of a beam
- Execution of selected inspection function sets linked to the probe position
- Execution of the selected inspection function triggered by special events
The last 2 modes require special precautions at the equipment hardware in order to allow a versatile adaptation of the software to the specific problem.
8. LITERATURE
- A. Erhard, H. Wüstenberg, G. Schenk, W. Möhrle:Calculation and Construction of Phased Array-UT Probes;Proceedings 3rd German-Japanese joint Seminar on Research of Structural Strength and NDE Problems in Nuclear Engineering. Non-destructive Examination III; August 29 and 30, 1985, Stuttgart/West-Germany; Editor Prof. Kussmaul, MPA-Stuttgart III.2.2
- H. Wüstenberg, A. Erhard, G. Schenk, W. Möhrle:Construction des palpeurs-multiéléments avec ultrasons Revue Pratique de Contrôle Qualité Industriel, No. 133 bis 24. Année, Septembre 1985, p. 43-53
- G. Schenk, H. J. Montag, H. Wüstenberg, A. Erhard; Entwicklung und Anwendungsmöglichkeiten eines rechnergestützten Gruppenstrahlerkonzepts für die Ultraschallprüfung Amts- und Mitteilungsblatt der Bundesanstalt für Materialforschung und -prüfung (BAM) 15, Nr. 4, 1985
- H. Wüstenberg, W. Möhrle, W. Wegner:Winkelprüfköpfe mit Schielwinkelschwenk durch laufzeitgesteuerte Gruppenstrahler;DGZfP DACH-Jahrestagung 1987, Lindau, 25.-27.5.1987, Berichtsband 10, Teil 2, S. 538-550
- Wüstenberg H., A. Erhard, G. Schenk, H.-J. Montag:Anwendung der Ultraschalltomographie an Turbinen und Generatorwellen; Materialprüfung 29 (1987), Nr. 10, S. 297-302
- H. Wüstenberg, W. Möhrle, E. Schulz Phased Array Concept for the Ultrasonic Inservice Inspection of the Spherical Bottom of BWR-Pressure Vessels.
Nuclear Engineering and Design 112 (1989), S. 105-114
- M. Goto, S. Nagai, K. Uchida, Y. Kato, K. Onda;
Automated Phased Array UT System for Turbine Blade Inspection
ASM International, 1990
- NDT Systems S.A., France;
ALLIN High Speed Digital Ultrasonic Inspection System;
Materials Evaluation October 1993
- Desruelles-D., Burat-O., Pierre-G. Framatome Tech Center, Saint Marcel, F Inspection of tube using ultrasonic phased array probes Proceedings of the 14th World Conference on NDT (14th WCNDT), New Delhi,India, Dec 8-13, 1996. Vol. 4, (1996) page 2031-2034, New Delhi: Oxford and IBH Publ.
- Erhard, A., G. Schenk., W. Möhrle, H.-J. Montag Schweißnahtprüfung mit Real-Time-Scanner-Prüfköpfen; in: Berichtsband 59.1 der DGZfP-Jahrestagung "ZfP als Dienstleistung in einer veränderten Industriestruktur" Dresden, 05.-07.Mai 1997, S.103-111
- Roy-O., Mahaut-S., Serre- M.Commissariat a l'Energie Atomique, Saclay, F NDT of specimen of complex geometry using ultrasonic adaptive techniques. The F.A.U.S.T. system.Review of Progress in Quantitative Nondestructive Evaluation. Proceedings of the 24th Annual Symposium, San Diego, USA, July 27-August 1, 1997, Volume 17B (1998) page 1689-1695, New York: Plenum Press
- Spies-M., Gebhardt-W., Kröning-M.IzfP Saarbrücken Recent developments in phased array technology.Konferenz-Einzelbericht: Jahrestagung 1998 Zerstörungsfreie Materialprüfung. 70 Jahre ZfP von Schweißverbindungen, Bamberg, D, 7.-9.September 1998. Vol. 1. Deutsche Gesellschaft für Zerstörungsfreie Prüfung e. V. (DGZfP)
- Ciorau,P., D. Macgillivray, A. Lamarre, F. Jacques Feasibility Study of Ultrasonic Inspection Using Phased Array of Turbine Blade Root and Rotor Steeple Groves Part 2 Proceedings; EPRI Phased Array Inspection Seminar, Sept. 8.-9. 1998
- Ichiro Komura, Taiji Hirasawa, Satoshi Nagai (Toshiba),Jun-ichi Takabayashi (Keihin), Katsuhiko Naruse (Isogo Nuclear)Crack Detection and Sizing Technique by Ultrasonic and Electromagnetic Methods Proceedings of the 25th MPA Seminar, MPA Stuttgart, Germany, October 7 - 8, 1999
- Schlengermann, U. Schallfeldausbildung bei ebenen Ultraschallquellen mit fokussierenden Linsen. Acustica 30 (1974) Nr. 6, S. 291-294
- H. Wüstenberg, E. Schulz, W. Möhrle, J. Kutzner:Zur Auswahl der Membranformen bei Winkelprüfköpfen für die Ultraschallprüfung Materialprüfung 18 (1976) Nr. 7, S. 223-230
- Wüstenberg, H.; Kutzner, J.:Empfindlichkeitseinstellung beim Einsatz fokussierender Prüfköpfe in der Ultraschallprüfung an ebenen und gekrümmten Bauteilen Materialprüfung 19 (1977) Nr. 10, Oktober 1977
- H. Wüstenberg: Improvements in the Design of Focussed Angle Probe;Nondestructive Testing Communications, 1985, Vol. 2, pp. 55-64
- K. J. Langenberg, T. Kreutter, P. Fellinger Physikalische Elastodynamik statt Punktquellensynthese Gesamthochschule Kassel, Dezember 1987
- H. Wüstenberg, W. Möhrle, BAM Berlin Erfahrungen mit theoretischen Modellen für Schallfeld- und Impulsverhalten beim Bau von Sonderprüfköpfen für die UltraschallprüfungBerichtsheft der Deutschen Gesellschaft für ZfP e.V. zur DACH-Tagung 6.-8. Mai 1991 Luzern/Schweiz
- H. Wuestenberg, R. Boehm Simulation of an Ultrasonic Inspection "http://www.ultrasonic.de"
Copyright 1. Nov 1996
- Montag, H.-J. (BAM - Berlin)Datenstrukturen für die automatisierte Auswertung
in: Berichtsband 62 der DGZfP, Seminar "Automatisierung der Ultraschallprüfung, Gerätetechnik und Regeln zur Anwendung und Auswertung", Saarbrücken, 17.-18.November 1997, S.129-138