Code - Title
| Ma X | 253 - ANALYSIS OF THE REASON TO PRODUCE NOISY IN ULTRASONIC DETECTING OF TITANIUSM ALLOYS
|
| MacLauchlan D | 196 - RECENT ADVANCEMENTS IN THE APPLICATION OF EMATS TO NDE
|
| Maerz N | 589 - EXPERIMENTAL NON-DESTRUCTIVE TESTING OF FRP MATERIALS, INSTALLATION, AND PERFORMANCE, DALLAS COUNTY BRIDGE, MISSOURI, USA
|
| Maes G | 567 - HIGH-PERFORMANCE PIPE WELD INSPECTION USING STATE-OF-THE-ART PHASED ARRAY UT EQUIPMENT AND METHODOLOGY
|
| Maev R | 448 - NEW GENERATION OF HIGH RESOLUTION ACOUSTIC IMAGING TECHNIQUE FOR MATERIAL CHARACTERIZATION AND NDT
|
| Mahaut S | 381 - NEW FEATURES FOR PHASED ARRAY TECHNIQUES INSPECTIONS : SIMULATION AND EXPERIMENTS
415 - SIMULATION OF ULTRASONIC DEFECT RESPONSES IN REALISTIC INSPECTION CONFIGURATIONS: THEORETICAL PREDICTIONS AND EXPERIMENTAL VALIDATIONS
|
| Makarov V | 203 - INTEGRATED EXAMINATION OF TECHNICAL CONDITION OF MOLYBDENUM BOATS
|
| Malyutenko V | 606 - REMOTE MICRO MAPPING OF HEAT FLOWS IN SEMICONDUCTOR DEVICES
|
| Mandache C | 292 - MAGNETIC FLUX LEAKAGE INVESTIGATION OF INTERACTING DEFECTS: COMPETITIVE EFFECTS OF STRESS CONCENTRATION AND MAGNETIC SHIELDING
|
| Mandelis A | 38 - LASER PHOTO-CARRIER RADIOMETRY: TECHNIQUE AND APPLICATIONS TO SEMICONDUCTOR FABRICATION PROCESS NDE
39 - TRANSVERSE DEPTH-PROFILOMETRIC HARDNESS PHOTOTHERMAL PHASE IMAGING OF HEAT TREATED STEELS
|
| Mango S | 725 - TRANSITIONING TO DIGITAL RADIOGRAPHY - WHEN DOES IT MAKE SENSE?
|
| Manzke H | 607 - IMPROVEMENT OF THE APPLICABILITY OF SHEAROGRAPHY UNDER AIRCRAFT PRODUCTION AND MAINTENANCE CONDITION
|
| Marstboom K | 803 - ECOLOGICAL AND ECONOMICAL SOLUTIONS FOR FILM RADIOGRAPHY
|
| Marty P | 193 - NDT OF KISSING BONDS IN AERONAUTICAL STRUCTURES
|
| Maslouhi A | 702 - EVALUATION OF GLASS FIBRE/ POLYPROPYLENE COMPOSITES BY QUANTITATIVE LASER ULTRASONIC AND ACOUSTIC EMISSION TECHNIQUES
|
| Matyuk V | 780 - TESTING OF MECHANICAL PROPERTIES OF THE LIGHT-GAUGE ROLLED PRODUCTS OF LOW-CARBON STEELS IN THE ZINC GALVANIZING LINE BY THE PULSE MAGNETIC METHOD
|
| Mayer K | 261 - ULTRASONIC PHASED ARRAY AND SYNTHETIC APERTURE IMAGING IN CONCRETE
|
| Mc Hugh J | 615 - ULTRASOUND PROCESS MONITORING OF REACTIVE PLASTICS
616 - CHARACTERISATION OF EPOXY BASED MATERIALS USED IN THE DEVELOPMENT OF ULTRASOUND TRANSDUCERS
|
| McGregor A | 128 - THE APPLICATION OF LONG RANGE GUIDED ULTRASONICS FOR THE INSPECTION OF RISER PIPES
|
| McMillan J | 791 - IMPROVEMENTS OF THE APPLICATION OF EMAT TECHNOLOGY
|
| Meade W | 92 - Inspection Reliability Comparison of Digital Radiography, Film Radiography and Radioscopy for Inspection of Inconel Welds
|
| Medina L | 78 - ARTMAP NETWORK AND WAVELET ANALYSIS FOR FLAWS CHARACTERIZATION
|
| Meyer P | 223 - OUR EXPERIENCE WITH SINGLE CRYSTAL PIEZOCOMPOSITE TRANSDUCER MATERIALS
|
| Mijarez R | 511 - CONTINUOUS MONITORING GUIDED WAVE ENCODED SENSOR FOR FLOOD DETECTION OF OIL RIGS CROSS BEAMS
|
| Mogilner L | 510 - DEVELOPMENT OF TECHNOLOGY ULTRASONIC THICK MEASURING AT DYNAMIC MODE
|
| Moguilner L | 433 - NEW TECHNOLOGICAL AND TECHNICAL DECISIONS IN DIAGNOSTICS OF STEEL GAS MAINS INSIDE INHABITED AND INDUSTRIAL BUILDINGS
|
| Moles M | 83 - AUTOMATED ULTRASONIC INSPECTION OF PRESSURE VESSEL WELDS
84 - COMPLETE INSPECTION OF FRICTION STIR WELDS IN ALUMINUM USING ULTRASONIC AND EDDY CURRENT ARRAYS
85 - PIPELINE GIRTH WELD INSPECTIONS USING ULTRASONIC PHASED ARRAYS
86 - FASTFOCUS™ PHASED ARRAY SYSTEM FOR AIR PLANE FASTENER INSPECTIONS
|
| Monchalin J | 721 - OPTICAL AND LASER NDT: A RISING STAR
722 - NON CONTACT GENERATION AND DETECTION OF ULTRASOUND WITH LASERS
|
| Monks J | 742 - EMAT ULTRASOUNIC SYSTEM DEVELOPMENT: FROM THE LAB TO THE PROCESS LINE
|
| Montero De Espinosa F | 252 - AIR-COUPLED PIEZOELECTRIC ARRAY TRANSDUCERS FOR NDT APPLICATIONS
|
| Moreau A | 731 - INLINE MEASUREMENTS OF TEXTURE AND RECRYSTALLIZATION ON ALUMINUM ALLOYS
|
| Morozov M | 387 - A COMPUTATIONAL TECHNIQUE FOR AUTOMATED RECOGNITION OF SUBSURFACE CRACKS IN AERONAUTICAL RIVETED STRUCTURES
|
| Morro F | 812 - THE USE OF COMPUTED RADIOGRAPHY AS A DIRECT FILM REPLACEMENT
|
| Moysan J | 414 - SIMULATIONS OF THE INFLUENCE OF THE GRAINS ORIENTATIONS ON ULTRASOUNDS PROPAGATION
|
| Mozurkewich G | 303 - NONDESTRUCTIVE TESTING ACTIVITIES, NEEDS, AND TRENDS IN THE AUTOMOTIVE INDUSTRY
|
| Mtenga P | 480 - IRT EVALUATION OF BOND LAYER THICKNESS FOR CFRP BONDED TO CONCRETE
|
| Mucciardi F | 122 - A SENSOR FOR CONTINUOUS TEMPERATURE MEASUREMENT IN STEELMAKING ENVIRONMENTS
|
| Mudge P | 785 - PRACTICAL ENHANCEMENTS ACHIEVABLE IN LONG RANGE ULTRASONIC TESTING BY EXPLOITING THE PROPERTIES OF GUIDED WAVES
|
| Mueller B | 262 - MICRO CRACK CHARACTERIZATION OF METAL MATRIX COMPOSITES BY 3D-REFRACTION-COMPUTED-TOMOGRAPHY
352 - X-RAY REFRACTION TOPOGRAPHY CHARACTERIZES INTERNAL NANO INTERFACES
355 - X-RAY DIFFRACTION TOPOGRAPHY IMAGES MATERIALS BY MOLECULAR PROBE
|
| Mugallimov F | 830 - NEW TECHNIQUE AND TECHNOLOGY OF AN INSPECTION OF RIVER PIPELINE CROSSING OF PIPELINES
|
| Mulaveesala R | 354 - ELECTRO-THERMAL MODELING AND MATLAB-SIMULINK SIMULATION OF LOCK-IN THERMOGRAPHY FOR NON-DESTRUCTIVE CHARACTERISATION
|
| Muravin G | 513 - QUANTITATIVE ACOUSTIC EMISSION NDI FOR ANALYSING DYNAMIC FRACTURE
|
| Murayama R | 67 - DEVELOPMENT OF ULTRASONIC WAVE NONDESTRUCTIVE INSPECTION ROBOT WITHOUT COUPLING MEDIUM USING EMAT
642 - DEVELOPMENT OF A NON-CONTACTING STRESS MEASUREMENT SYSTEM DURING TENSILE TESTING USING THE ELECTROMAGNETIC ACOUSTIC TRANSDUCER FOR A LAMB WAVE
|
| Murphy R | 805 - NDT CERTIFICATION - GLOBAL HARMONIZATION
|
| Murray T | 571 - HIGH FREQUENCY LASER BASED ACOUSTIC MICROSCOPY USING A CW GENERATION SOURCE
|
| Murugaiyan R | 208 - TIME OF FLIGHT DIFFRACTION (TOFD), AN ADVANCED NON-DESTRUCTIVE TESTING TECHNIQUE FOR INSPECTION OF WELDS FOR HEAVY WALLED PRESSURE VESSELS
|
| Muzhitskiy V | 77 - PORTABLE ELECTROMAGNETIC-ACOUSTIC THICKNESS GAUGES (EMATG)
144 - TEN YEARS OF EXPERIENCE OF STRESS-CORROSION AND OTHER PIPELINES’ SURFACE FLAWS TESTING BY MEANS OF EDDY CURRENT TECHNIQUE
210 - DIGITAL PROCESSING METHODS IN EDDY-CURRENT FLAW DETECTION
|
| Myers J | 90 - MICROWAVE NONDESTRUCTIVE EVALUATION OF CARBON FIBER REINFORCED POLYMER CONCRETE BEAMS UNDER CYCLIC LOADING
157 - VALIDATION OF FRP COMPOSITE TECHNOLOGY THROUGH FIELD TESTING
762 - Use of the Total Station for Serviceability Monitoring of Bridges with Limited Access
763 - Non Destructive Testing of Dallas County Bridge
|
| Nagae M | 318 - DAMAGE ESTIMATION METHOD FOR GAS TURBINE HOT SECTION COMPONENTS BASED ON NDI MICROSTRUCTURE ANALYSIS
|
| Nagy P | 231 - RESIDUAL STRESS ASSESSMENT IN SURFACE-TREATED NICKEL-BASE SUPERALLOYS
|
| Nakamura N | 106 - RESONANCE ULTRASOUND SPECTROSCOPY FOR EVALUATING ELASTIC CONSTANTS AND INCOHESIVE BONDS OF THIN FILMS
|
| Nassar S | 714 - OPTICAL INSPECTION OF MECHANICALLY FASTENED COMPOSITE JOINTS
|
| Nielsen S | 377 - AUTOMATIC LASER ULTRASONICS FOR RAIL INSPECTION
|
| Nogues M | 112 - RESIDUAL STRESS EVALUTION ON INDUSTRIAL HEAVY PLATES BY ACOUSTICAL BIREFRINGENCE
|
| Norman J | 459 - EVALUATION OF SPOT WELD FORMATION AS A FUNCTION OF DEGRADATION AND ELECTRODES RELATIVE POSITION USING ACOUSTIC WAVE REFLECTION MODE
|
| Obrutsky A | 47 - DESIGN AND CONSTRUCTION OF EDDY CURRENT SENSORS WITH RECTANGULAR PLANAR COILS
740 - REFLECTOGRAPHY, AN NDT METHOD FOR IMAGES DIAGNOSIS
|
| Obrutsky De Marini L | 441 - EDDY CURRENT TECHNOLOGY FOR HEAT EXCHANGER AND STEAM GENERATOR TUBE INSPECTION
|
| O'Connor M | 822 - NEAR FIELDTM INSPECTION OF FERROMAGNETIC HEAT EXCHANGER TUBES
|
| Ogi H | 68 - ELECTROMAGNETIC-RESONANCE-ULTRASOUND MICROSCOPY (ERUM) FOR QUANTITATIVE EVALUATION OF LOCALIZED ELASTIC CONSTANTS OF SOLIDS
|
| Ohtani T | 101 - CHANGE OF ULTRASONIC ATTENUATION AND MICROSTRUCTURE EVOLUTION DURING CREEP OF A STAINLESS STEEL
|
| O'Neill B | 724 - WASPALOY FATIGUE DAMAGE MONITORING USING SAW ACOUSTO-ELASTICITY
|
| Osami K | 362 - AGED CONCRETE STRENGTH AND PROPAGATION VELOCITY RATIO OF LONGITUDINAL AND TRANSVERSE WAVE
|
| Osamu Y | 46 - INJECTION OF REPAIRING MATERIALS TO CRACKS USING ULTRASONIC RECTANGULAR DIFFRACTION METHOD
|
| Padua G | 709 - ESTIMATED ACCURACY OF CLASSIFICATION OF DEFECTS DETECTED IN WELDED JOINTS BY RADIOGRAPHIC TESTS
715 - CLASSIFICATION OF WELDING DEFECTS IN X-RAYS USING TRAVERSE PROFILES TO THE WELD SEAM
|
| Panetta P | 535 - CHARACTERIZATION OF SOLID LIQUID SUSPENSIONS FOR PROCESS MEASUREMENT AND CONTROL UTILIZING NON-INVASIVE ULTRASONIC MEASUREMENTS
536 - NON-CONTACT MEASUREMENT OF PLASTIC DEFORMATION IN PIPELINES UTILIZING EMATS
538 - ULTRASONIC MATERIALS CHARACTERIZATION OF DEGRADATION IN CIVIL STRUCTURES
|
| Papadakis E | 683 - FINANCIAL CALCULATIONS FOR PROCESS CONTROL BY NON-DESTRUCTIVE 100% INSPECTION
|
| Park I | 557 - NONCONTACT AIR-COUPLED GUIDED WAVE MODE IDENTIFICATION USING WAVELET TRANSFORM
|
| Patel N | 825 - ULTRASONIC TECHNIQUE FOR STUDYING SURFACE RESIDUAL STRESSES RESULTED IN MACHINING
|
| Perez C | 335 - NOZZLE INSPECTION USING PHASED ARRAY TECHNOLOGY
|
| Pichenot G | 338 - EDDY CURRENT MODELING FOR NONDESTRUCTIVE TESTING
339 - EDDY CURRENT ARRAY PROBE DEVELOPMENT FOR NONDESTRUCTIVE TESTING
341 - EDDY CURRENT MODELING OF FERRITE-CORE PROBES, APPLICATION TO THE SIMULATION OF EC SIGNALS FROM SURFACE BREAKING FLAWS IN AUSTENITIC STEEL
|
| Piwakowski B | 530 - P-T TRANSFORMATION AS THE EFFICIENT TOOL FOR DETERMINATION OF THE VELOCITY DISPERSION CHARACTERISTICS IN COMPLEX STRUCTURES
|
| Plis R | 598 - BLUE ETCH ANODIZE: A CONTINUING WORKHORSE INSPECTION METHOD FOR AEROSPACE PARTS
|
| Poguet J | 66 - REPRODUCIBILITY AND RELIABILITY OF NDT PHASED ARRAY PROBES
386 - NEW FEATURES AND INNOVATION FOR NDT PHASED ARRAY PROBES
|
| Popovics J | 590 - THE USE OF SURFACE WAVES TO CHARACTERIZE IN-PLACE QUALITY OF CONCRETE
|
| Porco F | 600 - NDT PROTOCOLS FOR THE DIAGNOSTICS AND MAINTEINANCE OF EARLY REINFORCED CONCRETE STRUCTURES: A CASE STUDY
|
| Pörtzgen N | 611 - ADVANCES IN IMAGING OF NDT RESULTS
|
| Pouet B | 575 - NEW LASER ULTRASONIC INTERFEROMETER FOR INDUSTRIAL APPLICATIONS
|
| Prevorovsky Z | 766 - NONLINEAR ELASTIC WAVE SPECTROSCOPY OF POLYMER SAMPLES WITH LASER INDUCED CRACKS
|
| Prokhorenko P | 778 - SUBSURFACE WAVES IN SOLIDS WITH CURVED SURFACE AND ACOUSTICAL IMPEDANCE ON IT
781 - NEW APPROACH TO THE DESCRIPTION OF DEFECTS DEVELOPMENT AT PENETRANT INSPECTION
|
| Pursley J | 123 - APPLICATIONS OF CMOS DIGITAL X-RAY
|
| Pushkina I | 174 - DETERMINATION OF NECESSARY AND SUFFICIENT NUMBER OF SENSORS IN CASE OF PIPELINES WALLS’ STRESS-CORROSION TESTING BY MAGNETIC FIELD LEAKAGE TECHNIQUE
176 - DYNAMIC MEASUREMENTS OF PARAMETERS OF RAILWAY TOP STRACTURE BY EDDY-CURRENT EQUIPMENT
180 - OPTICAL STRUCTUROSCOPY: DEVELOPMENT OF EFFICIENT DIGITAL ALGORITHMS IMPROVING MEASRUREMENT ACCURACY
182 - NEW ACHIEVEMENTS IN THE FIELD OF DEVELOPMENT OF MOBILE X-RAY TV SYSTEM
183 - NEW MEANS OF THE THERMOVISION INSPECTION DESIGNED FOR TASKS OF ANTI-TERRORISM SECURITY AND TECHNOGENIC SAFETY
184 - OPTICAL TESTING METHODS AND THEIR REALISATION IN THE INSTRUMENTS DEVELOPED BY JSC “SPECTRUM” – RII”
185 - CRAWLER CONTROL PROCEDURE
|
| Quarry M | 315 - A FLEXURAL MODE TUNING TECHNIQUE FOR MEMBRANED BOILER TUBING
|
| Que K | 158 - STUDY ON FLEXIBLE PHASED ARRAY ULTRASOUND TESTING
|
| Rabtchevich A | 779 - THE DYNAMIC INDENTATION DEVICE FOR NONDESTRUCTIVE TESTING OF METALLIC ARTICLES MECHANICAL PROPERTIES
|
| Rack A | 370 - CHARACTERIZATION OF METAL FOAMS WITH SYNCHROTRON-TOMOGRAPHY AND 3D IMAGE ANALYSIS
|
| Raj B | 734 - PREDICTING STRAIN RATE DURING IR IMAGING OF TENSILE DEFORMATION USING MLP BASED ANN
735 - MAGNETIC BARKHAUSEN EMISSION TECHNIQUE FOR ASSESSMENT OF PERFORMANCE THROUGH INSIGHT OF MATERIALS AND MICROSTRUCTURES
|
| Rajendran V | 495 - EFFECT OF PRECIPITATION HARDENING BY AGING OF 8090 AL-LI ALLOY ON ULTRASONIC PARAMETERS
|
| Rao B | 826 - MODEL BASED STUDY OF EDDY CURRENT STANDARD FOR INSPECTION OF AEROSPACE STRUCTURES
|
| Rastkhah N | 126 - SAFE USE OF RADIATION SOURCES IN INDUSTRIAL RADIOGRAPHY, A SURVEY IN HAZARDS EVALUATION IN IRAN
134 - NATIONAL CERTIFICATION SCHEME IN IRAN, ADVANTAGES AND LIMITATIONS
140 - SCATTERING CORRECTION IN INDUSTRIAL COMPUTED TOMOGRAPHY
274 - CORROSION EVALUATION OF PIPES BY RADIOGRAPHY
|
| Rebuffel V | 228 - X-RAY IMAGING MODALITIES FOR THE INSPECTION OF NUCLEAR WASTE DRUMS
229 - DESIGN OF AN X-RAY IMAGING SYSTEM TO ANALYSE CORIUM-WATER INTERACTION
337 - RECENT IMPROVEMENTS FOR SCATTER SIMULATION IN SINDBAD, A COUPLED PHOTON MONTE CARLO AND CAD SOFTWARE
|
| Redmer B | 435 - MOBILE 3D-X-RAY TOMOGRAPHY FOR ANALYSIS OF PLANAR DEFECTS IN WELDS BY "TOMOCAR"
|
| Reinhart C | 566 - MODERN VOXEL BASED DATA AND GEOMETRY ANALYSIS SOFTWARE TOOLS FOR INDUSTRIAL CT
|
| Revel G | 697 - NON-CONTACT ULTRASONIC SENSORS FOR DENSITY MEASUREMENT AND DEFECT DETECTION ON WOOD
|
| Rhazi J | 751 - DETECTION OF FRACTURES IN CONCRETE
|
| Rideout C | 422 - NONDESTRUCTIVE QUANTIFICATION OF INDUCED SURFACE TREATMENT AND RELAXATION EFFECTS IN METALS
|
| Rivas S | 408 - AUTOMATED SPOT WELD INSPECTION IN THE AUTOMOTIVE INDUSTRY
|
| Rizzi M | 344 - DETECTION OF LASER ULTRASONIC SURFACE DISPLACEMENT BY WIDE APERTURE FIBER OPTIC AMPLIFIER
|
| Rosani A | 149 - MICROVAWE IMAGING FOR NONDESTRUCTIVE EVALUATION OF CIVIL STRUCTURES
|
| Rousseau G | 521 - FEEDER PIPING NDE – CURRENT CAPABILITIES AND FUTURE DIRECTION
|
| Rummel W | 619 - QUALIFICATION AND VALIDATION OF THE PERFORMANCE CAPABILITY (POD) FOR NONDESTRUCTIVE INSPECTION PROCEDURES
|
| Russo S | 659 - NON DESTRUCTIVE TEST FOR STRUCTURAL REHABILITATION. THE CASES OF DEVIL'S AND S.DONATO'S MASONRY BRIDGES IN VENICE
|
| Ryzhikov V | 272 - MULTI-ENERGY RADIOGRAPHY FOR NON-DESTRUCTIVE TESTING ON THE BASE OF SCINTILLATION CRYSTAL DETECTORS
|
| Sabbagh H | 646 - MODELING PITTING AND CORROSION PHENOMENA BY EDDY CURRENT VOLUME-INTEGRAL EQUATIONS
647 - ASSESSING THERMAL BARRIER COATINGS BY INVERSION OF EDDY-CURRENT IMPEDANCE DATA
|
| Sabsabi M | 679 - LASER-INDUCED BREAKDOWN SPECTROSCOPY: A NEW TOOL FOR PROCESS CONTROL
|
| Safizadeh M | 222 - AUTOMATIC CLASSIFICATION AND CHARACTERIZATION OF HIDDEN CORROSION USING PULSED EDDY CURRENT DATA
|
| Saka M | 129 - TECHNIQUES FOR NDE OF CLOSED CRACKS
|
| Salzburger H | 599 - DRY UT BY GUIDED SHEAR HORIZONTAL WAVES USING EMAT’S
|
| Samokrutov A | 255 - NON-DESTRUCTIVE TESTING OF RAILS IN CASE OF GUIDED WAVES USE
258 - WELDS ULTRASONIC TOMOGRAPHY BASED ON THE PHASED ANTENNA ARRAYS WITH SMALL-APERTURE TRANSDUCERS.
|
| Santos F | 348 - OPTICAL TOOL FOR IMPACT DAMAGE CHARACTERIZATION ON AIRCRAFT FUSELAGE
425 - XHINIA - A PORTABLE DIGITAL X-RAY SYSTEM TO BE DEPLOYED INTO AEROSPACE PRODUCTION AND IN-SERVICE ENVIRONMENTS
|
| Sarete J | 297 - NEW NDE PERSPECTIVES WITH MAGNETORESISTANCE ARRAY TECHNOLOGIES. FROM RESEARCH TO INDUSTRIAL APPLICATIONS.
298 - “ RASCANI “ : X-RAY BASED EXPERTISE FOR LOW COST INDUSTRIAL TOMOGRAPHY.
577 - ULTRASONIC SYSTEM FOR HIGH SPEED RAIL WHEEL RING INSPECTION
|
| Sato M | 502 - SIZING OF SMALL SURFACE-BREAKING TIGHT CRACKS BY USING LASER-ULTRASONICS
|
| Sauerwein C | 662 - EXTENDED 3D CT METHODS FOR THE INSPECTION OF LARGE COMPONENTS
760 - Inspection of New Materials, Components and Safety-Relevant Joints by Different 3D X-Ray Methods
|
| Schmarje N | 189 - LITHIUM NIOBATE CEMENT COMPOSITES FOR HIGH TEMPERATURE APPLICATIONS
|
| Schmitz S | 288 - ULTRASONIC TESTING LINE FOR THE AUTOMATIC INSPECTION OF SEAMLESS TUBES OF UP TO MAX. 250 MM OUTER DIAMETER, WITH INTEGRATED TUBE END TEST
|
| Schwartz C | 304 - USE OF TANGENTIAL RADIOGRAPHY AND RESONANCE ULTRASONIC TECHNIQUES TO EVALUATE BONDING QUALITY
|
| Seebacher S | 309 - INNOVATIVE NDT CONCEPTS FOR AEROSPACE INDUSTRY - THE INCA PROJECT
|
| Servent R | 558 - PRESENT AND FUTURE OF ET INSPECTION IN THE AUTOMOTIVE INDUSTRY
|
| Seung Hoon N | 504 - A NONDESTRUCTIVE ELECTRICAL METHOD FOR EVALUATING MECHANICAL PROPERTIES OF AL- FOAM
|
| Severina I | 444 - APPLICATION OF HIGH-RESOLUTION ACOUSTIC IMAGING FOR ADHESIVE BONDS EVALUATION
458 - ADHESIVE CURE MONITORING WITH ACOUSTIC METHOD
|
| Seviaryn F | 811 - ADAPTIVE FILTRATION OF ULTRASONIC SIGNALS IN CAR BODY ADHESIVE BONDS EVALUATION
|
| Shah B | 215 - PROFICIENCY TESTING PROGRAMME IN ULTRASONIC TESTING
|
| Sharapov A | 327 - TO THE QUESTION OF BIMETALLIC MATERIALS’ ULTRASONIC TESTING OF “STEEL- BABBIT” TYPE.
|
| Shark L | 273 - DEVELOPMENTS IN LOW COST OPTICAL DETECTION AND SIGNAL PROCESSING FOR LASER ULTRASONICS
|
| Shepard R | 730 - ELECTROMAGNETIC ACOUSTICAL TRANSDUCER (EMAT) INSPECTION OF STORAGE TANKS
761 - QUANTITATIVE CHARACTERIZATION OF THERMOGRAPHIC SEQUENCE DATA
|
| Shevaldykin V | 256 - EMAT TRANSFORMATION IN PULSED MAGNETIC FIELD AND ITS USE IN PORTABLE INSTRUMENTS FOR ACOUSTIC MEASUREMENTS.
|
| Shi C | 329 - THE STUDY ON ATTENUATION RULE OF X-RAY AND ? -RAY IN EXPLOSIVE
|
| Shoichi I | 130 - STRESS DIAGNOSIS METHOD BASED ON THE SECTION FLATNESS OF A BENT PIPE
|
| Shyu H | 257 - THE STATUS OF PERFORMANCE DEMONSTRATION IN TAIWAN
|
| Sinclair A | 195 - ULTRASONIC EVALUATION OF WEAK LINER/PROPELLANT BONDING IN A ROCKET MOTOR
428 - ENHANCEMENT OF SYNTHETIC APERTURE FOCUSING TECHNIQUE (SAFT) BY ADVANCED SIGNAL PROCESSING
434 - A NEW SIGNAL PROCESSING TECHNIQUE FOR ENHANCEMENT OF ULTRASONIC TESTING SIGNALS
|
| Sjerve E | 450 - IIW COMMISSION VC - ULTRASONICALLY BASED WELD INSPECTION
|
| Smith R | 436 - ADVANCES IN TRANSIENT EDDY-CURRENT IMAGING FOR AEROSPACE APPLICATIONS
438 - ADVANCED ULTRASOUND WAVEFORM ANALYSIS PACKAGE FOR MANUFACTURING AND IN-SERVICE USE
|
| Solomakha R | 613 - ESTIMATION OF STRESS, FATIGUE AND CAPACITY OF WELDS BY MEASUREMENTS OF MAGNETIC CHARACTERISTIC – COERCIVE FORCE (HC)
614 - NEW POSSIBILITIES OF NDT OF NUCLEAR REACTORS FRAME ON THE BASIS OF METAL MAGNETIC CHARACTERISTICS MONITORING
|
| Song S | 540 - IMPROVEMENT OF CONSPICUITY BY FUSION OF PULSE-ECHO DATA
|
| Sosnin F | 267 - INFLUENCE OF NDT ON REDUCTION OF LOSSES CAUSED BY EMERGENCIES IN RUSSIA.
|
| Stanic D | 582 - EDDY CURRENT INSPECTION OF CLADDING MATERIAL ON VVER 440 REACTOR PRESSURE VESSELS
|
| Steel K | 291 - A WIRELESS ULTRASONIC NDT SENSOR SYSTEM
|
| Stein M | 102 - EXPERIENCE OF USING SMALL-SIZE BETATRON MIB-5 IN THE STRUCTURE OF INDUSTRIAL COMPUTED TOMOGRAPH FOR TESTING OF HEAVY-WALL PRODUCTS
104 - SMALL-SIZE BETATRONS FOR RADIGRAPHIC INSPECTION
|
| Stepinski T | 397 - NARROWBAND ULTRASONIC SPECTROSCOPY FOR NDE OF LAYERED STRUCTURES
398 - OPTIMAL LINEAR RECEIVE BEAMFORMER FOR ULTRASONIC IMAGING IN NDE
|
| Stocco D | 302 - ANALYSIS OF SPOTWELD JOINTS BY ULTRASONIC INSPECTION, FEM AND RESIDUAL STRESS MEASUREMENTS.
|
| Storozhenko V | 260 - INFORMATION SIMULATION AND PROCESSING AT INSPECTION OF PRODUCTS WITH INTERNAL INHOMOGENEITIES USING ACTIVE THERMAL METHOD
|
| Stubbs D | 474 - AN AUTOMATED ULTRASONIC SYSTEM FOR INSPECTION OF AIRCRAFT TURBINE ENGINE COMPONENTS
799 - THE ROLE OF NDE IN THE LIFE MANAGEMENT OF STEAM TURBINE ROTORS
|
| Sukhorukov V | 220 - ROPE NDT AS MEANS TO RAISE SAFETY OF CRANE AND ELEVATOR USE
|
| Sun Z | 539 - PHASED ARRAY GUIDED WAVE FOCUSING IN PIPE
694 - APPLICATIONS OF FLAT GEOMETRY REMOTE FIELD EDDY CURRENT TECHNIQUES IN AIRCRAFT NONDESTRUCTIVE INSPECTION
|
| Svahn P | 340 - DEFECT SIMULATIONS FOR INTERDENDRITIC STRESS COROSSION CRACKS IN ALLOY 182 WELDS
|
| Swiderski W | 95 - NON-DESTRUCTIVE TESTING BY INFRARED THERMOGRAPHY FOR MILITARY APPLICATIONS IN POLAND
|
| Tadashi K | 514 - THEORY AND APPLICATION OF MEM PROCESSED IMPACT-ECHO FOR DETECTING VOID IN PC DUCT
|
| Tai C | 173 - HIDDEN FLAWS MEASUREMENT OF THIN TITANIUM-ALUMINUM BONDED PLATES USING ULTRASONIC TECHNIQUES
322 - DETECTION OF PARTIAL DISCHARGE IN CAST-RESIN DRY-TYPE TRANSFORMER BY USING ACOUSTIC EMISSION TECHNIQUE
|
| Takatsubo J | 246 - NONDESTRUCTIVE EVALUATION OF CRACKS BY AN ULTRASONIC TRANSIT TIMING METHOD.
|
| Takeo F | 494 - ADVANCEMENT OF THE CLOSELY COUPLED PROBES POTENTIAL DROP TECHNIQUE FOR NDE OF SURFACE CRACKS
|
| Takeuchi A | 35 - AN ATTEMPT OF ESTIMATION OF SOLID CONTACT AREA RATIO USING LONGITUDINAL ULTRASONIC WAVE PULSES
|
| Tang B | 37 - THE DESIGN OF NEUTRON RADIOGRAPHY FACILITY AND ITS APPLICATION IN SPRR-300
|
| Tanguy J | 417 - UT OF STEEL FORGINGS BY TRANSVERSE WAVES. COMPARISON OF EVALUATION AND ACCEPTANCE LEVELS OF FRENCH NUCLEAR PRACTICE (RCC-M) AND NEW EUROPEAN STANDARDS.
|
| Thiele H | 696 - RADIOGRAPHIC INSPECTION OF WELDINGS BY DIGITAL SENSORS
|
| Thompson J | 772 - APPROVAL OF NDT PERSONNEL UNDER THE PROVISIONS OF THE EUROPEAN PRESSURE EQUIPMENT DIRECTIVE
820 - Abstract not available
|
| Tian G | 775 - STUDY OF MAGNETIC SENSORS FOR PULSED EDDY CURRENT TECHNIQUES
|
| Titov S | 437 - ULTRASONIC MATERIAL CHARACTERIZATION SYSTEM EMPLOYING AN ARRAY OF RECEIVING TRANSDUCERS
|
| Tong P | 621 - DETERMINE NDT LABORATORY INSPECTION UNCERTAINTY BY ROBUST ISOGUM METHOD
648 - USING THE TRANSIENT ELASTIC WAVE TECHNIQUE TO IMAGE THE DEFECT OF CONCRETE STRUCTURE
|
| Topp D | 605 - APPLICATION OF THE ACFM INSPECTION METHOD TO RAIL AND RAIL VEHICLES
|
| Tosti E | 124 - X-RAY INSPECTION USING DIGITAL DEVICES APPLIED TO SPACE ENGINES USING CARBON FIBER CASE
|
| Treimer W | 234 - REVIEW ABOUT INCOHERENT AND COHERENT SIGNALS FOR COMPUTERIZED NEUTRON TOMOGRAPHY
|
| Trétout H | 275 - LASER ULTRASONIC TECHNOLOGY IN EUROPE FOR INNOVATIVE INSPECTION OF AIRCRAFT STRUCTURES
|
| Troitsky V | 640 - WORKPLACE OF NDT OPERATOR (ARM-D) FOR DIGITAL PROCESSING OF ROENTGENOGRAMS
|
| Tscheliesnig P | 111 - DETECTION OF CORROSION ATTACK ON SHIPS, ESPECIALLY OIL TANKERS WITH ACOUSTIC EMISSION (AE)
|
| Tsuji T | 493 - ELASTICITY CHARACTERIZATION OF PIEZOELECTRIC DOMAIN BOUNDARY BY ULTRASONIC ATOMIC FORCE MICROSCOPY
|
| Tsukatani I | 93 - INVESTIGATION OF MONITORING TECHNOLOGIES FOR HEAT TRANSFER CORROSION IN REPROCESSING EQUIPMENT
|
| Tucholski E | 119 - NONDESTRUCTIVE EVALUATION OF AIRCRAFT AND SPACECRAFT WIRING
|
| Turley J | 807 - NEW LOW COST, HIGH PERFORMANCE SHAPEMETER FOR SMALLER ROLLING MILLS & PROCESS LINES
|
| Turner J | 211 - NARROW GAP TIG AND ELECTRON BEAM WELD INSPECTION IN AUSTENITIC STAINLESS STEEL USING PULSE ECHO, TOFD AND PHASED ARRAY ULTRASONICS
|
| Udpa L | 429 - AUTOMATED ANALYSIS OF EDDY CUURENT SIGNALS FOR STEAM GENERATOR TUBE INSPECTION
728 - NOVEL METHODS FOR DETECTING FRACTURES IN PROSTHETIC HEART VALVES
776 - Eddy Current Testing - Are we at the limits?
|
| Van den Bos B | 393 - OPTIMISATION OF SHEAROGRAPHY TESTING USING STATISTICAL DESIGN OF EXPERIMENTS
|
| Vengrinovich V | 57 - NEW TECHNIQUES FOR RESOLUTION ENHANCEMENT IN 3D X-RAY TOMOGRAPHIC IMAGING FROM INCOMPLETE DATA
58 - STRESS AND TEXTURE MEASUREMENT USING BARKHAUSEN NOISE AND ANGULAR SCANNING OF DRIVING MAGNETIC FIELD
|
| Venkatraman B | 736 - A NOVEL METHOD FOR AUTOMATED EVALUATION OF RADIOGRAPHIC WELD IMAGES
|
| Victor G | 142 - INFERIOR FUELS OIL SIMULATED COMBUSTION TESTING, AS EQUIVALENT NDT
|
| Vieira Gomes L | 305 - PORTUGUESE INDEPENDENT SCHEME FOR NDT PERSONNEL CERTIFICATION
|
| Viswanathan K | 232 - DIGITAL SIGNAL PROCESSING OF ULTRASONIC SIGNALS FROM WELD DEFECTS A COMPARATIVE STUDY
|
| Vontobel P | 365 - NEUTRONS FOR THE STUDY OF ADHESIVE CONNECTIONS
593 - NON-DESTRUCTIVE INVESTIGATIONS OF SWISS MUSEUMS OBJECTS WITH NEUTRON AND X-RAY IMAGING METHODS
|
| Vun R | 692 - NON-CONTACT ULTRASONIC CHARACTERIZATION OF PROPERTIES IN ORIENTED STRANDBOARDS
693 - NON-CONTACT ULTRASONIC CHARACTERIZATION OF HOT MIX ASPHALT (HMA)
|
| Wartel T | 13 - TUBE CRACK DETECTION BY AE MONITORING OF DEEP DRAWING OPERATIONS IN THE AUTOMOTIVE INDUSTRY
|
| Wells J | 154 - SUMMARY OF BALLISTIC IMPACT DAMAGE IN TI-6AL-4V ALLOY WITH X-RAY COMPUTED TOMOGRAPHY
155 - ON THE FUTURE OF 3D VISUALIZATION IN MEDICAL AND INDUSTRIAL
|
| Wiesauer K | 280 - POLARISATION-SENSITIVE OPTICAL COHERENCE TOMOGRAPHY FOR MATERIAL CHARACTERISATION AND TESTING
|
| Wirdelius H | 426 - MODELLING OF ULTRASONIC BACKSCATTERING DUE TO GRAIN GROWTH IN A WELDED REGION
|
| Wolfe J | 456 - TANK INSPECTION AND CERTIFICATION UNDER THE GUIDELINES OF API 653 “TANK INSPECTION, REPAIR, ALTERATION AND RECONSTRUCTION”
|
| Xing C | 481 - EFFECTS OF STRESS CYCLES ON SURFACE MAGNETIC FIELD
|
| Yamada H | 156 - HIGH RESOLUTION X-RAY IMAGING BY PORTABLE SYNCHROTRON RADIATION SOURCE "MIRRORCLE"
|
| Yamanaka K | 508 - EVALUATION OF CLOSED CRACKS BY ANALYSIS OF SUBHARMONIC ULTRASOUND WITH CLOSURE STRESS
|
| Yan Z | 166 - THE ADAPTIVE NOISE CANCELLER BASED ON BACK PROPAGATION AND THE GENETIC ALGORITHMS TOGETHER
|
| Yang Y | 472 - THE ANGLE DISPLACEMENT MEASURE SYSTEM OF TIRE
534 - RECENT DEVELOPMENT OF DIGITAL SHEAROGRAPHY FOR NONDESTRUCTIVE TESTING
673 - RECENT DEVELOPMENTS FOR SURFACE DISTORTION MEASUREMENT
|
| Yaru M | 695 - THE RESEARCH OF ULTRASONIC DETECTION METHOD FOR CAR BACK OBSTRUCTION
|
| Yi S | 478 - AN IMPROVED CONE-BEAM FILTERED BACKPROJECTION RECONSTRUCTION ALGORITHM BASED ON X-RAY ANGULAR CORRECTION AND MULTIRESOLUTION ANALYSIS
|
| Yukuan M | 699 - EIGEN VECTOR ALGORITHM FOR 3-D NEAR-FIELD MULTIPLE SOURCES LOCALIZATION
700 - RESEARCH ON NEAR FIELD PASSIVE LOCATION BASED ON PHASE MEASUREMENT TECHNOLOGY BY FREQUENCY DIFFERENCE
701 - NEAR FIELD CYCLOSTATIONARY SOURCE LOCALIZATION BY HIGH ORDER CYCLIC CUMMULANT
|
| Yukuan M | 131 - A STUDY ON HOLE TESTING OF INTRAMEDULLARY NAIL BASED ON ULTRASONIC SENSOR
368 - REAL-TIME DATA SAMPLE AND WAVELET ANALYSIS SYSTEM BASED ON DSP FOR AE SIGNAL PROCESS
631 - FLUORESCENCE MAGNETIC PARTICLE FLAW DETECTING SYSTEM BASED ON LOW LIGHT LEVEL CCD
|
| Zabrodin A | 741 - CONSTRUCTION FEATURES OF AUTOMATED SYSTEMS FOR ULTRASONIC TESTING OF SHEET AND PROFILED PRODUCTS WITH THE USE OF ELECTROMAGNETIC ACOUSTIC TRANSDUCERS (EMAT)
|
| Zagrebelnyy V | 107 - COMBINED USE OF VISUAL-OPTICAL AND EDDY CURRENT METHODS ON NON-DESTRUCTIVE TESTING IN EVALUATION OF THE DEFECTS IN STRUCTURAL ELEMENTS
|
| Zahran O | 439 - AUTOMATIC CLASSIFICATION OF DEFECTS IN TIME-OF-FLIGHT-DIFFRACTION DATA
|
| Zawisky M | 141 - PHASE TOMOGRAPHY IN NEUTRON INTERFEROMETRY
|
| Zhang W | 379 - WAVELET ANALYSIS BASED ULTRASONIC NONDESTRUCTIVE TESTING OF POLYMER BONDED EXPLOSIVE
591 - APPLICATIONS OF FULL FIELD OPTICAL METHOD FOR MEASURING STRAIN CONCENTRATION
|
| Zhanxian X | 625 - CRAFT ENGINE BLADE’S CRACK TESTING ON SITE BY ALTERNATE MAGNETIC FIELD NON-TOUCH MOULD
626 - AIRCRAFT ON -EQUIPMENT TESTING TECHNOLOGY
628 - THE TRAINNING MODEL AND PRACTICE OF “DOUBLE CERTIFICATES”-THE ADVANCING ABOUT TEACHING REVOLUTION OF NONDESTRUCTIVE TESTING ENGINEERING FOR AIRCRAFT STRUCTURE
|
| Zhao X | 88 - WIRELESS NONDESTRUCTIVE INSPECTION OF AIRCRAFT WING WITH ULTRASONIC GUIDED WAVES
|
| Zhicheng H | 172 - THE FAST ALGORITHM STUDY FOR WAVELET IMAGE DENOISING BASED ON DSP
|
| Zhou Z | 202 - RESEARCH ON AUTOMATIC INSPECTION TECHNIQUES OF REAL-TIME RADIOGRAPHY FOR TURBINE BLADE
|
| Zhu H | 43 - IDENTIFICATION OF SHAPES OF TINY PITS ON AN INNER WALL USING BACK PROPAGATION NEURAL NETWORK
56 - MEASUREMENT OF OBJECT SPATIAL DISPLACEMENT BY ULTRASONIC SPECKLE CORRELATION METHOD
169 - INTENSELY SPONTANEOUS MAGNETIZATION OF A DRILL STEM FOR OIL AND GAS FIELD
170 - MAGNETIC PARTICLE PATTERN IN RADIATING FROM NEAR CORNERS OF A KEYSLOT ON WORKPIECE SURFACE
171 - MAGNETIC LEAKAGE FIELD CAUSED BY A RECTANGULAR SLOT ON THE WORKPIECE SURFACE
752 - THE GROWTH OF QUALIFICATION AND CERTIFICATION OF NDT PERSONNEL IN CHINA AND OUR VIEW POINT OF ISO 9712
|
| Zhukov Y | 204 - AUTOMATIC INSPECTION OF FE WELDING DEFECTS
|
| Zirnhelt J | 743 - MAGNETIC MEMORY METHOD (MMM): A CRITICAL REVIEW
744 - PERFORMANCE BASED QUALIFICATION: AN NDT SERVICE INDUSTRY PERSPECTIVE
|
| Zoughi R | 91 - MICROWAVE FIELD MEASUREMENT OF DELAMINATIONS AND THEIR GROWTH IN CFRP CONCRETE MEMBERS IN A BRIDGE
|
| Zscherpel U | 745 - RADIOGRAPHIC EVALUATION OF CORROSION AND DEPOSITS: IAEA CO-ORDINATED RESEARCH PROJECT-CALIBRATION TEST PIECES
831 - Unsharpness characteristics of digital detectors for industrial radiographic imaging
|
| Zuev L | 162 - NON-DESTRUCTIVE ESTIMATION OF MATERIAL STRENGTH BY PRECISE MEASUREMENT OF ULTRASOUND PROPAGATION RATE
|
| |