 code | ABSTRACT includes links to Full-Text and Options | GENERAL NDE | FULL-TEXT and Options |
|
 43 | IDENTIFICATION OF SHAPES OF TINY PITS ON AN INNER WALL USING BACK PROPAGATION NEURAL NETWORK | Hongmao Zhu, Huazhong University of Science and Technology, China | |
 186 | THE ISSUES OF GLOBALIZATION OF NDT AND TECHNICAL DIAGNOSTICS | Vladimir V. Klyuev, JSC "Spectrum" - RII", Russia | |
 189 | LITHIUM NIOBATE CEMENT COMPOSITES FOR HIGH TEMPERATURE APPLICATIONS | Nicole Schmarje, University Of Paisley, United Kingdom | |
 543 | ULTRASONIC SPECTROSCOPY USING A RAPID SWEEP TECHNIQUE | Joseph M Buckley, Sonatest Plc, United Kingdom | |
 779 | THE DYNAMIC INDENTATION DEVICE FOR NONDESTRUCTIVE TESTING OF METALLIC ARTICLES MECHANICAL PROPERTIES | A.V. Rabtchevich, Institute of Applied Physics, Belarus | |
 781 | A NON-LINER MODEL WITH DAMPING FOR IMPACT ANALYSIS OF A RIGIG INDENTOR ON TO VISCO-ELASTIC HALF SPACE | A. Kren, Institute of Applied Physics, Belarus | |
 821 | SECURITY OF NUCLEAR SUBSTANCES AND PRESCRIBED EQUIPMENT | David Cochrane | |