SHEAROGRAPHY AND APPLICATIONS IN NONDESTRUCTIVE EVALUATION

Michael Y. Y. Hung Manufacturing Engineering & Engineering Management Department City University of Hong Kong Hong Kong

Abstract:

This article reviews shearography and its applications in nondestructive testing. Shearography is a laser-based technique for full-field and non-contacting measurement of surface deformation (displacement or strains). Despite being a relative young technique, it has already received considerable industrial acceptance, in particular, for nondestructive testing. One major difference of shearography from other NDT techniques is the mechanics of revealing flaws. Shearography reveals defects in an object by identifying defect-induced deformation anomalies which are more relevant to structural weakness. Other applications of shearography include strain measurement, material characterization, residual stress evaluation, leak detection, vibration studies and 3-D shape measurement.

Introduction:

Shearography is an optical method for measuring surface deformation. Unlike traditional measurement techniques, shearography does not require the laborious task of mounting a large number of strain gages or transducers. It is a non-contacting method that yields full-field information about surface displacement or displacement derivatives. Shearography was developed to address several limitations of holography. Its significant advantages include (1) not requiring a reference light-beam, thus leading to simple optical setups, reduced coherence length requirement of the laser, and lax vibration isolation; and (2) direct measurement of surface strains (first-order derivatives of surface displacements). These distinct advantages have rendered shearography as a practical measurement tool that can be employed in industrial settings, and it has already gained wide industrial acceptance for nondestructive testing. For instance, the rubber industry routinely uses shearography for evaluating tires, and the aerospace industry has adopted it for nondestructive testing of aircraft structures, in particular, composite structures. Recently the technique has been extended to non-destructive evaluation of civil engineering structures. Other applications of shearography include: measurement of strains, material properties, residual stresses, 3-D shapes, vibrations, as well as leakage detection.

Three versions of shearography are in existence which are based on different recording media : photographic

[1]

; thermoplastic

[2]

; and digital

[3]

. Recently,

a unified approach for practising holography and shearography was reported

[4]

.

In this paper, only the digital version of shearography is presented.

Description of Digital Shearography :

A schematic diagram of digital shearography is shown in Fig. 1. The object to be evaluated is illuminated with laser light radiating from a point-source, and it is imaged by an image-shearing camera connected to a microcomputer for recording and processing. The camera comprises a CCD image sensor, a lens and an image shearing device. The image shearing device consists of a double-refractive prism and a polarizer. The function of the image shearing device is to produce a pair of laterally displaced (sheared) images, and hence the technique is named as shearography. The principle of image-shearing using a doubly-refractive prism is illustrated in Figure 2 showing that a light beam passing through the prism is split into two angularly separated beams. Conversely, through the image-shearing device, two non-parallel beams of light scattered from two different object points become nearly collinear. Since the spatial frequency of the interference fringe pattern of two beams is proportional to the sine of the half angle between the interfering beams, two nearly collinear beams produce a very low frequency interference pattern that is comfortably resolved by a video image sensor such as CCD.

1



The two sheared wavefronts transmitted by the two axes of the image-shearing device, however, are orthogonally polarized, hence they will not interfere with each other. To enable interference, a polarizer with its polarization axis oriented at an azimuth of 45o is required. As an object surface is generally optically rough, interference of the two sheared wavefronts will result in a speckle pattern embedded in the shearographic image. The speckle pattern is slightly altered when the object is deformed. Two speckle patterns of the test object, one before and another after it is slightly deformed, are digitized into a microcomputer via a frame grabber. As will be shown below, the difference of the two speckle patterns will enable reconstruction of a visible fringe pattern that depicts displacement-derivatives with respect to the direction of image-shearing. Fig. 3 shows a fringe pattern depicting the deflection derivatives of a rectangular plate clamped along its boundaries and loaded by uniform pressure.

Fig. 1 Schematic diagram of digital shearography

Fig. 2 Illustration of the doubly-refractive prism as a shearing device. Two non-parallel rays scattered from two different points on the object are combined and become collinear, resulting in a very low spatial frequency interference pattern.

Fig. 3 Fringe patterns depicting the deflection derivative with respect to x (left) and y (right), respectively, of a plate deformation.

2



NDT Applications:

When an object containing a flaw is loaded, strain concentration at the vicinity of the defect is induced. If the flaw is not too remote from the object surface, the induced strain concentration would cause anomalies in the surface strain distribution. Subsequently, these anomalies are translated into fringe-anomalies if two speckle patterns, taken one before and another after loading, of the object are compared. Thus, shearography reveals flaws, both surface and internal, through identification of anomalies in the fringe pattern. Shearographic nondestructive inspection is full-field and non-contacting.

Shearography vs Ultrasound

Shearography has found wide applications in nondestructive testing and it has already received industrial acceptance as a useful NDT tool, particularly for composite structures such as tires and honeycomb structures. It is particularly effective in revealing delaminations in laminated composites. Fig 4 shows a comparison of test result obtained using digital shearography and C- scan ultrasonic testing on a composite sample. Both techniques readily reveal an edge pullout and a delamination. With digital shearography, the flaws are revealed in less than one second, whilst the ultrasonic technique requires point-by-point scanning along the test surface and at the same time, proper fluid coupling between the transducer and the test surface is to be ensured. A limitation of shearography is the need to apply suitable stress-increments to the test object during inspection, since the underlying principle of this technique is based upon the response of defects to stresses. However, the mechanics of revealing flaw in shearography yields information more relevant to the structural weakness.

Results:

Some examples of nondestructive testing using shearography are illustrated in Fig 4 through Fig. 12.

Fig. 4 Comparison of shearography with C-scan ultrasound in the detection of a delamination and an edge pullout in a composites panel. Time required: around 1 second for shearography and 10 minutes for ultrasound. Moreover, fluid coupling is needed in the ultrasound testing

3



Fig. 5 shows several defects along the steel-belt edge of a truck tyre. A tyre is a very complex composite structure. It is composed of materials with various degree of stiffness ranging from rubber, cord, carbon to steel. Furthermore, the structure undergoes very large deformation. The means of stressing is partial vacuum.

Fig. 6 Two cracks on the interior of a steel pressure vessel was revealed by internal pressurization. The vessel is made of steel and the wall thickness is 10mm.

Crack


4



(a)


(b)


Fig. 7 Evaluation of welding integrity in steel tubes. (a) good weld , (b) bad weld which is characterized by excessive deformation indicated by the denser fringe pattern. The means of stressing is internal pressurization.

Fig. 8 Debonded regions in an adhesively bonded plate structure was revealed by means of vibrational excitation at (a) 2.51 KHz and (b) 8.68 KHz. The structure was supposed to be bonded along the horizontal center region to a rigid structure. A perfectly bonded region should appear as black area in the image. The test shows a debonded region at the middle of the adhesive bond.

Debond


5



Fig. 9 The deformation fringe pattern of a concrete block wall . The local discontinuity in the fringe pattern shows a separation between two concrete blocks. The wall was loaded by a lateral force normal to the wall.

Loosened rivet


Fig. 10 Fringe pattern reveals a loosened bolt in a riveted joint. The loosened rivet is on the right characterized by having fewer fringes on the rivet heads. The specimen was stressed by a uni-axial tension.

6



Fig. 11 Residual Stress Measurement. A hole was drilled to release residual stresses in a specimen, and shearography was used to measure the deformation caused by the stress release. Fringe patterns from top to the bottom show three stress levels in the specimen.

Leak location

Fig. 12 Leak Detection. The fringe pattern reveals leakage of gas from a vessel. The escaping gas is helium which causes a phase change induced by the refractive index change. Shearography not only detects the gas leak but also reveals the leak location.

7



Discussion:

Defect detection

using shearography is based on the response of defects to stresses. The development of shearographic NDT procedures has therefore essentially become the development of a practical means of stressing the object that would readily reveal flaws. Ideally, the stress-increment should be similar to the service stresses so that flaws that are critical and detrimental to the service life of the object would be revealed, and cosmetic flaws that do not undermine the structural integrity of the test object can be ignored. This would minimize unnecessary rejects during inspection. In this regard, shearography has an advantage over ultrasonic testing, as the latter detects flaws by identifying inhomogeneities in the object and does not provide direct information on the criticality of the flaws. Exact duplication of the actual stress-increment for shearographic testing, however, is generally difficult. Therefore, various practical means of stressing the object must be developed. In developing these methods, an important precaution to be taken is restricting rigid-body motion of the object during stressing, as excessive rigid-body motion would cause speckles de-correlation, resulting in degradation of fringe quality. The methods that currently used that do not cause intolerable rigid-body motion of the test object include the use of pressure, vacuum, thermal, and acoustical and mechanical excitations. The use of microwave that excites water molecules is particularly effective for detecting moisture in plastics and non-metallic composites, but safety precautions must be taken seriously.

Conclusions:

A review of shearography and its applications in nondestructive testing is given in this paper. Unlike holography, shearography does not require a reference beam and hence it is more tolerable to environmental disturbances. Indeed, shearography can be employed in field/factory settings. This technique is still relatively young and its full capability awaits further exploration.

Acknowledgement:

The work described in this paper has been supported by the Central Allocation Grant Scheme of the Research Grants Council of Hong Kong, China ( CityU 1/01C)

References:

1. Hung, Y.Y. "Shearography: A New Optical Method for Strain Measurement and Nondestructive Testing", Optical Engineering, pp.391-395, May/June, 1982.

2. Hung, Y.Y. and J.D. Hovanesian,"Fast Detection of Residual Stresses in an Industrial Environment by Thermoplastic-based Shearography", Proceedings of the 1990 SEM Spring Conference on Experimental Mechanics, pp769-775, Albuquerque, New Mexico, June4-6, 1990.

3. Hung, Y.Y. "Digital Shearography and applications" Trends in Optical Non-destructive Testing and Inspection, pp287-308, Elsevier, 2000 (Editors: Pramond K. Rastogi and Daniele Inaudi).

4. Hung, Y.Y. and Shang, H.M. "

A unified approach for holography and shearography in surface deformation measurement and nondestructive testing", Optical Engineering, pp1197-1207, Vol 42 (5), May, 2003.

8