 code | ABSTRACT includes links to Full-Text and Options | MATERIALS CHARACTERIZATION | FULL-TEXT and Options |
|
 2 | USAGE OF BARKHAUSEN EFFECT FOR HARDENING QUALITY CONTROL OF NEAR-SURFACE LAYERS OF TRANSPORT MACHINE PARTS | Michail Budennyy, State Enterprise "malyshev Plant", Ukraine | 267
|
 9 | DAMAGE AND MAGNETIC PARAMETERS OF STEEL AFTER PLASTIC DEFORMATION UNDER HYDROSTATIC PRESSURE | Edward Gorkunov, Institute Of Engineering Science, Russia | 198
|
 12 | QUALITY INSPECTION OF SINTERED TUNGSTEN-COBALT POWDER PRODUCTS BY MAGNETIC TECHNIQUE | Edward Gorkunov, Institute Of Engineering Science, Russia | 220
|
 28 | INFLUENCE OF THE STRUCTURAL RELAXATION ON THE INDENTATION BEHAVIOR OF THE SURFACE OF SILICA OPTICAL FIBER | Rochdi El Abdi, University of Rennes, France | 509
|
 58 | STRESS AND TEXTURE MEASUREMENT USING BARKHAUSEN NOISE AND ANGULAR SCANNING OF DRIVING MAGNETIC FIELD | Valeriy Vengrinovich, Institute of Applied Physics, Belarus | 225
|
 59 | NONDESTRUCTIVE EVALUATION OF SUPERALLOY SPECIMENS WITH A THERMAL BARRIER COATING | Jaap Heida, National Aerospace Laboratory NLR, Netherlands | 768
|
 64 | ULTRASONIC VELOCITY MEASUREMENTS IN ALUMINA-ZIRCONIA CERAMIC COMPOSITE SYSTEM | Hector Carreon, Instituto de Investigaciones Metalurgicas, Mexico | 314
|
 68 | ELECTROMAGNETIC-RESONANCE-ULTRASOUND MICROSCOPY (ERUM) FOR QUANTITATIVE EVALUATION OF LOCALIZED ELASTIC CONSTANTS OF SOLIDS | Hirotsugu Ogi, Osaka University, Japan | 322
|
 71 | COMPARISON OF OPTICAL COHERENCE TOMOGRAPHY AND X-RAY COMPUTED TOMOGRAPHY FOR CHARACTERISATION OF GLAS-FIBRE POLYMER MATRIX COMPOSITES | Johann Kastner, University Of Applied Sciences Upper Austria, Austria | 1278
|
 82 | NONDESTRUCTIVE EVALUATION AND CHARACTERIZATION OF MECHANICAL STRENGTH OF WOOD BASED PANELS USING FOUR DIFFERENT METHODS. | Rolando Coro González, Cidemco Research Centre, Spain |
|
 101 | CHANGE OF ULTRASONIC ATTENUATION AND MICROSTRUCTURE EVOLUTION DURING CREEP OF A STAINLESS STEEL | Toshihiro Ohtani, Ebara Research Co., Ltd., Japan | 260
|
 103 | DEVELOPMENT OF ULTRASONIC AND MICROWAVE TECHNIQUES FOR DETECTION OF DECAY IN WOODEN CROSS-ARMS | Kaida Khalid, Universiti Putra Malaysia, Malaysia | 367
|
 105 | DETERMINATION OF MODULUS OF ELASTICITY OF WOOD BASED PANELS, USING THREE DIRECTIONS ULTRASONIC WAVES AND CANTILEVER BEAM VIBRATIONS. | Rolando Coro González, Cidemco Research Centre, Spain |
|
 106 | RESONANCE ULTRASOUND SPECTROSCOPY FOR EVALUATING ELASTIC CONSTANTS AND INCOHESIVE BONDS OF THIN FILMS | Nobutomo Nakamura, Osaka University, Japan | 189
|
 119 | NONDESTRUCTIVE EVALUATION OF AIRCRAFT AND SPACECRAFT WIRING | Edward Tucholski, U. S. Naval Academy, United States | 605
|
 120 | THE IMPORTANCE OF IMAGING IN NONDESTRUCTIVE CHARACTERIZATION OF MATERIALS | Robert E. Green, Johns Hopkins University, United States | 201
|
 138 | INVESTIGATING THE MICROSTRUCTURE-ULTRASONIC PROPERTY RELATIONSHIPS IN STEELS | C. Hakan Gür, Foundation Techniques Ltd, China | 613
|
 139 | DETERMINING THE IMPACT TOUGHNESS OF AGE-HARDENED 2024 AL-ALLOY BY NONDESTRUCTIVE MEASUREMENTS | C. Hakan Gür, Middle East Technical Univ., Turkey | 461
|
 162 | NON-DESTRUCTIVE ESTIMATION OF MATERIAL STRENGTH BY PRECISE MEASUREMENT OF ULTRASOUND PROPAGATION RATE | Lev B. Zuev, Institute of Strength Physics and Materials Science, Russia |
|
 198 | A CORRELATION STUDY BETWEEN INTERGRANULAR STRAINS AND MAGNETIC PROPERTIES OF MILD STEEL | Roxana Hutanu, Queen's University, Canada | 294
|
 214 | SIMULATION OF IN-SITU CONCRETE CONDITIONS USING A NOVEL ULTRASONIC TECHNIQUE | Abdelmalek Bouhadjera, Univrsity Of Jijel, Algeria | 313
|
 231 | RESIDUAL STRESS ASSESSMENT IN SURFACE-TREATED NICKEL-BASE SUPERALLOYS | Peter Nagy, University of Cincinnati, United States | 278
|
 262 | MICRO CRACK CHARACTERIZATION OF METAL MATRIX COMPOSITES BY 3D-REFRACTION-COMPUTED-TOMOGRAPHY | Bernd Randolf Mueller, Federal Institute For Materials Research And Testing, Germany | 796
|
 271 | EPOXY - FLY ASH COMPOSITES --- A STUDY ON C-SCAN NON DESTRUCTIVE IMAGE PATTERNS, MICROSCOPY AND STRENGTH AS A FUNCTION OF ASH FILLER CONTENT | Anish Kumar, Indian Institute Of Science, India | 1866
|
 304 | USE OF TANGENTIAL RADIOGRAPHY AND RESONANCE ULTRASONIC TECHNIQUES TO EVALUATE BONDING QUALITY | Christophe Schwartz, Cea Centre de Valduc, France | 392
|
 314 | MAGNETIC IMAGING OF CHROMIUM DEPLETION IN THERMALLY SENSITIZED NI-CR-FE ALLOYS | Yasuhiro Kamada, Iwate University, Japan | 320
|
 316 | MAGNETIC EVALUATION OF THE EMBRITLLEMENT ON COLD-ROLLED STEELS | Yasuhiro Kamada, Iwate University, Japan | 201
|
 329 | THE STUDY ON ATTENUATION RULE OF X-RAY AND ? -RAY IN EXPLOSIVE | Chengying Shi; Northwestern Polytechnical University, Xi’an, Shanxi, P.R.China, Xi'an Reserch Inst.of Hi-tech., China | 157
|
 340 | DEFECT SIMULATIONS FOR INTERDENDRITIC STRESS COROSSION CRACKS IN ALLOY 182 WELDS | Per-Håkan Svahn, Sqc, Swedish Qualification Center, Sweden | 756
|
 352 | X-RAY REFRACTION TOPOGRAPHY CHARACTERIZES INTERNAL NANO INTERFACES | Bernd Randolf Mueller, Bam ( Fed. Inst. For Materials Res. & Testing), Germany |
|
 358 | ACOUSTIC EMISSION IDENTIFICATION OF FAILURE MECHANISMS IN FIBER REINFORCED PLASTIC MATERIALS BY NEURAL NETWORKS | Nat Ativitavas, Ptt Public Company Limited, Thailand | 451
|
 363 | NONLINEAR ULTRASONIC SPECTROSCOPY OF FIRED ROOF TILES | Karel Hajek C., Brno University Of Technology,, Czech Republic | 227
|
 370 | CHARACTERIZATION OF METAL FOAMS WITH SYNCHROTRON-TOMOGRAPHY AND 3D IMAGE ANALYSIS | Alexander Rack, Hahn - Meitner - Institut Berlin, Germany | 893
|
 379 | WAVELET ANALYSIS BASED ULTRASONIC NONDESTRUCTIVE TESTING OF POLYMER BONDED EXPLOSIVE | Wei Bin Zhang, Institute Of Chemical Materials, CAEP., China | 206
|
 395 | 1-3 SINGLE CRYSTAL-POLYMER COMPOSITE TRANSDUCERS FOR BROADBAND ULTRASONIC NDT | Sandy Cochran, University Of Paisley, United Kingdom |
|
 426 | MODELLING OF ULTRASONIC BACKSCATTERING DUE TO GRAIN GROWTH IN A WELDED REGION | Håkan Wirdelius, Chalmers Lindholmen University College, Sweden | 3809
|
 437 | ULTRASONIC MATERIAL CHARACTERIZATION SYSTEM EMPLOYING AN ARRAY OF RECEIVING TRANSDUCERS | Serge Titov, Dept. Of Physics, University Of Windsor, Canada | 211
|
 458 | ADHESIVE CURE MONITORING WITH ACOUSTIC METHOD | Ina Severina, University of Windsor, Canada | 1144
|
 471 | INVERSION OF ULTRASONIC ATTENUATION FOR TEXTURAL INFORMATION OF POLYCRYSTALS | Salahuddin Ahmed, Pacific Northwest National Laboratory, United States | 277
|
 495 | EFFECT OF PRECIPITATION HARDENING BY AGING OF 8090 AL-LI ALLOY ON ULTRASONIC PARAMETERS | Venkatachalam Rajendran, Mepco Schlenk Engineering College, India |
|
 504 | A NONDESTRUCTIVE ELECTRICAL METHOD FOR EVALUATING MECHANICAL PROPERTIES OF AL- FOAM | Nahm Seung Hoon, Kongju National University, Korea, South | 483
|
 505 | SIMULATION OF THE ACOUSTIC EMISSION IMPULSE SHAPE VARIATION PROCESS IN METAL | Vladimir Kozharinov, Moscow State University, Russia | 106
|
 528 | QUANTITATIVE ANALYSIS OF SPATIAL PORE-PARTICLE-CORRELATIONS IN METALLIC FOAMS | Astrid Haibel, Hahn-Meitner-Institut, Germany | 689
|
 550 | CONCEPT OF ULTRASONICALLY-BASED MATERIALS CHARACTERIZATION IN NON-CHARACTERIZED ENVIRONMENT | Vjera Krstelj, Faculty Of Mechanical Engineering And Naval Architecture - University Of Zagreb, Croatia | 320
|
 585 | TECHNIQUES FOR HIGH RESOLUTION IMAGING OF WOOD STRUCTURE | Voichita Bucur, INRA - Centre de Nancy, France | 194
|
 616 | CHARACTERISATION OF EPOXY BASED MATERIALS USED IN THE DEVELOPMENT OF ULTRASOUND TRANSDUCERS | Jarlath Mc Hugh, Federal Institute For Material Research And Testing, Bam, Germany | 606
|
 623 | EXPERIMENTAL STUDY AND ANALYSIS OF THE STRUCTURAL NOISE OF THE ULTRASONIC SIGNAL. | Fairouz Bettayeb, Research Center on Welding and Control, Algeria | 712
|
 642 | DEVELOPMENT OF A NON-CONTACTING STRESS MEASUREMENT SYSTEM DURING TENSILE TESTING USING THE ELECTROMAGNETIC ACOUSTIC TRANSDUCER FOR A LAMB WAVE | Riichi Murayama, Fukuoka Institute Of Technology, Japan | 259
|
 654 | ULTRASONIC AND DIELECTRIC MONITORING OF THERMOSET CURE: SENSITIVITY TO PROCESS CONDITIONS. | Richard Challis |
|
 678 | SYNTHETIC FOCUSING FOR IMAGING THE ULTRASONIC BACKSCATTERED NOISE IN DUAL PHASE TITANIUM FORGED PIECES | Christophe Bescond, Cnrc/nrc - Institut Des Matériaux Industriels , Canada | 571
|
 719 | DETECTION OF CENTERLINE SIGMA PHASE IN AL-6XN PLATES VIA NONDESTRUCTIVE METHODS | Kirsten Lipetzky, Naval Surface Warfare Center Carderock Division, United States |
|
 724 | WASPALOY FATIGUE DAMAGE MONITORING USING SAW ACOUSTO-ELASTICITY | Brian O'Neill, University Of Windsor, Canada |
|
 727 | REAL-TIME SENSING OF METALLURGICAL TRANSFORMATIONS BY LASER-ULTRASOUND | Silvio Kruger, National Research Council - Canada, Canada | 228
|
 766 | NONLINEAR ELASTIC WAVE SPECTROSCOPY OF POLYMER SAMPLES WITH LASER INDUCED CRACKS | Zdenek Prevorovsky, Institute of Thermomechanics AS CR, Czech Republic |
|
 768 | STATISTICAL PROCESSING OF A VOLTAGE SIGNAL OF THE MAGNETIC BARKHAUSEN NOISE EMITTED BY QUENCHED AND TEMPERED SPECIMENS OF C45 STEEL | Janez Grum, Faculty of Mechanical Engineering, Slovenia | 465
|
 770 | Calibration of Various Sensor Units by Using Different Parameters of the Magnetic Barkhausen Noise | Janez Grum, Faculty of Mechanical Engineering, Slovenia | 390
|
 784 | HIGH RESOLUTION MICROTOMOGRAPHY AND FAST RADIOGRAPHY FOR REAL-TIME AND IN-SITU CHARACTERIZATION OF POROUS MICROSTRUCTURES | Tilo Baumbach, Fraunhofer Institute for Nondestructive Testing, Germany | 1399
|
 801 | NDT OF LOCAL ELASTIC ANISOTROPY AND DYNAMIC NONLINEARITY OF WOOD | Gerhard Busse, Institute for Polymer Testing and Polymer Science (IKP), Germany |
|
 828 | Lumber Stiffness Prediction Prior To Cant Sawing | Paul Harris | |