 code | ABSTRACT includes links to Full-Text and Options | NEW TECHNIQUES | FULL-TEXT and Options |
|
 56 | MEASUREMENT OF OBJECT SPATIAL DISPLACEMENT BY ULTRASONIC SPECKLE CORRELATION METHOD | Hongmao Zhu, Huazhong University of Science and Technology, China | 254
 |
 72 | NEAR-FIELD MICROWAVE IMAGING OF SUBSURFACE INCLUSIONS IN LAMINATED COMPOSITE STRUCTURES | Mohamed Aboukhousa, American University Of Sharjah, UAE | 146
 |
 73 | QUANTITATIVE RUST-UNDER-PAINT DETECTION UTILIZING NEAR-FIELD MICROWAVE NDE TECHNIQUES | Mohamed Aboukhousa, Concordia University, Canada | 222
 |
 173 | HIDDEN FLAWS MEASUREMENT OF THIN TITANIUM-ALUMINUM BONDED PLATES USING ULTRASONIC TECHNIQUES | Cheng-Chi Tai, National Cheng Kung University, Taiwan | 703
 |
 230 | AN INVESTIGATION INTO THE POTENTIAL OF MICROWAVE NDE FOR MARITIME APPLICATIONS | Graham Green, Qinetiq Ltd, United Kingdom | 542
 |
 246 | NONDESTRUCTIVE EVALUATION OF CRACKS BY AN ULTRASONIC TRANSIT TIMING METHOD. | Junji Takatsubo, National Institute of Advanced Industrial Science and Technology, Japan | 534
 |
 327 | TO THE QUESTION OF BIMETALLIC MATERIALS’ ULTRASONIC TESTING OF “STEEL- BABBIT” TYPE. | Anatoly Sharapov, Jsc "severstal", Russia | 107
 |
 494 | ADVANCEMENT OF THE CLOSELY COUPLED PROBES POTENTIAL DROP TECHNIQUE FOR NDE OF SURFACE CRACKS | Fumio Takeo, Hachinohe National College of Technology, Japan | 288
 |
 510 | DEVELOPMENT OF TECHNOLOGY ULTRASONIC THICK MEASURING AT DYNAMIC MODE | Leonid Yu. Mogilner, Polytest, Russia | 165
 |
 523 | HYDROGEN AS TRACER GAS FOR LEAK DETECTION | Matthias Block, Sensistor Technologies GmbH, Germany | 165
 |
 664 | DEVELOPMENT OF ADVANCED NEUTRON INDUCED PROMPT GAMMA-RAY ANALYSIS SYSTEM FOR SURVEY OF ANTI-PERSONNEL MINES | Tetsuo Iguchi, Nagoya University, Japan | 709
 |
 778 | SUBSURFACE WAVES IN SOLIDS WITH CURVED SURFACE AND ACOUSTICAL IMPEDANCE ON IT | P. Prokhorenko, Institute of Applied Physics, Belarus | 269
 |
 781 | NEW APPROACH TO THE DESCRIPTION OF DEFECTS DEVELOPMENT AT PENETRANT INSPECTION | P. Prokhorenko, Institute of Applied Physics, Belarus | 213
 |