CD-Proceedings
17th World Conference on Nondestructive Testing
25-28 Oct 2008, Shanghai, China
START
FOREWORD
PAPERS
AUTHORS
SEARCH
1. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
1
Magnetic Flux Leakage and Acoustic Emission Testing Technique for Atmospheric Storage tanks
F. Liu, S. Ding, F. Liu
Zhejiang Provincial Special Equipment Inspection and Research Institute, Hangzhou [China]
2
The automated device for leak-testing of nuclear fuel on their manufacturing
I. Loktev
1
, E. Frolov
2
1
JSC Novosibirsk Chemical Concentrates Plant, NCCP, Novosibirsk [Russia]
2
JSC Mashinostroitelny Zavod, Electrostal [Russia]
3
Loose Parts and Valve Flow Monitoring in Nuclear Power Plants Using Integrated Digital Systems
S. Vahaviolos
1
, S. Kattis
2
, M. Carlos
1
1
Physical Acoustics Corporation (PAC), Princeton Junction, NJ [USA]
2
Envirocoustics S.A., Athens [Greece]
4
Application of Acoustic Emission detection Technology on multilayer binding High Pressure Vessel
G. Dai, W. Li, Z. Yang
Daqing Petroleum Institute, Daqing [China]
5
Using Acoustic Emission Technique for Monitoring Real-time Fracture Behavior within Reinforced Concrete Structure Element under Load Test
Y. Kan
1
, K. Pei
2
, D. Lin
2
1
Chao Yang University of Technology, Wufeng, Taichung [Taiwan, China]
2
Institute of Nuclear Energy Research, Taoyuan [Taiwan, China]
6
Identification of Source Time Function for Train-induced Vibration of Underground Tunnels
J. Chai, T. Teng
National Center for Research on Earthquake Engineering (NCREE), Taipei [Taiwan, China]
7
Investigation on Acoustic Emission of Hydrogen Induced Cracking for Carbon Steel Used in Pressure Vessel
G. Shen
1
, L. Li
2
, W. Zhang
2
1
China Special Equipment Inspection and Research Institute, Beijing [China]
2
Hebei University, Baoding [China]
8
The Acoustic Emission Monitoring During the Bending Test of Q235 Steel Box Beam
Z. Wu
1
, G. Shen
2
, S. Wang
2
1
Wuhan University of Technology, Wuhan [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
9
Case Studies of Electric Power Equipment Diagnostics Using Acoustic Emission
O. Santos Filho, S. Zaghetto, G. Pereira
Eletronorte, Belem, PA [Brazil]
10
Application of NDT Procedures for Identification of Fatigue Life Stages of AlMg Alloys
P. Liskutin
1
, P. Mazal
1
, J. Fiala
2
1
Brno University of Technology, BUT, Brno [Czech Republic]
2
University of West Bohemia, Plzen [Czech Republic]
11
AE Intelligent Sensor Networks System Used in Tele-Monitoring of Civil Engineering
G. Tong
1
, F. Kong
2
, R. Wang
3
1
Chinese Academy of Sciences, Shanghai [China]
2
Shanghai ORDA Optoelectronic Science & Technology Co. Ltd, Shanghai [China]
3
Eletronorte, Belem, PA [Brazil]
12
Acoustic Emission Transferability using Transfer Function
A. Prateepasen, M. Srinang
King Mongkut’s University of Technology Thonburi, Bangkok [Thailand]
13
Non-destructive testing:the guarantee of the success of full scale aircraft fatigue test
R. Geng
Beijing Aeronautical Technology Research Center, Beijing [China]
14
Acoustic Emission in-service detection of cryogenic storage tank floors
Y. Xu, S. Ding, F. Liu
Zhejiang Provincial Special Equipment Inspection and Research Institute, Hangzhou [China]
15
Feature extraction of acoustic emission signals from low carbon steel pitting Based on Independent component analysis and wavelet transforming
W. Li, G. Dai, F. Long
Daqing Petroleum Institute, Daqing [China]
2. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
16
Borescope and Eddy Current Dual Probe for in Situ Detecting Cracks in an Aeroengine Labyrinth Disc
W. Tian, M. Pan, F. Luo
National University of Defense Technology, Changsha [China]
17
NDT as a tool, for Post-Irradiation Examination
A. Alghem, M. Kadouma, R. Benaddad
Nuclear research center of Birine/COMENA, Djelfa [Algeria]
18
Progress in NDT system engineering through sensor physics and integrated efficient computing
M. Kröning
1
, J. Ribeiro
2
, A. Vidal
3
1
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
2
Centro de Avaliacao Nao Destrutiva (CAND), Rio de Janeiro [Brazil]
3
Pontifica Universidade Catolica PUC, Rio de Janeiro [Brazil]
19
Eddy current and ultrasound data fusion applied to Carbon Fiber Reinforced Plastic evaluation
A. Savin, R. Steigmann, N. Iftimie
National Institute of R&D for Technical Physics, Iasi [Romania]
20
A Radio-frequency Measurement System for Metallic Object Detection Using Pulse Modulation Excitation
Y. Li, G. Tian
University of Newcastle, Newcastle upon Tyne [United Kingdom]
21
Ultrasonic and eddy current inspection of rail wheels and wheel set axles
B. Rockstroh, W. Kappes, F. Walte
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
3. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
22
Inspection and Identification of Inner-Outer Defects on Oil-Gas Pipeline
L. Yang
1
, G. Liu
1
, G. Zhang
2
1
Shenyang University Of Technology, Shenyang [China]
2
Shenyang Institute of Chemical Technology, Shenyang [China]
23
Status of the Thai Society for Nondestructive Testing and NDT in Thailand
A. Prateepasen, M. Srinang, M. Noypitak
King Mongkut’s University of Technology Thonburi, Bangkok [Thailand]
24
Data Fusion for Combining Techniques to in Situ Detect Defects of Turbine Blade
W. Tian, M. Pan, F. Luo
National University of Defense Technology, Changsha [China]
25
Adhesive bond testing by laser induced shock waves
M. Arrigoni, S. Kruger, J. Monchalin
National Research Council of Canada (NRC), Boucherville, Quebec [Canada]
26
Thermal performance of lead-free microelectronic BGA package with defects
H. Shang, J. Gao, I. Nicholson
Welding Institute (TWI Ltd), Port Talbot [United Kingdom]
27
Characterization of Impact Test Response of PCCP with System Identification Approaches
Z. Liu, A. Wang, D. Krys
National Research Council Canada (NRC), Ottawa, Ontario [Canada]
28
Monitoring of concrete Components Structure Condition Using Nonlinear Ultrasonic Spectroscopy
M. Korenská, M. Matysík, M. Manychova
Brno University of Technology, BUT, Brno [Czech Republic]
29
Opportunities and Challenges of Effective Inspection Industry in Nigerian Petroleum Sector
M. Adegbite, O. Erhimona
Petroleum Training Institute, Effurun, Delta State [NIGERIA]
30
Basic Principles of the Construction of Residual Resource Estimation Systems
V. Klyuev, M. Filinov, A. Fursov
JSC, SPECTRUM-RII, Moscow [Russia]
31
Research on Application of Pipe Crawling Device
B. Li, J. Zhang, B. Li
China Special Equipment Inspection and Research Institute, Beijing [China]
32
On the Nondestructive Evaluation of Composite Structures by Liquid-Crystal Thermography
H. Rezghi Maleki
1
, A. Afaghi Khatibi
2
, F. Honarvar
3
1
Bonab University, Bonab [Iran]
2
University of Tehran, Theran [Iran]
3
K. N. Toosi University of Technology, Tehran [Iran]
33
Firmware System for diagnostics of the mill rolls
A. Nichipuruk
1
, S. Murikov
2
, A. Stashkov
1
1
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
2
Research-Training Center (RTC), Magnitogorsk [Russia]
34
Why Not Enlarge the Non-Destructive Testing (NDT) Experience in Construction Maintenance - Problems, Practice, Ideas etc.?
V. Vladimirov
Sofia University St. Kliment Ohridski, Sofia [Bulgaria]
35
Problems of image restoration in metallography
M. Filinov, V. Bykov, A. Maslov
JSC, SPECTRUM-RII, Moscow [Russia]
36
A Novel Approach for Nonlinear Distortion Correction of Industrial Endoscope Images
H. Sun, Y. Zhang, F. Luo
National University of Defense Technology, Changsha [China]
37
Increased inspection productivity through advances in Remote Visual Inspection (RVI)
E. Hubben
1
, B. Morse
1
, C. Murner
2
1
GE Inspection Technologies, Skaneateles, NY [USA]
2
GE Inspection Technologies, Lewistown, PA [USA]
38
Study on the Penetration Theory of Flaw
X. Li
1
, P. Zhang
1
, Y. Pu
2
1
Laboratory of Jianshe Industry group, Chongqing [China]
2
Chongqing University, Chongqing [China]
39
Performance Based Qualification for NDT
M. Turnbow
Tennessee Valley Authority, Soddy Daisy [USA]
40
The Advent of Age with Integrated NDT Technology
J. Lin
Eddysun Electronic Co. Ltd., Xiamen [China]
41
Fault Indication Film Used in Magnetic Nondestructive Testing
B. Liu
Beijing Jinkeguang Technology Co. Ltd., Beijing [China]
42
Dynamic Strain Measurement Using Improved Bonding Fiber Bragg Grating
G. Hwang, C. Ma
National Taiwan University , Taipei [Taiwan, China]
43
Help Software Design of NDT Instrument Based on FLASH Cartoon
J. Lin
1
, H. Li
2
, Z. Cai
2
1
Eddysun Electronic Co. Ltd., Xiamen [China]
2
Jimei University, Xiamen [China]
44
Recent Advances in NDE Technologies for Turbines and Generators
W. Abbasi, M. Metala
Siemens Power Generation USA, Pittsburgh [USA]
45
POD Generator, Development of numerical modeling tools for quantitative assessment of the performance of non-destructive inspection techniques
A. Mast, A. Volker, J. Bloom
TNO Science & Industry, Delft [Netherlands]
46
Nondestructive Elastic-Wave Tests of Post-tensioned Concrete Girders in Road Bridge
K. Schabowicz, J. Hola
Wroclaw University of Technology, Wroclaw [Poland]
47
Mechanical characterization of porous structures by the combined use of micro-CT and in-situ loading
G. Kerckhofs, J. Schrooten, M. Wevers
Katholieke Universiteit Leuven, Heverlee [Belgium]
48
Automated MPI Test Fluid Quality Checks and Dye Penetrant Tam Panel Tests
T. Vetterlein
1
, M. Wagener
2
, H. Rongen
2
1
ITW TIEDE GmbH, Essingen [Germany]
2
Forschungszentrum Jülich, Jülich [Germany]
49
NDT certification procedure at hazardous production facilities
N. Konovalov, V. Shevchenko, O. Kochetkova
STC "Industrial Safety", Moscow [Russia]
50
Personnel Certification and Qualificatioin By the Independent Certification Body "SPEKTRCert" of JSC "MSIA "SPECTRUM"
I. Pushkina, D. Glotov, G. Tarasenko
SPEKTR-GROUP Association, Moscow [Russia]
51
ISO 17020 Accreditation of CNETSTEN NDT Laboratory Part 1
K. Sahaimi, A. Bensitel, S. Mimount
CNESTEN, Rabat [Morocco]
52
Energy in the future - new challenges for NDT
M. Farley
Doosan Babcock Energy Limited, Renfrew [United Kingdom]
53
EFNDT Guidelines on the overall NDT quality system in Europe
M. Farley
Doosan Babcock Energy Limited, Renfrew [United Kingdom]
54
DEVELOPMENT and IMPLEMENTATION of a SPECIFICATION for AUTHORISED QUALIFYING BODIES
J. Thompson
British Institute of Non-Destructive Testing,BINDT, Northampton [United Kingdom]
55
Non-destructive Testing of Mechanical Parameters for Wood-based Materials
Y. Hu
Northeast Forestry University, Harbin [China]
56
Analysis of the Relationship between the Limit Load of Structure and the Microscopic Character
G. Jiang
1
, Y. Zhang
1
, L. Sun
2
1
Beijing University of Technology, Beijing [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
57
Estimation of wall thinning defect size and location in pipes by Laser Speckle Interferometry
K. Kim, J. Park, H. Jung
Chosun University, Gwangju [Korea]
58
Soft Calibration Method to Uncertainty of Measurement About Nondestructive Quantitative Testing
L. Yao
China Air-Dynamic Research and Development Center, Mianyang [China]
59
TD Handy-Scan, a New Alternative in Hand Held Advanced Ultrasonic Equipment
M. Nel
AGR Technology Design, Winsford [United Kingdom]
60
ARM9-Based High Speed Multi-channels Eddy Current and Ultrasonic Testing System
Z. Zhang
1
, L. Zhao
2
1
Eddysun Electronic Co. Ltd., Xiamen [China]
2
Nanchang Hang Kong University, Nanchang [China]
61
Method for Dynamic State Monitoring of Pressure Vessel
X. Ma
Pressure Vessel Testing Center, Mianyang [China]
62
NDT Equipment Rental Practice
H. Hu, D. He
GE Inspection Technologies, Shanghai [China]
63
NDT Personnel Certification in Accordance with European and International Standards
G. Batov, N. Biryukova
STC, Kachestvo, LTD, Moscow [Russia]
64
The inspection system for mechanical non-destructive of NPPs type VVER steam generator tube sheet inspection.
M. Kuna, J. Plášek, P. JablonickÝ
VUJE a.s., Trnava [Slovak Republic]
65
NDT of Lattice Sandwich Metal Plate by Using DC Potential Drop Method
D. Zhang, Z. Chen, S. Xie
Xi'an Jiaotong University, Xi'an [China]
66
Fiber Bragg Gratings and Two Wave Mixing Spectral Demodulator System for Impact Detection and Localization
G. Kirikera, O. Balogun, S. Krishnaswamy
Northwestern University, Evanston, IL [USA]
67
Comments Toward the Harmonization of Qualification and Certification of Non-Destructive Testing Personnel in Arab Countries
W. Harara
Atomic Energy Commission of Syria, Damascus [Syria]
68
Low-frequency magnetic current features
B. Liu
Beijing Jinkeguang Technology Co. Ltd., Beijing [China]
69
Instrumental Technique for the Detection and Identification of Radioactive, Fissible and Extrahazardous Substances
N. Kuzelev, I. Ivanov, V. Yumashev
Russian National Technical Physics and Automation research Institute, VNIITFA, Moscow [Russia]
70
Imaging of internal cracks in concrete structures using the VOLUME rendering technique
P. Liu, P. Yeh
National Taiwan University , Taipei [Taiwan, China]
4. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
71
Advanced NDT with high resolution Computed Tomography
T. Paul, Z. He
phoenix x-ray Systems + Services GmbH, Wunstorf [Germany]
72
Quality Evaluation for the Digital Radiography Inspection Based on Imaging Parameters
F. Kong
GE Inspection Technologies, Shanghai [China]
73
On the Detection of Inhomogeneities in Steel by Computed Tomography
B. Harrer
1
, J. Kastner
1
, H. Degischer
2
1
Upper Austrian University of Applied Sciences, Wels [Austria]
2
Vienna University of Technolog, Vienna [Austria]
74
True 3D-CT-reconstruction in comparison to the FDK-algorithm
A. Lange, M. Hentschel, A. Kupsch
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
75
Algebraic Reconstruction Technique Class for Linear Scan CT of Long Object
B. Liu, L. Zeng, D. Ji
Chongqing University, Chongqing [China]
76
A De-Convolution Technique used for NDT in X-ray & CT.
K. Chui, D. Stanfield, A. Wride
Image Enhancement Technology Ltd, Uxbridge [United Kingdom]
77
aRTist - Analytical RT Inspection Simulation Tool for Industrial Application
G. Jaenisch, C. Bellon, U. Ewert
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
78
Radiographic and Tomographic Inspection of Wooden Specimens with Fission Neutrons
K. Osterloh
1
, T. Bücherl
2
, A. Hasenstab
3
1
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
2
Technische Universität München, Garching [Germany]
3
TÜV Rheinland, LGA, Nürnberg [Germany]
79
X-ray detection and data acquisition for NDT applications
M. Homer, S. Jaye
Sens-Tech Ltd, Ruislip [United Kingdom]
80
Real-time Radiographic Non-destructive Inspection for Aircraft Maintenance
X. Wang
1
, B. Wong
1
, C. Tui
2
1
Nanyang Technological Univ., Singapore [Singapore]
2
Republic of Singapore Air Force, Singapore [Singapore]
81
3D Image Reconstruction from Low Energy and Noisy X-ray Projection Data
V. Vengrinovich, S. Zolotarev, I. Reshetouski
National Academy of Sciences of Belarus, Minsk [Belarus]
82
X-Ray Net Weight Control of Pharmaceutical Products
F. Bessler, W. Bauer
Robert Bosch GmbH - Corporate Research, Stuttgart [Germany]
83
Realization and application of simulation technology in Direct Radiography
C. Sun, G. Tang, Z. Wang
China Academy of Engineering Physics, CAEP, Mianyang [China]
84
Scan and Reconstruction of Helical Cone-beam Industrial CT for Big Workpiece
X. Zou, L. Zeng
Chongqing University, Chongqing [China]
85
Segmentation of Casting Defects in X-Ray Images Based on Fractal Dimension
J. Wang, X. Hou, Y. Cai
Chongqing University, Chongqing [China]
86
Optimization Research on Weld Image Based on Computed Radiography System
M. Zheng
1
, K. Ding
2
, G. Chen
2
1
Beijing Jiaotong University, Beijing [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
87
Ridgelet Compression Method of Luggage X-ray Inspection Images
Z. Li, L. Zeng, R. Zhou
Chongqing University, Chongqing [China]
88
Real-time X-ray Image Processing Based on Information Fusion for Weld Defects Detection
D. Du , R. Hou, J. Shao
Tsinghua University, Beijing [China]
89
Industrial ray DR/ICT integrated inspection testing system (1) Hardware system
K. Ding
1
, L. Liang
1
, J. Fu
2
1
China Special Equipment Inspection and Research Institute, Beijing [China]
2
Beijing University of Aeronautics and Astronautics, Beijing [China]
90
A Method of weld Edge Extraction in the X-ray Linear Diode Arrays Real-time imaging
G. Chen, K. Ding, L. Liang
China Special Equipment Inspection and Research Institute, Beijing [China]
91
Structural Index of Metal Matrix Composites Evaluated with Computed Tomography
J. Goebbels
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
92
Segmentation of Weld Defects in X-ray Image Based on Partial Surface Reconstruction
R. Hou, D. Du , J. Shao
Tsinghua University, Beijing [China]
93
Digital Comparisons in Oil & Gas
J. Zekoski, J. Costain
GE Inspection Technologies, Lewistown, PA [USA]
94
Referenceless Beam Hardening Correction in 3D Computed Tomography Images of Multi-Material Objects
M. Krumm, S. Kasperl, M. Franz
Fraunhofer Institute for Integrated Circuits (IIS), Fürth [Germany]
95
The Multi-Sensor Tomolibri® - Measurements with Computed Tomography (CT)
S. Kasperl
1
, M. Maisl
2
, D. Neumayer
3
1
Fraunhofer Institute for Integrated Circuits (IIS), Fürth [Germany]
2
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
3
Fraunhofer Institut Produktionstechnik und Automatisierung, Stuttgart [Germany]
96
Image Registration Combining Digital Radiography and Computer-Tomography Image Data
F. Herold
YXLON International X-Ray GmbH, Hamburg [Germany]
97
Industrial Ray DR/ ICT integration inspection testing system (2) Software and Testing
L. Liang
1
, K. Ding
2
, K. Ding
1
1
China Special Equipment Inspection and Research Institute, Beijing [China]
2
Beijing Jiaotong University, Beijing [China]
98
Enhanced Spatial Resolution in 2D CT-Reconstruction without Filtered Back-Projection: DIRECTT
A. Kupsch, A. Lange, M. Hentschel
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
99
Digital Radiography in Industry
W. Harara
Atomic Energy Commission of Syria, Damascus [Syria]
100
Study on the density characterization of the CT image
H. Chen, S. Yang
The 213th Research Institute of China Ordnance Industry, Xi'an [China]
101
Method for three-dimensional evaluation and visualisation of the distribution of fibres in glass-fibre reinforced injection molded parts by µ-X-ray computed tomography
F. Pfeifer
1
, J. Kastner
1
, R. Freytag
2
1
Upper Austrian University of Applied Sciences, Wels [Austria]
2
Transfercenter für Kunststofftechnik GmbH, Wels [Austria]
102
Digital Radiography and its Advantages in Field NDT Inspections Today
R. Pincu
Vidisco Ltd., Or-Yehuda [Israel]
103
CT Reconstruction with Good-Orientation and Layer Separation for Multilayer Objects
T. LIU
1
, B. Wong
2
, T. Chai
3
1
Singapore Institute of Manufacturing Technology, Singapore [Singapore]
2
Nanyang Technological Univ., Singapore [Singapore]
3
Institute of Microelectronics, Singapore [Singapore]
5. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
104
Effect of Lift-off on Pipeline Magnetic Flux Leakage Inspection
L. Yang
1
, G. Zhang
2
, G. Liu
1
1
Shenyang University Of Technology, Shenyang [China]
2
Shenyang Institute of Chemical Technology, Shenyang [China]
105
Increased Use of Remote Field Technology for in-line Inspection of Pipelines Proves the Value of the Technology for this Application
D. Russell, V. Shen
Russell NDE Systems Inc., Edmonton [Canada]
106
New Techniques for the Quantification of Defects Through Pulsed Magnetic Flux Leakage
J. Wilson, M. Kaba, G. Tian
University of Newcastle, Newcastle upon Tyne [United Kingdom]
107
Resolution of Magnetic Intelligent Tool in Case of Stress-corrosion Cracks Detection
A. Kovalenko
Avtogaz JSC, Moscow [Russia]
108
Smart Two Wire Vibration Switch - New Class of Monitoring Device
G. Zusman
VibraSpectrum Ltd., Moscow [Russia]
109
AC Conductivity of Non Magnetic Metallic Alloys
F. Fraudita, C. Gonzalez, A. Gallipoli
Universidad Central de Venezuela, Caracas [Venezuela]
110
Eddy Current Non-Destructive Testing Application Research of Marine Engines
Z. Cai
1
, H. Li
1
, J. Lin
2
1
Jimei University, Xiamen [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
111
Study on ET Technique to Measure Oxide Thickness of Rods for PWR
D. Li
1
, J. Xiong
1
, J. Lin
2
1
Nuclear Power Institute of China (NPIC), Chengdu [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
112
Geometry Parameters Estimation of Defects in Multi-layered Structures Based on Eddy Current Nondestructive Testing Technique with Bayesian Networks
B. Ye, P. Huang, M. Fan
Zhejiang University, Hangzhou [China]
113
3D Magnetic Field Responses to a Defect Using a Tangential Driver-coil for Pulsed Eddy Current Testing
Y. Zhang, H. Sun, F. Luo
National University of Defense Technology, Changsha [China]
114
Development and Application of Pulsed Eddy Current Testing System for Ferromagnetic Pipes
C. Huang
1
, X. Wu
1
, S. Lin
2
1
Huazhong University of Science and Technology, Wuhan [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
115
Magnetic Field Mapping for Complex Geometry Defect - 3D Transient Problem
I. Zainal abidin, G. Tian, Y. Li
University of Newcastle, Newcastle upon Tyne [United Kingdom]
116
Detection of wire disconnection using new rope tester
Y. Hirama
1
, H. Wakiwaka
2
, K. Tashiro
2
1
Non-Destructive Inspection Consulting Engineer, Tamiya Cho, Ushiku [Japan]
2
Shinshu University, Nagano [Japan]
117
Characterization of Carbon Fibre Reinforced Composite by Means of Non-Destructive Eddy Current Testing and FEM Modeling
X. Li, W. Yin, A. Peyton
University of Manchester, Manchester [United Kingdom]
118
Eddy Probe System on the Basis of New Technology
A. Kirpichev
1
, P. Shkatov
2
, A. Klushev
1
1
GlobalTest, Sarov [Russia]
2
Moscow state university of instrument making and informatic, Moscow [Russia]
119
Simulator for Education of Eddy Current Testing Specialists
P. Shkatov, D. Bydanov, S. Kluyev
Moscow state university of instrument making and informatic, Moscow [Russia]
120
Electromagnetic health monitoring of BSCC prosthetic heart valves
R. Grimberg
1
, S. Chan
2
, A. Savin
1
1
National Institute of R&D for Technical Physics, Iasi [Romania]
2
Michigan State University, East Lansing, MI [USA]
121
A Detection Method for the Fuel Balls Passing through the Pipeline of Pebble-Bed High Temperature Gas Cooled Reactor
Z. Han , K. Yuan, L. Zhang
Tsinghua University, Beijing [China]
122
The Important Role of Eddy Current Testing in Railway Track Maintenance
A. Dey, H. Thomas, R. Pohl
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
123
Research on Surface Defect Detection Using Pusled Eddy Current Testing Technology
D. Zhou
1
, B. Zhang
1
, G. Tian
2
1
Nanjing University of Aeronautics and Astronautics, Nanjing [China]
2
University of Newcastle, Newcastle upon Tyne [United Kingdom]
124
Recognition and Improvement in the Classification of Imperfections Detected by Eddy Current Inspection
F. Lesage, X. Guo, B. Bisiaux
CEV – V&M France – Vallourec Group, Aulnoye-Aymeries [France]
125
High Resolution Eddy current testing of superconducting wires using GMR sensors
M. Kreutzbruck
1
, K. Allweins
2
, H. Bernau
2
1
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
2
University of Giessen, Giessen [Germany]
126
Modelling of Eddy Current inspections with CIVA
C. Gilles-Pascaud, G. Pichenot, C. Reboud
Commissariat Energie Atomique (CEA), Gif-Sur-Yvette [France]
127
3D Finite Element Analysis of Marine Steel Plate Magnetic Leakage Testing
H. Li
1
, J. Lin
2
, Z. Cai
1
1
Jimei University, Xiamen [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
128
Eddy Current Measurement of Case Hardened Depth of Steel Components
J. Cuffe
1
, H. Sun
2
, Y. Plotnikov
2
1
GE Inspection Technologies, Lewistown, PA [USA]
2
GE Global Research, Niskayuna NY [USA]
129
Advances in Eddy Current Array Sensor Technology
J. Bureau, R. Ward, W. Jenstead
GE Inspection Technologies, Lewistown, PA [USA]
130
The First 20 Years of the A.C. Field Measurement Technique
M. Lugg
TSC Inspection Systems, Milton Keynes [United Kingdom]
131
Eddy Current Tools for Education and Innovation
G. Mook, J. Simonin
University of Magdeburg, Magdeburg [Germany]
132
Electromagnetic Imaging using Probe Arrays
G. Mook, F. Michel, J. Simonin
University of Magdeburg, Magdeburg [Germany]
133
Development of Automated Electromagnetic Techniques for Inspecting Inner Cracks of LPG Tanks
Y. Wu, F. Hsieh, M. Peng
Industrial Technology Research Institute, Taiwan [Taiwan, China]
134
Research & Development of Integrated MMM/EC/MFL Testing System
J. Lin
1
, F. Lin
2
, C. Lin
2
1
, []
2
Eddysun Electronic Co. Ltd., Xiamen [China]
135
High-Precision Internal Diameter Measurement Using Eddy Current Arrays
B. Lepage
1
, S. Labbé
1
, D. Katz
2
1
Olympus NDT, Waltham, MA [USA]
2
US Army ARDEC, Picatinny, N.J. [USA]
136
Impedance Evaluation of a Probe-Coil's Lift-off and Tilt Effect in Eddy-Current Nondestructive Inspection by 3D Finite Element Modeling
Y. Zhang, F. Luo, H. Sun
National University of Defense Technology, Changsha [China]
137
Optimization of structure and operation algorithms for electromagnetic plated coatings thickness meters with the use of digital technologies
V. Syasko, A. Bulatov, I. Pivovarov
Constanta ltd, St-Petersburg [Russia]
138
Detection of Hidden Flaws with GMR-based Eddy Current Technique
J. Na
University of Dayton, Dayton, OH [USA]
139
The MFL technique for surface flaws of the weld zone with residual magnetization method
N. Kasai, H. Koshino, K. Sekine
Yokohama National University, Yokohama [Japan]
140
Three Modeling Methods in MFL Testing
Z. Huang, P. Que
Shanghai Jiaotong University, Shanghai [China]
141
Encircling ET Inspection on Corrugated Tubes Destined to Gas Tubes for EGR Heat Exchanger
B. Bisiaux
1
, P. Gerard
2
, M. Lopes
3
1
CEV – V&M France – Vallourec Group, Aulnoye-Aymeries [France]
2
Valtimet - Vallourec Group, Aulnoye-Aymeries [France]
3
Changzhou Carex Valinox Components Co. Ltd, Aulnoye-Aymeries [China]
142
An Holistic Approach to Automatic Classification of Steel Plate Corrosion Defects using Magnetic Flux Leakage
A. Romero ramirez, N. Pearson, J. Mason
Swansea University, Swansea [United Kingdom]
143
Development of Instruments for NDT of Rail-Tracks with Use of Contactless Electromagnetic Acoustic Emission Transducers (EMATs)
V. Gordely, V. Gordely
VIGOR, Moscow [Russia]
144
3D Finite Element Analysis of Marine Steel Plate Magnetic Leakage Testing
H. Li
1
, Y. He
2
, J. Lin
1
1
Jimei University, Xiamen [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
145
A Novel NDT Method for Measuring Thickness of Brush-Electroplated Nickel Coating on Ferrous Metal Sueface
S. Dong
1
, B. Xu
1
, J. Lin
2
1
Academy of Armored Forces Engineering, Beijing [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
146
To Identify the weaknesses of concrete from GPR images with employing evolution curve model
Y. Huang, S. Hus, S. Lin
Chao Yang University of Technology, Wufeng, Taichung [Taiwan, China]
147
Numerical Simulation and Experiment on Magnetic Flux Leakage Inspection of Cracks in Steels
Y. Wang, Y. Xu, S. Ding
Zhejiang Provincial Special Equipment Inspection and Research Institute, Hangzhou [China]
148
Array Pulsed Eddy Current Imaging Technique for Nondestructive Testing of Aging Aircraft
F. Luo, Y. He, B. Yang
National University of Defense Technology, Changsha [China]
149
Microwave Measurement and Quantitative Evaluation of Wall Thinning in Metal Pipes
Y. Ju, L. Liu, M. Ishikawa
Nagoya University, Nagoya [Japan]
150
Health status of ancient buildings: interferometric radar NDT inspection
R. Garziera, M. Amabili, L. Collini
University of Parma, Parma [Italy]
151
Impedance Tomography and Conductivity Stratification of Cold Rolled Recrystaliced Aluminum Alloy
C. Gonzalez, F. Fraudita, A. Gallipoli
Universidad Central de Venezuela, Caracas [Venezuela]
152
Simulation of magnetic field distribution of excitation coil for EM flow meter and its validation using magnetic camera
J. Wang, G. Tian, A. Simm
University of Newcastle, Newcastle upon Tyne [United Kingdom]
153
New Method of Investigation of Rising Damp in Brick Walls by means of Impedance Tomography
J. Hola, Z. Matkowski, K. Schabowicz
Wroclaw University of Technology, Wroclaw [Poland]
154
The difference among three reference standards used in the performance evaluation of wire rope EMT instrument
H. Chen
1
, Y. Kang
2
, J. Ruan
1
1
Wuhan University, Wuhan [China]
2
Huazhong University of Science and Technology, Wuhan [China]
155
The Fluorescene Penetrant Agent Manufacture and Its Wastewater Treatment
Z. Lin
1
, Z. Chen
1
, D. Li
2
1
Xiamen Chemical Industry Machinary Plant, Xiamen [China]
2
Honeywell TAECO Aerospace (Xiamen) Co. Ltd, Xiamen [China]
156
A breakthrough in high-speed digital eddy current testing technology
A. Gopalan, M. Junger
Rohmann GmbH, Frankenthal [Germany]
157
Buried Corrosion Detection in Multi-layer Airframe Structures Using Pulsed Eddy Current
C. Murner
1
, J. Hansen
2
1
GE Inspection Technologies, Lewistown, PA [USA]
2
GE Inspection Technologies Ltd., St. Albans [United Kingdom]
158
Adaptive Eddy Current Flaw Detectors
P. Shkatov, G. Didin, V. Garipov
Moscow state university of instrument making and informatic, Moscow [Russia]
159
A Novel Self-Compensating GMR-Based Eddy Current Probe for Hidden Crack Detection
M. Fan, P. Huang, B. Ye
Zhejiang University, Hangzhou [China]
160
Recent Developments of Multi-elements Eddy Currents Probes
B. Marchand, J. Decitre, O. Casula
Commissariat Energie Atomique (CEA), Gif-Sur-Yvette [France]
161
The Design of High Strength Bolts Scanning Testing Imaging System Based on the Eddy Current Array Probe
M. Lou, Y. Guo
Shanghai research institute of materials, Shanghai [China]
162
Determination of Metallic Fatigue in Nitrided Steel using a MDK Magnetic Nondestructive Tester
A. Onuki
1
, H. Kohama
2
1
Yamagata University (Formerly), Yonezawa-shi,Yamagata [Japan]
2
Kaisei Engineer Co. Ltd, Yamato-shi, KANAGAWA [Japan]
163
Automatic Differential Lift-off Compensation (AD-LOC) Method in Pulsed Eddy Current Inspection
J. Qiao, J. Hansen, I. Mayes
GE Inspection Technologies Ltd., St. Albans [United Kingdom]
164
Numerical Value Analysis of Eddy Current Probe Coil of Placement Model Based on ANSYS
J. Yu, J. Ren, J. Tang
Nanchang Hang Kong University, Nanchang [China]
165
An Iterative Phase Difference Detection Method for High Sensitivity Eddy Current Sensor
T. Tsujisawa
1
, K. Yamakawa
2
, K. Abe
2
1
Ashikaga Institute of Technology, Ashikaga [Japan]
2
Azuma Systems Corporation, Kumagaya [Japan]
166
Practice of Inline Pipeline Inspection with MDSCAN Intelligent Pigs
D. Slesarev
1
, D. Sukhorukov
1
, E. Vasin
2
1
Intron Plus Ltd., Moscow [Russia]
2
Diascan, Lukhovitsy [Russia]
167
Electromagnetic on-Line Testing of Rolled Products and Tubes. Problems and Solutions
Y. Fedosenko
JSC, SPECTRUM-RII, Moscow [Russia]
168
Electromagnetic sensors array for the determination of soil condition
R. Grimberg, A. Savin, R. Steigmann
National Institute of R&D for Technical Physics, Iasi [Romania]
6. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
169
Modeling and analysis of the influence of heating parameters on surface temperature signals
Y. Liu
1
, X. Guo
2
, G. Guo
1
1
Beijing Institute Of Aeronautical Materials, Beijing [China]
2
Beihang University, Beijing [China]
170
Defect detection of Al specimen of using Lock-in photo-infrared thermography technique
K. Kim, H. Kim, M. Kim
Chosun University, Gwangju [Korea]
171
Computerized Portable Eddy-Current Flaw Detectors
V. Muzhitsky, A. Efimov, A. Shubochkin
JSC, SPECTRUM-RII, Moscow [Russia]
172
Infrared Thermal Wave Nondestructive Evaluation for Antioxide Coating on Metal Substrate
Y. Li
1
, Y. Zhao
1
, C. Zhang
2
1
Beijing Institute of Technology, Beijing [China]
2
Capital Normal University, Beijing [China]
173
Ultrasonic Infrared Thermal Wave Technology and its Applications in Nondestructive Evaluation
D. Chen, C. Zhang, L. Feng
Capital Normal University, Beijing [China]
174
Thermographic Evaluation of Aircraft Composite Materials
B. Wong
1
, C. Tui
2
, W. Bai
1
1
Nanyang Technological Univ., Singapore [Singapore]
2
Republic of Singapore Air Force, Singapore [Singapore]
175
Euclidean Distance Based Color Image Segmentation Algorithm for Dimensional Characterization of Lack of Penetration from Weld Thermographs for on-Line Weld Monitoring in GTAW
B. Rani, N. Nandhitha, N. Manoharan
Sathyabama University, Chennai [India]
176
Fatigue Crack Detection by Ultrasound Infrared Thermography
M. Choi, K. Kang, S. Lee
Korea Research Institute of Standards and Science, Daejeon [Korea]
177
Induction Thermography as a Tool for Reliable Detection of Surface Defects in Forged Components
U. Netzelmann, G. Walle
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
178
Finite Element simulation and Experimental verification of Infrared Thermal Wave Non-destructive Inspection for the Defects in Welded Joint
S. Zhao
1
, C. Zhang
1
, Y. Li
2
1
Capital Normal University, Beijing [China]
2
Beijing Institute of Technology, Beijing [China]
179
Detection of Defects in Composite Pyrotechnic Materials and Products by IR NDT Methods
W. Swiderski, M. Miszczak
Military Institute of Armament Technology, Zielonka [Poland]
180
Infrared Thermal Wave Nondestructive Testing for Cf /SiC Ceramic Matrix Composite
Y. Duan
1
, X. Zhang
2
, C. Zhang
2
1
Beijing University of Aeronautics and Astronautics, Beijing [China]
2
Capital Normal University, Beijing [China]
181
An IR Lock-in Thermography Nondestructive Test System Based on the Image Sequence Processing
J. Liu, J. Dai, Y. Wang
Harbin Institute of Technology, Harbin [China]
182
Finite Element Method Applied to Thermal Nondestructive Characterization of Delamination in the Dam Structure
A. Elballouti, S. Belattar
Chouaib Doukkali University, El Jadida [Morocco]
183
The Reliable Implementation of Thermosonics NDT
M. Morbidini, P. Cawley
Imperial College , London [United Kingdom]
184
Characterisation of Colmonoy Coatings using Lock-in Thermography
B. Venkatraman, M. Menaka, B. Raj
Indira Gandhi Centre for Atomic Research, Kalpakkam [India]
185
Automatic System for Crack Detection Using Infrared Thermographic Testing
S. Štarman, V. Matz
Starmans Electronics, Prague [Czech Republic]
186
Application of Infrared Thermography in NDT of Plasma-Facing Components for Tokamaks
P. Qi, Q. Li, G. Luo
Chinese Academy of Science, Hefei [China]
187
Testing of Temperature Field of Explosives in the Cast Process by Infrared Imaging
H. Zhou, Y. Tian, W. Zhang
China Academy of Engineering Physics, CAEP, Mianyang [China]
188
Thermographic inspection of bond quality of FRP strengthed concrete
C. Chiang, Y. Laio, W. Yu
Chao Yang University of Technology, Wufeng, Taichung [Taiwan, China]
189
Recent progresses in the inspection of aerospace components by infrared thermography
C. Ibarra-Castanedo
1
, X. Maldague
1
, E. Grinzato
2
1
Université Laval, Quebec City, Quebec [Canada]
2
Istituto per le Tecnologie della Costruzione - Consiglio (ITC-CNR), Padova [Italy]
7. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
190
Influence of Stress Concentration Factor on Magnetic Memory Effect of Steel Samples under Dynamic Tension Load
C. Shi, S. Dong, B. Xu
Academy of Armored Forces Engineering, Beijing [China]
191
Magnetic Memory Inspection of High Pressure Manifolds
X. Ding, J. Li, F. Li
Xinjiang Petroleum Administration Down-hole Services Company, Kelamayi [China]
192
Simulation of Stress-magnetization Effect on 18CrNi4A Steel by ANSYS
J. Ren, M. Shu, K. Song
Nanchang Hang Kong University, Nanchang [China]
193
Experimental Research on the Microcosmic Mechanism of Stress-magnetic Effect for Magnetic Memory Testing
J. Ren, C. Chen, S. Ren
Nanchang Hang Kong University, Nanchang [China]
194
Technical Diagnostics of Equipment and Constructions with Residual Life Assessment Using the Method of Metal Magnetic Memory
A. Dubov, S. Kolokolnikov
Energodiagnostika Co. Ltd., Reutov [Russia]
195
Estimation of gas and oil pipelines condition based on the method of metal magnetic memory.
A. Dubov, S. Kolokolnikov
Energodiagnostika Co. Ltd., Reutov [Russia]
196
Quality assessment of welded joints by the metal magnetic memory method compared to conventional NDT methods and means for materials' properties assessment
A. Dubov, S. Kolokolnikov
Energodiagnostika Co. Ltd., Reutov [Russia]
197
Stress Testing is a New NDT Type in the Russian Standard GOST R 52330-2005 and International Standard ISO-9712
A. Dubov, S. Kolokolnikov
Energodiagnostika Co. Ltd., Reutov [Russia]
198
New Standards ISO 24497 on the Metal Magnetic Memory Method. the Program of Personnel Training and Certification.
A. Dubov, S. Kolokolnikov
Energodiagnostika Co. Ltd., Reutov [Russia]
199
Magnetization and Demagnetization of Ferromagnetic Materials Staying in Static State in Geomagnetic Field
W. Zhong
Nanjing Gas Turbine Research Institute, Nanjing [China]
200
The Third Group of Spacial Distribution of Magnetic Leakage Field Yielded By a Rectangular Slot on the Workpiece Surface
W. Zhong
Nanjing Gas Turbine Research Institute, Nanjing [China]
201
The Magnetic Dipole Theory for Non-Destructive Testing in China
W. Zhong
Nanjing Gas Turbine Research Institute, Nanjing [China]
202
The effect of hydrogen sulphide on the magnetic behaviour of tube steel X42SS in uniaxial tension
E. Gorkunov
1
, S. Zadvorkin
1
, I. Veselov
2
1
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
2
Russian Research Institute for the Tube and Pipe Indusries, Ekaterinburg branch, Ekaterinburg [Russia]
203
The feasibility of estimating elastic-plastic strain in powder structural steel with different residual porosity by magnetic methods
E. Gorkunov, S. Zadvorkin, S. Mitropolskaya
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
204
Progress in Nondestructive Evaluation of Stress Concentration with MMM Method
L. Zhong, L. Li, X. Chen
Tsinghua University, Beijing [China]
205
Applied Research of Magnetic Memory Method (MMM) on Amusement Devices
B. Hu
1
, G. Shen
1
, L. Li
2
1
China Special Equipment Inspection and Research Institute, Beijing [China]
2
Tsinghua University, Beijing [China]
206
Study on Magnetic Memory Method (MMM) for Fatigue Evaluation
B. Hu, G. Chen, G. Shen
China Special Equipment Inspection and Research Institute, Beijing [China]
207
Stress Measurement Using Magnetic Barkhausen Noise and Metal Magnetic Memory Testing
P. Wang
1
, S. Zhu
1
, G. Tian
2
1
Nanjing University of Aeronautics and Astronautics, Nanjing [China]
2
University of Newcastle, Newcastle upon Tyne [United Kingdom]
208
A Study of Inspecting the Stress on Downhole Metal Casing in Oilfields with Magnetic Memory Method
Q. Liu
1
, J. Lin
2
, M. Chen
1
1
Daqing Logging & Testing Services Company, Daqing [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
209
Metal Magnetic Memory Testing Technique for Stress Measurement
S. Zhu
1
, P. Wang
1
, G. Tian
2
1
Nanjing University of Aeronautics and Astronautics, Nanjing [China]
2
University of Newcastle, Newcastle upon Tyne [United Kingdom]
8. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
210
Non-destructive Characterization of Pearlite Spheroidisation by Magnetic Barkhausen Noise Method
H. GÜr, K. Davut
Middle East Technical University (METU), Ankara [Turkey]
211
The Evaluation of Structure-Property Relationships in the Dual Matrix Ductile Iron by Magnetic Barkhausen Noise Analysis
H. GÜr
1
, M. Ozer
2
, M. Erdogan
2
1
Middle East Technical University (METU), Ankara [Turkey]
2
Gazi University, Ankara [Turkey]
212
Investigating the Austempering Parameters of Ductile Iron by Magnetic Barkhausen Noise Technique
H. GÜr
1
, V. Kilicli
2
, M. Erdogan
2
1
Middle East Technical University (METU), Ankara [Turkey]
2
Gazi University, Ankara [Turkey]
213
Comparison Between Creep Failure Analysis and Magnetic Barkahusen Noise Results
J. Angelo
1
, L. Padovese
2
, M. Alberteris Campos
2
1
Desenvolvimento e Consultoria Ltda., Sao Paulo [Brazil]
2
Universidade de S.Paulo (USP), Sao Paulo [Brazil]
214
The Comparison Test Between Two NDT Methods of Magnetic Couple and Touch Head on the Branch Pipe Angle Weld
Y. Liang, Y. Wang
Shandong Kejie Engineering NDT Co.Ltd, Jinan [China]
215
Bi-axial stress quantitative evaluation with Barkhausen noise: the past and perspectives
V. Vengrinovich, D. Dmitrovich
National Academy of Sciences of Belarus, Minsk [Belarus]
216
Application of Magnetic Particle Inspection in the Field of the Automotive Industry
T. Vetterlein
ITW TIEDE GmbH, Essingen [Germany]
217
Bacterial Magnetic Particles for Applications in NDT&E, Detection of Flaws and Cracks in Sample Materials
E. Siores, A. Lamb, L. Swallow
University of Bolton, Bolton [United Kingdom]
218
The application of magnetic, electromagnetic-acoustic and eddy-current methods to the assessment of plastic deformation under cyclic loading of annealed medium-carbon steel
E. Gorkunov, R. Savrai, A. Makarov
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
219
Magnetic methods for estimating elastic and plastic starins in steels of different classes
E. Gorkunov
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
220
Relation between Magnetism and Charpy Impact Properties in Thermally Aged Fe-Cu Model Alloys
Y. Kamada, Y. Tozawa, Y. Sato
Iwate University, Morioka [Japan]
221
Investigation of friction and abrasive effects in engineering steels with micromagnetic measurements
V. Vengrinovich
1
, V. Busko
1
, A. Makarov
2
1
National Academy of Sciences of Belarus, Minsk [Belarus]
2
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
222
Study on the Method of Detection of the Marks of Ferromagnetic Material Based on the Array of Hall Element
R. Chen, L. Li
Tsinghua University, Beijing [China]
223
Feasibility Study of Magnetic NDE by Impedance Measurement using Single-yoke
H. Kikuchi, F. Sato, K. Ara
Iwate University, Morioka [Japan]
224
A permanent magnet device for measuring the coersive force
E. Gorkunov, V. Tabachnik
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
9. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
225
The NDT Study of Metal Composite Material Tube
J. Lin
1
, J. Ren
2
, L. Bai
2
1
Eddysun Electronic Co. Ltd., Xiamen [China]
2
Nanchang Hang Kong University, Nanchang [China]
226
No UV radiation in magnetic-powder inspection
H. Berg
1
, R. Soehnchen
2
1
BMB Gesellschaft für Materialprüfung mbH, Heilbronn [Germany]
2
Automation W+R GmbH, München [Germany]
227
Research on and Development of Steam Pipeline Creep Real-time Monitoring System Based on Virtual Instrument Technology
L. Zhu
1
, H. He
2
, Q. Ding
3
1
Xi'an Thermal Power Research Institute Co. Ltd., Xi'an [China]
2
Xidian University, Xi'an [China]
3
Xi'an University of Science and Technology, Xi'an [China]
228
Advanced Matrix Phased Array Settings for Inspection
F. Reverdy, S. Mahaut, P. Dubois
Commissariat Energie Atomique (CEA), Gif-Sur-Yvette [France]
229
NDE Technology of Pressure Equipments in Line with International Standards
Y. Li
Jiangsu Taihu Boiler Co. Ltd, Wuxi [China]
230
Design of Transmission Scheme for Radiation Detection &Management Information
J. Liu
1
, C. Liu
2
1
No.8 Bureau of China Construction Co., Ltd, Nanjing [China]
2
CEEG (Nan jing) Pv-Tech Co. Ltd, Nanjing [China]
10. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
231
The Value of DICONDE
A. Koetz
1
, S. Clendening
2
1
GE Inspection Technologies, Skaneateles, NY [USA]
2
GE Inspection Technologies, Lewistown, PA [USA]
232
Industrial Computer Tomography - a Universal Inspection Tool
C. Reinhart
Volume Graphics GmbH, Heidelberg [Germany]
233
Eddy current and ultrasound data fusion applied to Carbon Fiber Reinforced Plastic evaluation
R. Grimberg, A. Savin, R. Steigmann
National Institute of R&D for Technical Physics, Iasi [Romania]
234
Testing Instrument for Internal Stress of Long Seamless Rails
X. Qi, J. Chen, X. Zheng
Beijing University of Chemical Technology, Beijing [China]
235
Procedure for NDT and Traditional Methods of Ancient Buildings Diagnosis, by Using Thermograph,Digital Images and Other Instruments Data Analysis.
L. Palaia, R. Sánchez, V. López
Polytechnic University of Valencia, Valencia [Spain]
236
Correlation leak detector for control of underwater pipeline leakproofness
A. Ovchinnikov, B. Lapshin
Tomsk Polytechnic University, Tomsk [Ukraine]
237
The Basic Study of Safety Evaluation for Cylinder wall of Small output 2 Cycle Engine
S. Syuutei, E. Tsutomu
Shibaura Institute of Technology, Tokyo [Japan]
11. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
238
Advanced Optical Coherence Tomography techniques: novel and fast imaging tools for NDT
D. Stifter, K. Wiesauer, M. Wurm
Upper Austrian Research GmbH, Linz [Austria]
239
Evaluation of Rubber - Composites Bonding Components by Using Laser Electronic Shearography
S. Liu, F. Liu, L. Li
Beijing Aeronautical Manufacturing Technology Research Institute (BAMTRI) , Beijing [China]
240
Studies on Digital Shearography for Testing of Aircraft Composite Structures and Honeycomb-based Specimen
J. Zhang
1
, R. Geng
2
1
University of Science and Technology of China, Hefei [China]
2
Beijing Aeronautical Technology Research Center, Beijing [China]
241
Aerospace NDT with Advanced Laser Shearography
J. Newman
Laser Technology Inc., Norristown, PA [USA]
242
Detection capabilities of state-of-the-art Shearography systems
E. Moser, J. Collrep
Dantec-Ettemeyer, Ulm [Germany]
12. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
243
The ways of penetrant testing applicability for rough surfaces
N. Migoun, N. Delenkovsky
National Academy of Sciences of Belarus, Minsk [Belarus]
244
Automated Dye Penetrant Systems with Process Control and Documentation in the Aerospace Industry
T. Vetterlein
1
, M. Wagener
2
, H. Rongen
2
1
ITW TIEDE GmbH, Essingen [Germany]
2
Forschungszentrum Jülich, Jülich [Germany]
245
Equipment and Mobile Laboratories for Ndt and Diagnostics of Underground Communication Lines
V. Koltsov
1
, Y. Kondratiev
2
1
Joint Venture Seba Spektrum , Moscow [Russia]
2
Joint Venture Seba Energo, Moscow [Russia]
246
Non destructive testing of materials subject to atmospheric stress corrosion cracking
M. Van dalen
1
, C. Wicker
2
, G. Wilson
2
1
South African Institute of Welding, Johannesburg [South Africa]
2
Eskom, Cape Town [South Africa]
13. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
247
Nondestructive Evaluation of Uranium- PLutonium Mixed Oxide(MOX) fuel ts by Gamma Autoradiography
J. Panakkal, D. Mukherjee, H. Kamath
Bhabha Atomic Research Centre, Maharashtra [India]
248
Digital Radiography and Computed Radiography for enhancing the Quality and Productivity of weldments in Boiler components
R. Pardikar
Bharat Heavy Electricals Limited, BHEL, Tiruchirappalli [India]
249
Low Frequency Acoustic (Impedance) Flaw Detectors of the New Generation and Their Application
V. Muzhitsky, A. Sysoev, A. Efimov
JSC, SPECTRUM-RII, Moscow [Russia]
250
Influence of lack-of-fusion defects on load capacity of MAG welded joints
M. Jovanovic
1
, J. Grum
2
, M. Uran
1
1
Welding Institute, Ljubljana [Slovenia]
2
University of Ljubljana, Ljubljana [Slovenia]
251
Improved Procedure for Computed Radiography - a Comparative Study on Welded Tube Sections by Film Radiography and Computed Radiography
J. Beckmann
1
, S. Rachny
2
, U. Ewert
1
1
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
2
Applus RTD Inspektionsgesellschaft mbH, Frechen [Germany]
252
A new fully digital system for RT inspection of metal tube to tube sheet joints of heat exchangers
U. Zscherpel
1
, P. Rost
2
, K. Spartiotis
3
1
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
2
BASF, Ludwigshafen [Germany]
3
Oy Ajat Ltd, Espoo [Finland]
253
Flaw Size Dependent Contrast Reduction and Additional Unsharpness by Scattered Radiation in Radiography - Film and Digital Detectors in Comparison-
U. Ewert, U. Zscherpel, C. Bellon
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
254
Feature Extraction and Optimisation for X-ray Weld Image Classification
Y. Yin, G. Tian
University of Newcastle, Newcastle upon Tyne [United Kingdom]
255
Prediction of density in porous materials by x-ray techniques
A. Bateni, M. Ahmadi, N. Parvin
Amir Kabir University of Tech (AUT), Tehran [Iran]
256
Computed Radiography and Microtomography of Riveted Lap Joints of GlareTM Subjected to Constant Amplitude Loading (CAL) Fatigue
S. Rett, D. Santana, J. Yanaguizawa
Federal University of Pernambuco, Recife-PE [Brazil]
257
X-Ray Testing Sensitivity of Carbon Fiber Reinforced Aluminium Matrix Composite
G. Wu, Y. Li, J. Su
Harbin Institute of Technology, Harbin [China]
258
The exploration to the case of X-ray detection of the vertical angle Weld
W. Yan, P. Zeng, G. Zhang
Chongqing Construction Engineering Non-destructive Test Limited Company, Chongqing [China]
259
A method of Ray digital imaging automatic Inspection on Tube to tube sheet welded joints Based on VC + +
W. Zhao
1
, K. Ding
2
, G. Chen
2
1
Tianjin University, Tianjin [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
260
Use of Monte-Carlo method for the reconstruction of response functions and radiation spectra in radiography
M. Zhukovskiy, S. Podoliako
Russian Academy of Sciences, Moscow [Russia]
261
Digital Radiographic Imaging Inspection System on the Tube to Tube sheet Welding Joints of Heat Exchanger
K. Ding, G. Chen, B. Shou
China Special Equipment Inspection and Research Institute, Beijing [China]
262
NDT Data Management - Archive and Data Sharing
A. Koetz
GE Inspection Technologies, Skaneateles, NY [USA]
263
Factors affecting Probability of Detection with Computed Radiography
G. Mohr
1
, P. Willems
2
1
GE Inspection Technologies, Lewistown, PA [USA]
2
Industrial & Scientific Consulting BVBA, Stekene [Belgium]
264
Computed Radiography with isotopes- Suitability for Weld Inspection
M. Venugopal, P. Thapa, R. Venkatachalam
GE Global Research Center, Bangalore [India]
265
The Optimizing Technology Research of Imaging Quality on X-ray Digital Imaging
W. Guo
1
, L. Liang
2
1
Beijing University of Posts and Telecommunication, Beijing [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
266
Digital Camera Application in X-ray Real Time Control of European Launcher's Ariane 5 Booster Segments.
E. Tosti
AVIO Propulsione AeroSpaziale, Colleferro [Italy]
267
An Quantitative Evaluation of the Canadian Forces New Radiology Inspection Systems for the Detection of Water Ingress in CF188 Flight Control Surfaces
B. Tang
1
, P. Hungler
2
, C. Sweetapple
3
1
Department of National Defence Canada, Kingston, Ontario [Canada]
2
Royal Military College of Canada, Kingston, Ontario [Canada]
3
Aerospace and Telecommunication Engineering Support Squadron, Astra [Canada]
268
Gamma Ray System Operated by Divers for Underwater Inspection
C. Marinho
1
, C. Camerini
1
, R. Lopes
2
1
Petrobras S.A, Rio de Janeiro [Brazil]
2
Federal University of Rio de Janeiro (UFRJ), Rio de Janeiro [Brazil]
269
Gauging Information Systems, Means of Technological Diagnostics and Intelligent Gauges in Nuclear Power Engineering and Industry
N. Kuzelev
Russian National Technical Physics and Automation research Institute, VNIITFA, Moscow [Russia]
270
X-Ray Thickness Gauges of the RIT10 Family for Thickness Measurement at Line Production of Rolled Metal
B. Artemiev, A. Maslov
SPEKTR-GROUP Association, Moscow [Russia]
271
X-ray pulse apparatus based on explosive electron emission
E. Peliks
Spectroflash Ltd, St-Petersburg [Russia]
272
Ray Detection Digital Image Quality and Influential Factors
X. Zeng
Guangdong Yingyuan Steel Products Co. Ltd, Qingyuan [China]
273
A Review of Current Status in Applying Special Radiographic Techniques to Pressure Equipment in China
Y. Li
Jiangsu Taihu Boiler Co. Ltd, Wuxi [China]
274
Evaluations on the Composite Bonding Quality by Ultrasonic Amplitude Measurements
J. Lee, H. Jee, N. Ju
Korea Institute of Material Science, CHANGWON [Korea]
275
Constitution and Prospect of Chinese Radiography Digital Imaging Nondestructive Testing Standard
X. Zeng
Guangdong Yingyuan Steel Products Co. Ltd, Qingyuan [China]
276
Computed Radiography deployed subsea by a Romotely Operated Vehicle
J. McNab, B. Steel
Oceaneering International Inspection, Aberdeen, Scotland [United Kingdom]
277
Strategies for Film Replacement in Radiography - Films and Digital Detectors in Comparison -
U. Ewert
1
, U. Zscherpel
1
, K. Bavendiek
2
1
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
2
YXLON International X-Ray GmbH, Hamburg [Germany]
278
Simulation Studies of Radiographic Inspections with CIVA
R. Fernandez
1
, A. Schumm
2
, J. Tabary
3
1
Commissariat Energie Atomique (CEA), Gif-Sur-Yvette [France]
2
Electricité de France (EDF) R&D , Clamart [France]
3
Commissariat Energie Atomique (CEA-LETI), Grenoble [France]
14. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
279
Progress of Nondestructive Testing and Evaluation in China
G. Shen
China Special Equipment Inspection and Research Institute, Beijing [China]
280
An Overview of the Rapidly Developing Non-Destructive Testing Technology in China
R. Geng
Beijing Aeronautical Technology Research Center, Beijing [China]
281
Recent Developments of Aircraft Nondestructive Evaluation Based on Advanced Sensor Techniques
G. Qi, H. Lei, R. Geng
Beijing Aeronautical Technology Research Center, Beijing [China]
282
The Role of IAEA/AFRA on the Promotion of NDT in Africa
K. Danso
1
, J. Guild
2
, F. Herelli
3
1
Ghana Atomic Energy Commission, Accra [GHANA]
2
Southern African Institute of Welding (SAIW), Johannesburg [South Africa]
3
Centre Technique Des Industries Mecaniques et Electriques (CETIME), Tunis [Tunisia]
283
From Fifteen to Two Hundred NDT-methods in Fifty Years
T. Aastroem
, []
284
Non-destructive testing in Belarus
N. Migoun, S. Novikov
National Academy of Sciences of Belarus, Minsk [Belarus]
285
NDT Integrated Technology Based on Computer Network
J. Lin
1
, J. Ren
2
1
Eddysun Electronic Co. Ltd., Xiamen [China]
2
Nanchang Hang Kong University, Nanchang [China]
286
Advanced Publishing in NDT
R. Diederichs
1
, E. Ginzel
2
1
NDT.net, Kirchwald [Germany]
2
Materials Research Institute, Waterloo [Canada]
287
50th Anniversary of Non-Destructive Testing in Russia
V. Klyuev, Y. Fedosenko
SPEKTR-GROUP Association, Moscow [Russia]
15. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
288
The Development of Laser Ultrasonic Visualization Equipment and its Application in Nondestructive Inspection
B. Wang
1
, J. Takatsubo
2
1
Tsukuba Technology Co. Ltd., Tsukuba [Japan]
2
Advanced Industrial Science and Technology (AIST), Tsukuba [Japan]
289
Study on the Character of Metal Magnetic Memory Signal in the Course of High-cycle Fatigue Experiment for 16MnR Steel
J. Li
1
, Y. Zhang
1
, G. Shen
2
1
Beijing University of Technology, Beijing [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
290
Research on Pipeline Corrosion and Cracking Inspection by Broad-band Ultrasonic Pig Technology
F. He
1
, S. He
2
, J. Yang
1
1
Beijing Institute of Petrochemical Technology, Beijing [China]
2
Nuclear Industry Training Center, Beijing [China]
291
The Numerical Investigation into the Influence of the Scattering Effect from the Aggregates of Concrete on the Transient-elastic-wave-based NDT Technologies
J. Tong
1
, C. Chiang
2
, W. Chuang
2
1
Hungkuang University, Shalu Township, Taichung [Taiwan, China]
2
Chao Yang University of Technology, Wufeng, Taichung [Taiwan, China]
292
Influence of Inclusion on Crack Tip in Rotating Disc by Photoelasticity and Caustic Method
S. Syuutei, H. Keiich, E. Tsutomu
Shibaura Institute of Technology, Tokyo [Japan]
293
Ultrasonic Examination of "Difficult Welds"
W. Michnowski, R. Mis, J. Mierzwa
Zaklad Badan Materialow (ZBM) ULTRA, Wroclaw [Poland]
294
Determination of Elastic modulus of thin materials by Speckle Interferometry
A. Naseem, K. Kim, H. Chang
Chosun University, Gwangju [Korea]
295
Detectability of kissing bonds using the non-linear high frequency transmission technique
D. Yan , B. Drinkwater, S. Neild
University of Bristol, Bristol [United Kingdom]
296
Interaction of Rayleigh Waves Induced by Interdigital Transducer with Fatigue Crack
J. Na
1
, S. Kuhr
1
, J. Blackshire
2
1
University of Dayton, Dayton, OH [USA]
2
US Air Force Research Lab, Dayton, OH [USA]
297
Application of Wide Band AE Sensor in Model Test of Reinforced Concrete Structures
W. Zhang
1
, C. Xia
2
, F. Kong
1
1
Shanghai COVORDA Electronic Systems Co. Ltd., Shanghai [China]
2
Shanghai Research Institute of Building Sciences, Shanghai [China]
298
Industrial Ultrasonic Examination of plates with EMAT
A. Kirikov
1
, V. Britvin
2
, A. Kashin
2
1
Nordinkraft AG, Pforzheim [Germany]
2
Nordinkraft Company, Cherepovets [Russia]
299
Holistic Approach for Structural Integrity Evaluation of Composite Main Rotor Blades
K. Dragan, S. Klimaszewski
Air Force Institute of Technology, Warsaw [Poland]
300
Integrated Time of Flight Diffraction Set Up Software
J. Verkooijen
1
, A. Mclay
2
1
Sonovation B.V., Oosterhout [Netherlands]
2
Sonovation Ltd, Cheshire [United Kingdom]
301
Water Content Diagnostics of Concrete Using Nonlinear Acoustics Means
D. Zhou, X. Liu, X. Gong
Nanjing University, Nanjing [China]
302
Data Computing Disk of Line Convergent Detector
S. Lin
QianGuo Refinery SongYuan City, Songyuan [China]
303
Immersion Multi-zone Ultrasonic Inspection System of Large-diameter Special Billets
J. Jin
1
, X. Liu
2
, D. Han
1
1
GE Inspection Technologies, Shanghai [China]
2
Fushun Special Steel Co. Ltd, Fushun [China]
304
Evaluation of Impact Damages in RTM Stitched Composites by Using Ultrasonic Multiple Imaging Techniques
S. Liu, F. Liu, E. Guo
Beijing Aeronautical Manufacturing Technology Research Institute (BAMTRI) , Beijing [China]
305
Experimental system dependent factors in the measurement of ultrasonic nonlinear parameter by using contact PZT transducer
I. Choi
1
, J. Lee
1
, K. Jhang
2
1
Graduate School of Hanyang University, Seoul [Korea]
2
Hanyang University, Seoul [Korea]
306
Ultrasonic Evaluation of Friction Stir Welding
F. Liu, S. Liu, L. Li
Beijing Aeronautical Manufacturing Technology Research Institute (BAMTRI) , Beijing [China]
307
Study on Characteristic of Thin Layer Rubber Based on Ultrasonic Echo Testing
J. Chang
1
, X. Wang
2
, Y. Shan
1
1
Dalian Maritime University, Dalian [China]
2
Dalian University of Technology, Dalian [China]
308
Evaluation of the Fiberglass-Reinforced Plastics Interfacial Behavior by using Ultrasonic Wave Propagation Method
J. Chang, J. Xu
Dalian Maritime University, Dalian [China]
309
Optimization of Ultrasonic Testing System Applicable to High Manganese Steel Rails
R. Hirokawa, Y. Mizutani, Y. Kurokawa
Tokyo Institute of Technology, Tokyo [Japan]
310
3i in NDT
N. Ng, W. Ha
De Hua Materials Testing Co. Ltd., Hong Kong [China]
311
Application of full data acquisition technology in automatic ultrasonic inspection
Y. Teng, D. Wu, Z. Zhao
Beijing Jiaotong University, Beijing [China]
312
An Investigation into the Performance of Complex Plane Spilt Spectrum Processing Ultrasonics on Composite Materials
M. Johannes
1
, P. Rubbers
2
1
CSIR, Pretoria [South Africa]
2
SCM, Sunnighill [South Africa]
313
Ultrasonic Testing of Austenitic Welds at the Russian NPP
V. Badalyan, A. Vopilkin, P. Samarin
Scientific and Production Center, SPC ECHO+, Moscow [Russia]
314
Acoustical Holography Implementation for Defected Rails Inspection
A. Vopilkin, D. Kononov, D. Tikhonov
Scientific and Production Center, SPC ECHO+, Moscow [Russia]
315
Ultrasonic Transducers Calibration System with 3D Processing AUGUR 5.4
A. Bazulin, E. Bazulin, D. Tikhonov
Scientific and Production Center, SPC ECHO+, Moscow [Russia]
316
Automated Ultrasonic Pipe Weld Inspection
W. Deutsch
Karl Deutsch Pruef- und Messgeraetebau, Wuppertal [Germany]
317
Application of Ultrasonic Guided Wave to Heat Exchanger Tubes Inspection
I. Park, Y. Kim, S. Park
Seoul National University of Technology, Seoul [Korea]
318
Comparison between in - line ultrasonic monitoring of the spot weld quality and conventional NDT methods applied in a real production environment
D. Stocco
1
, A. Chertov
2
, R. Maev
2
1
Mercedes-Benz do Brasil Ltda, Sao Bernardo do Campo [Brazil]
2
University of Windsor, Windsor, Ontario [Canada]
319
Line Maintenance Solutions for composite damage evaluation
C. Murner
1
, W. Yzelman
1
, A. Koetz
2
1
GE Inspection Technologies, Lewistown, PA [USA]
2
GE Inspection Technologies, Skaneateles, NY [USA]
320
The Study the Preferred Magnetization Direction of Long Line Magnetostrictive Position Sensor
Z. Wang, X. Chang
TaiYuan University of Technology, Taiyuan [China]
321
Determination of Relation Between Elastic Constant and Sintered Temperature in WC-Ni Composites
I. Sarpün
1
, S. Tuncel
2
, V. Özkan
1
1
Afyon Kocatepe University, Afyon [Turkey]
2
TÜBITAK Marmara Research Center, Gebze / Kocaeli [Turkey]
322
High Temperature Integrated and Flexible Ultrasonic Transducers for NDT
M. Kobayashi, C. Jen, J. Bussiere
National Research Council of Canada (NRC), Boucherville, Quebec [Canada]
323
Ultrasonic Inspection of Steam Generators at CANDU Power Plants
A. Chen
1
, K. Chan
1
, J. Huggins
2
, T. Malkiewicz
2
1
Kinectrics Inc., Toronto [Canada]
2
Ontario Power Generation, Toronto [Canada]
324
Sizing in Phased Array Technique using Diffraction and Amplitude Displacement
G. Nardoni, M. Certo, P. Nardoni
I&T Nardoni Institute, Brescia [Italy]
325
Experimental investigation on porosity of carbon fiber-reinforced composite using ultrasonic attenuation coefficient
L. Lin
1
, M. Luo
2
, H. Tian
1
1
Dalian University of Technology, Dalian [China]
2
Beijing Aerospace Research Institute of Materials and Processing Technology, Beijing [China]
326
Monitor the circumferential welds of Multi-layer Thick-wall Pressure Vessels Serving at Elevated Temperature by Ultrasonic Testing
X. Li
1
, B. Tang
2
1
Guangdong Institute of Special Equipment Inspection, Guangzhou [China]
2
Guangzhou Keanda NDT Co. Ltd., Guangzhou [China]
327
The reliability of the ultrasonic characterization of welds by the artificial neural network
F. Bettayeb
1
, H. Benbartaoui
2
, B. Raouraou
2
1
Research center on welding and control, Algiers [Algeria]
2
University of Science and Technology (USTHB), Algiers [Algeria]
328
The Ultrasonic Feature Imaging Testing of special structure
M. Lu, Y. Zhu, X. Liu
Nanchang Hang Kong University, Nanchang [China]
329
Thin multi-layer plate testing with Ultrasonic Feature Scan Imaging System
M. Lu
1
, D. Fu
2
, Q. Li
2
1
Nanchang Hang Kong University, Nanchang [China]
2
Tsinghua University, Beijing [China]
330
Ultrasonic Feature Imaging System for Testing Bimetal Rotor Clad Layer
X. Liu
1
, M. Lu
2
, Y. Chen
1
1
Tsinghua University, Beijing [China]
2
Nanchang Hang Kong University, Nanchang [China]
331
Quantitative Evaluation of Brazed Joints in Flat Structure with Ultrasonic Inspection method
J. Liang, Y. Shi, D. Yang
Beijing Institute Of Aeronautical Materials, Beijing [China]
332
Application of Bare Piezoelectric Ceramics in Monitoring Resin Transfer Moulding (RTM) Process
C. Lu, A. Postula
University of Queensland, Brisbane, QLD [Australia]
333
A New Testing Method Combining EMAT with Eddy Current
F. Huang
1
, Z. Zhou
1
, J. Lin
2
1
Beijing University of Aeronautics and Astronautics, Beijing [China]
2
Eddysun Electronic Co. Ltd., Xiamen [China]
334
Observation of Trapped Thin Oil Film Behavior between Ball and Disc with Using Ultrasonic Technique
A. Takeuchi
1
, S. Terada
2
, S. Toda
2
1
Kochi University of Technology, Kochi [Japan]
2
Automax Co. Ltd., Tokyo [Japan]
335
Simulation of Scattering Acoustic Field in Rod and Identify of Ultrasonic Flaw Detecting Signal
K. Yuan, W. Song, Y. Chen
Tsinghua University, Beijing [China]
336
Research on Ultrasonic Velocity Imaging of Metal Matrix Composites with TIRP Method
Y. Gao
1
, Z. Zhou
1
, F. He
2
1
Beijing University of Aeronautics and Astronautics, Beijing [China]
2
Beijing Institute Of Aeronautical Materials, Beijing [China]
337
Influence of precipitates and dislocations on the acoustic nonlinearity
C. Kim, T. Park, I. Park
Seoul National University of Technology, Seoul [Korea]
338
Ultrasonic NDE of thin Composite plate Based on an enhanced Wigner-Ville distribution
G. Wu, J. Su , D. Zhu
Harbin Institute of Technology, Harbin [China]
339
Corrosion Assessment of Offshore Oil Pipeline Based on Ultrasonic Technique
Q. Zhang, P. Que, H. Lei
Shanghai Jiaotong University, Shanghai [China]
340
In-motion ultrasonic testing of the tread of high-speed railway wheels using the inspection system AUROPA III
H. Salzburger
1
, L. Wang
2
, X. Gao
2
1
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
2
Southwest Jiaotong University, Chengdu [China]
341
Application of Logarithmic Amplifier to Ultrasonic Imaging
T. Sasahara
1
, H. Inoue
2
1
Central Research Institute of Electric Power Industry, Kanagawa [Japan]
2
Tokyo Institute of Technology, Tokyo [Japan]
342
Inspection of CANDU reactor pressure tubes using ultrasonics
M. Trelinski
Ontario Power Generation, Toronto [Canada]
343
US spectroscopy applied to evaluation of some prosthesis made from syntherized zirconium oxides
R. Grimberg, A. Savin, R. Steigmann
National Institute of R&D for Technical Physics, Iasi [Romania]
344
Microdefect Detection in High-Temperature Resistant Steel by Using Ultrasound Laser Interferometer
Y. Smorodinsky, Y. Zhitlukhina, D. Perov
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
345
The Utrasonic Detection of the Large Welded Gear
Y. Chen
1
, C. Qu
1
, X. Yue
2
1
Chongqing gearbox limited liability corporation, Chongqing [China]
2
Chongqing University, Chongqing [China]
346
TOFD-Scan Imaging Based on Synthetic Aperture Focusing Technique
Z. Wang, Y. Zhou, J. Tian
Wuhan Zhongke Innovation Technology Company Limited, Wuhan [China]
347
Controlled excitation of ultrasonic transducers
A. Volker, M. Van der heiden
TNO Science & Industry, Delft [Netherlands]
348
High resolution transforms
A. Volker
TNO Science & Industry, Delft [Netherlands]
349
Using ultrasonic pulse velocity to evaluate residual compressive strength of post-fire-curing concrete
H. Yang
1
, Y. Lin
1
, C. Hsiao
2
1
National Chung-Hsing University, Taichung [Taiwan, China]
2
National Taichung Institute of Technology, Taichung [Taiwan, China]
350
Non-Destructive Examination for Ageing Management of Indian Nuclear Power Plants
P. Nanekar, B. Shah
Bhabha Atomic Research Centre (BARC), Mumbai [India]
351
Development, Validation and Execution of the Automated Ultrasonic Testing of a Subsea Pipeline Hot Tap Weld
M. Miller
Shell Exploration and Production, Aberdeen, Scotland [United Kingdom]
352
Detection of a Surface-Breaking Crack Depth by Using the Surface Waves of Multiple Laser Beams
S. Park, Y. Cheong, S. Baik
Korea Atomic Energy Research Institute (KAERI), Daejeon [Korea]
353
Development of reinforced concrete corrosion amount presumption method by ultrasonic method
Y. Sakurada, H. Irie, Y. Yoshida
Nippon Telegraph and Telephone Corporation, Tsukuba [Japan]
354
Ultrasonic Pulse Signal Diffraction from Different Flaws in Elastic Media
D. Perov, A. Rinkevich, Y. Smorodinsky
Russian Academy of Sciences, RAS, Ural Branch , Ekaterinburg [Russia]
355
Testing Application of Scanning Acoustic Microscope for Adhesive Characteristics of Explosive-Aluminum-Alloy Interface
Z. Yang, W. Zhang, Y. Tian
China Academy of Engineering Physics, CAEP, Mianyang [China]
356
Development of Ultrasonic Line-Focus SH-Wave Probe
Y. Moriya, H. Inoue
Tokyo Institute of Technology, Tokyo [Japan]
357
Ultrasonic TOFD Testing Model for Crack Measurement in Thick Wall Weldment
T. Gang, D. Chi
Harbin Institute of Technology, Harbin [China]
358
Fretting Cracking Ultrasonic Detection in Generator Teeth
X. Jian
1
, S. Smalley
1
, J. Knowles
2
1
Phoenix Inspection Systems Ltd, Warrington [United Kingdom]
2
ALSTOM Power Service, Baden [Switzerland]
359
Electromagnetic Acoustic Transducers for in and out of plane Ultrasonic Wave Detection
X. Jian
1
, S. Dixon
2
, K. Quirk
1
1
Phoenix Inspection Systems Ltd, Warrington [United Kingdom]
2
University of Warwick, Coventry [United Kingdom]
360
Cellular polypropylene Ferroelectret Film: Piezoelectric Material for non-contact Ultrasonic Transducers
J. Döring, V. Bovtun, M. Kreutzbruck
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
361
Application of Portable Non-Destructive Testing Instruments to Enhance Performance of Hot Strip Mill Rolls.
R. Verma, K. Singh, G. Murty
Steel Authority of India, Ranchi [India]
362
Automated Inspection of Complex Composite Components in the Production Cycle
A. Maurer
1
, R. Henrich
2
, W. De Odorico
1
1
GE Inspection Technologies, Alzenau [Germany]
2
Airbus Deutschland GmbH, Bremen [Germany]
363
Advancements in Pipeline Girth Weld Inspection
J. Stetson
GE Inspection Technologies, Lewistown, PA [USA]
364
Inclusion Evaluation of the Slab by the Focused Ultrasonic Method
G. Zhang
1
, Y. Wang
1
, Y. Hua
2
1
Tongji University , Shanghai [China]
2
University of Shanghai for Science and Technology, Shanghai [China]
365
Inline-Process and Quality Control of Spotwelds of Car Bodies - Ultrasonic Sensors integrated in Resistance Welding Electrodes
G. Vogt
VOGT Werkstoffprüfsysteme GmbH, Burgwedel [Germany]
366
Development of Ultrasonic Transducer Testing Austenitic Stainless Steel Weld
Y. Chen
Guangdong Special Equipment Inspection Institute, Guangzhou [China]
367
Process Monitoring of Cast Explosive Solidification Molding by on-line Multichannel Ultrasonic Measurement
W. Zhang, Y. Tian, H. Zhou
China Academy of Engineering Physics, CAEP, Mianyang [China]
368
Advanced NDE inspection methods for detection of SCC in blade attachments and blade roots
H. Rauschenbach, M. Clossen, M. Opheys
Siemens Power Generation, Mülheim [Germany]
369
Related Problems in Ultrasonic Detection of Porcelain Insulator
L. Chen, J. Wang
Anhui Electric Power Research Institute, Hefei Anhui [China]
370
Performance of UT creeping waves in crack sizing
M. Carboni, M. Sangirardi
Politecnico di Milano, Milano [Italy]
371
An analysis of UT echoes coming from fatigue cracks and artificial defects on railway axles
M. Carboni
Politecnico di Milano, Milano [Italy]
372
PipeWIZARD Version 4 - a New, Improved Pipeline AUT Girth Weld Inspection System
M. Moles, S. Labbé
Olympus NDT, Waltham, MA [USA]
373
Olympus NDT Training Academy
M. Moles
Olympus NDT, Waltham, MA [USA]
374
Calibration Method Study of Ultrasonic Thickness Gauge
X. Peng
TIME GROUP Inc. Bejing, Beijing [China]
375
Electromagnetic-Acoustic Transducers for in-Service Manual Testing of Heated Objects
V. Bobrov, A. Samokrutov, V. Shevaldykin
JSC, SPECTRUM-RII, Moscow [Russia]
376
A Complete Solution for Weld Inspections - Phased Arrays and Diffraction Sizing
M. Moles, S. Labbé
Olympus NDT, Waltham, MA [USA]
377
Comparing Sound Absorption Characteristic of Acoustic boards made of Aspen Particles and Different Percentage of Wheat and Barely Straws
M. Saadatnia, G. Ebrahimi, M. Tajvidi
Tehran University, Karaj [Iran]
378
Round-Robin NDE Testing for Charpy Impact Specimens of Cold-rolled and Thermally Aged Fe-1wt.%Cu Alloys
Y. Kamada
1
, H. Kikuchi
1
, K. Joubouji
2
1
Iwate University, Morioka [Japan]
2
Institute of Nuclear Safety System Inc., Mihama [Japan]
379
Acoustic Emission Testing of the Shell of Electromagnetic Valve
G. Xu, Y. Chen, Z. Cao
Shanghai Institute of Space Power -sources, Shanghai [China]
380
Nondestructive Inspection of Composite Structures: Methods and Practice
D. Hsu
Iowa State University, Ames, Iowa, [USA]
381
Evaluation of Crack Depth Using Nonlinear Acoustic Effect
T. Lee, K. Jhang, M. Jin
Hanyang University, Seoul [Korea]
382
Current NDT Research & Development for NPP Inspections
P. Bieder
1
, G. Dobmann
2
, M. Kröning
2
1
QNET East Asia, Shanghai [China]
2
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
383
Multiparameter eddy-current NDT method for quality control of thin-sheet, multilayer products and coatings
S. Klyuev, V. Shaternikov
SPEKTR-GROUP Association, Moscow [Russia]
384
A Study on Advanced Ultrasonic Measurement of Flaw Length
S. Shiroshita
1
, Y. Yokono
2
1
Non-Destructive Inspection Co.,Ltd., Osaka [Japan]
2
Pony Industry Co.,Ltd., Osaka [Japan]
385
Ultrasonic Characterization of Flaws
A. Karpelson
Kinectrics Inc., Toronto [Canada]
386
In Situ Inspection with Ultrasonic Creeping Wave for Rabbet of Turbine Blade
X. Xie, M. Tu , X. Yang
First Aeronautic Institute of Air Force, Xinyang [China]
387
State and Tendencies of Development in Russia of Portable Non-Cooled IR-Imaging Systems for Search Tasks
A. Kovalev, G. Tarasenko, A. Kovalev
JSC, SPECTRUM-RII, Moscow [Russia]
388
Application of Non-contact Lamb generated EMAT Technique to Thickness Reduction Inspection
I. Park, J. Lee, Y. Kim
Seoul National University of Technology, Seoul [Korea]
389
Studies of Broad-band Ultrasonic Techniques for Inspection of Bounding Quality in ITER First Wall
X. Li
1
, J. Shen
1
, F. He
2
1
Capital Normal University, Beijing [China]
2
Nuclear Power Institute of China, Beijing [China]
390
Real-time dual-channel ultrasonic system for inspection of aircraft structures
B. Regez
1
, G. Kirikera
1
, I. Komsky
1
, S. Krishnaswamy
1
, B. Lasser
2
1
Northwestern University, Evanston, IL [USA]
2
Imperium Inc, Silver Spring,MD [USA]
391
Selected CANDU pressure tube degradation mechanisms and inspection related issues
M. Trelinski
Ontario Power Generation, Toronto [Canada]
392
Evaluation of Depth of Deterioration of Concrete Structure after Fire Using Stress Wave Method
C. Cheng
Choayang University of Technology, Aberdeen [Taiwan, China]
393
Detection of Electric Discharge Machining State by Using Ultrasonic Technique
S. Hori, N. Nishiwaki
Tokyo University of Agriculture and Technology, Tokyo [Japan]
394
PROline - ultrasonic testing for electron beam and laser weld seams of transmission control gears - Many more Applications in Production
G. Vogt, C. Koehler
VOGT Werkstoffprüfsysteme GmbH, Burgwedel [Germany]
395
E-ROTA Process and System for Dimensional Characterization of Tubes
P. Coperet
Socomate International, Crécy la Chapelle [France]
396
Case Studies on Uncertainties of Ultrasonic Weld Testing Interpretation
K. Nachimuthu
1
, S. Babu
2
1
Non Destructive Testing Society (Singapore), Singapore [Singapore]
2
VSL Singapore Pte Ltd, Singapore [Singapore]
16. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
397
Development of EMA Guided Wave Technique for Testing of Wires
H. Jia, H. Fan
Central Iron & Steel Research Institute, Beijing [China]
398
Modelling of guided ultrasonic wave in aircraft wiring
Y. Gharaibeh, S. Soua, S. Chan
TWI Ltd, Cambridge [United Kingdom]
399
Application of Laser-Generated Ultrasound for Evaluation of Wall-thinning in Carbon Steel Elbow
D. Kim, S. Lee, J. Lee
Pusan National University, PUSAN [Korea]
400
Detection of Protective Coating Disbonds in Pipe Using Circumferential Guided Waves
J. Van Velsor
1
, J. Rose
1
, J. Nestleroth
2
1
Pennsylvania State University, University Park, PA [USA]
2
Battelle Memorial Institute, Columbus, OH [USA]
401
Ultrasonic Guided Wave Nondestructive Testing for Helicopter Rotor Blade
X. Qi
1
, J. Rose
1
, C. Xu
2
1
Pennsylvania State University, University Park, PA [USA]
2
Beijing Institute of Technology, Beijing [China]
402
Inspection of Adhesively Bonded Joints Using Ultrasonic Guided Waves
P. Puthillath
1
, J. Rose
1
, C. Xu
2
1
Pennsylvania State University, University Park, PA [USA]
2
Beijing Institute of Technology, Beijing [China]
403
Guided Wave Thickness Measurement Tomography for Structural Health Monitoring in Critical Zones of Pipelines
L. Breon
1
, J. Rose
1
, C. Xu
2
1
Pennsylvania State University, University Park, PA [USA]
2
Beijing Institute of Technology, Beijing [China]
404
Recent Advances on Guided Waves in Pipe Inspection
J. Rose
1
, J. Mu
1
, Y. Cho
2
1
Pennsylvania State University, University Park, PA [USA]
2
Pusan National University, PUSAN [Korea]
405
Study on Automatic Testing of Treads of Running Railroad Wheels
H. Fan, H. Jia
Central Iron & Steel Research Institute, Beijing [China]
406
Ultrasonic Tomography of Guided Wave
L. Jin
1
, Y. Cho
1
, J. Rose
2
1
Pusan National University, PUSAN [Korea]
2
Pennsylvania State University, University Park, PA [USA]
407
Wireless Ultrasonic Transducer Network for Structural Health Monitoring of an Aircraft Wing
X. Zhao, T. Qian, G. Mei
Intelligent Automation Inc., Rockville [USA]
408
Study on Simulation of Guided Wave Propagation in Pipes
C. Shen, Y. Wang, F. Sun
Naval University of Engineering, Wuhan [China]
409
Study on Relationship between Amplitudes of Reflection Signals and Positions of Magnetostrictive Transducer
Y. Wang, L. Shen, F. Sun
Naval University of Engineering, Wuhan [China]
410
The Affection of Pipes Characteristics to Exciting Frequency for Guided Waves NDT
Y. Wang, L. Shen, C. Shen
Naval University of Engineering, Wuhan [China]
411
Research on an Inspection Method for De-bond Defects in Aluminum Skin-Honeycomb Core Sandwich Structure with Guided Waves
F. He
1
, Z. Zhou
2
, Z. Feng
3
1
Beijing Institute Of Aeronautical Materials, Beijing [China]
2
Beijing University of Aeronautics and Astronautics, Beijing [China]
3
Academy of Military Transportation, Beijing [China]
412
Research on Line-scan Inspection Method with Guided Waves
Z. Zhou
1
, Z. Feng
2
1
Beijing University of Aeronautics and Astronautics, Beijing [China]
2
Academy of Military Transportation, Beijing [China]
413
Nondestructive Determination of Elastic Constants of Thin Plates Based on PVDF Focusing Ultrasound Transducers and Lamb Wave Measurements
L. Wei, C. Chung, Y. Lee
National Cheng Kung Univesity, Tainan [Taiwan, China]
414
Research for Field Application of Heat Exchanger Facilities using Guided Wave
D. Gil, Y. Ahn, S. Park
Korea Electric Power Research Institute, Daejeon [Korea]
415
Ultrasonic Thickness Inspection of Oil Pipeline Based on Marginal Spectrum of Hilbert-Huang Transform
Y. Mao, P. Que, Q. Zhang
Shanghai Jiaotong University, Shanghai [China]
416
Permanent corrosion monitoring using guided waves
A. Volker, A. Mast, J. Bloom
TNO Science & Industry, Delft [Netherlands]
417
Contact defect detection in plates using guided wave and vibro-acoustic modulation
J. Jiao
1
, B. Drinkwater
2
, S. Neild
2
1
Beijing University of Technology, Beijing [China]
2
University of Bristol, Bristol [United Kingdom]
418
Visualization of weld defects in water by laser-ultrasonics
T. Miura, S. Yamamoto, M. Ochiai
Toshiba Corporation, Yokohama [Japan]
419
Research of Double Mode Ultrasonic Testing in Multi-layered Adhesive Structure of the Solid Rocket Motor
J. Zhang
North University of China, Taiyuan [China]
420
New Ultrasonic Guided Wave Testing using Remote Excitation of Trapped Energy Mode
M. Onoe
1
, K. Oka
2
, T. Suzuki
2
1
University of Tokyo, Tokyo [Japan]
2
KGK Co. Ltd., Kawasaki [Japan]
421
Feasibility Studey of Blockage Detection Inside Pipes Using Guided Ultrasonic Waves
J. Ma, M. Lowe, F. Simonetti
Imperial College , London [United Kingdom]
422
Long Range Guided Wave Pipe Inspection - the Advantages of Focusing
J. Davies, P. Cawley, M. Lowe
Imperial College , London [United Kingdom]
423
Ultrasonic Guided Waves - Evaluation of Trials for Pipeline Inspection
F. Marques
1
, A. Demma
2
1
Petrobras S.A, Rio de Janeiro [Brazil]
2
Guided Ultrasonics Limited, London [United Kingdom]
424
Propagation of torsional waves in a waveguide of arbitrary cross section immersed in a fluid
Z. Fan
1
, M. Lowe
1
, M. Castaings
2
1
Imperial College , London [United Kingdom]
2
Université Bordeaux, Talence [France]
425
Study on the Lift-off Effect of EMAT
Y. Zhang, S. Huang, W. Zhao
Tsinghua University, Beijing [China]
426
An Automatic Guided Wave Pulse Position Modulation System Using Steel Pipes as a Communication Channel for Flood Detection in Steel Offshore Oilrigs
R. Mijarez
1
, F. Martinez
1
, P. Gaydecki
2
1
Instituto de Investigaciones Eléctricas, Cuernavaca [Mexico]
2
University of Manchester, Manchester [United Kingdom]
17. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
427
TOFD Inspection with Phased Arrays
C. Brillon
1
, T. Armitt
2
, O. Dupuis
1
1
Olympus NDT, Waltham, MA [USA]
2
Lavender International NDT Consultancy Services Ltd, Sheffield [United Kingdom]
428
Inspection of thick part with Phased Array Volume Focusing
D. Braconnier, T. Murakami
KJTD Co. Ltd., Osaka [Japan]
429
2D arrays and Volume Focusing combined inspection technique
D. Braconnier, M. Takahashi
KJTD Co. Ltd., Osaka [Japan]
430
Inspection of Complex Geometries Using Flexible Phased-Array Transducers
G. Toullelan, A. Nadim, O. Casula
Commissariat Energie Atomique (CEA), Saclay [France]
431
Designing of the high spatial resolution phased array transducer for crack type distinction
Y. Kurokawa, Y. Mizutani, H. Inoue
Tokyo Institute of Technology, Tokyo [Japan]
432
on the Use of Advanced UT Phased Array Methodology and Equipment
G. Maes, D. Richard
Zetec, Quebec City, Quebec [Canada]
433
Qualification works for the mechanized Pre-service Inspection (PSI) for the Primary Circuit of the new European Pressurized Water Reactor (EPR)
J. Laube
1
, F. Lasserre
2
, G. Guse
1
1
intelligeNDT Systems & Services GmbH & Co. KG, Erlangen [Germany]
2
AREVA NP SAS, Paris [France]
434
The Ultrasonic Phased Array Inspection Technology Used in Tubular Joint Welds of Offshore Platform Structures
B. Shan, H. Wang, X. Zhao
Harbin Institute of Technology, Harbin [China]
435
Application of ultrasonic phased array in acoustic logging
B. Zhang, X. Wu, J. Gong
Chinese Academy of Science, CAS, Beijing [China]
436
Development of an Ultrasonic Ray Model for Phased Array Ultrasonic Testing in Austenitic Weldments
J. Ye, H. Kim, S. Song
Sungkyunkwan University, Suwon [Korea]
437
Prediction of side-drilled hole signals captured by a linear phased arrays with steering and focusing beams
T. Gang, X. Zhao
Harbin Institute of Technology, Harbin [China]
438
Potential new approaches to ultrasonic quantitative NDE (QNDE) by combining high speed defect reconstruction procedures based on sampling phased array techniques with probabilistic failure assessment
G. Dobmann
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
439
Qualification of Manual Phased Array Ultrasonic Techniques for Pipe Weld Inspection in Nuclear Power Plants
J. Poirier
1
, R. Ward
2
1
GE Inspection Technologies, Limonest [France]
2
GE Inspection Technologies, Lewistown, PA [USA]
440
Characterization of small defects using ultrasonic arrays: a scattering coefficient matrix approach
J. Zhang, B. Drinkwater, P. Wilcox
University of Bristol, Bristol [United Kingdom]
441
Practical Experiences in Manual Ultrasonic Phased Array Inspection
M. Berke, J. Buechler
GE Inspection Technologies, Hürth [Germany]
442
Ultrasonic phased array tools for composite inspection during maintenance and manufacturing
J. Habermehl, A. Lamarre
Olympus NDT, Waltham, MA [USA]
443
FAAST-FAST AUTOMATED ANGLE SCAN TECHNIQUE
P. Coperet
Socomate International, Crécy la Chapelle [France]
444
Manual phased arrays for weld inspections using North American codes
M. Moles
Olympus NDT, Waltham, MA [USA]
445
Application of Measurement System R&R Analysis in Ultrasonic Testing
X. Zhang, B. Chen, Y. Zhu
Nanchang Hang Kong University, Nanchang [China]
446
Ultrasonic Echo-Pulse Tomography of Concrete Using Shear Waves Low-Frequency Phased Antenna Arrays
A. Samokrutov
1
, A. Bishko
2
, V. Shevaldykin
1
1
JSC, SPECTRUM-RII, Moscow [Russia]
2
Acoustic Control Systems Ltd., Moscow [Russia]
447
Application of Phased Arrays in Combination with Virtual Dynamic Focusing for Ultrasonic Tomographic Imaging of Metals
A. Samokrutov
1
, S. Alekhin
2
, V. Shevaldykin
1
1
JSC, SPECTRUM-RII, Moscow [Russia]
2
Acoustic Control Systems Ltd., Moscow [Russia]
448
Curved Arrays for Improved Inspection of Small Pipe Welds
M. Moles, J. Zhang
Olympus NDT, Waltham, MA [USA]
449
Thick Part Inspection using Volume Focusing Technique and Large Aperture Phased Array
D. Braconnier, T. Murakami
KJTD Co. Ltd., Osaka [Japan]
450
A Breakthrough in Sputtering Target Inspections: Ultra-High Speed Phased Array Scanning with Volume Focusing
D. Braconnier, T. Murakami
KJTD Co. Ltd., Osaka [Japan]
451
Improving the Inspectability of Stainless Steel and Dissimilar Metal Welded Joints Using Inverse Phase-Matching of Phased Array Time-Domain Signals
M. Kröning
1
, A. Bulavinov
1
, K. Reddy
2
1
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
2
Qnet Engineering Ltd., Chennai [India]
452
Sampling phased array, a new technique for ultrasonic signal processing and imaging now available to industry
J. Verkooijen
1
, A. Boulavinov
2
1
Sonovation B.V., Oosterhout [Netherlands]
2
Fraunhofer-Institute for Non-Destructive Testing, IZFP, Saarbrücken [Germany]
453
Study of Ultrasonic Techniques on the inspection of NPP components
C. Hsiao, N. Shie, Y. Wu
Industrial Technology Research Institute, Taiwan [Taiwan, China]
454
Ripple and Uniformity Measurement of a Phased-Array Testing-Machine for round-Bar Testing
S. Falter
1
, J. Maier
2
, U. Tezcan
3
1
GE Inspection Technologies, Hürth [Germany]
2
Böhler Edelstahl GmbH , Kapfenberg [Austria]
3
GE Marmara Technology Center, Istanbul [Turkey]
455
Mechanical Property Analysis with Ultrasonic Phased Array
W. Song, K. Yuan, Y. Chen
Tsinghua University, Beijing [China]
456
Getting Phased Array Approvals and Certifications
M. Moles
Olympus NDT, Waltham, MA [USA]
18. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
457
Simulation of Digital Filtering to Optimize Pipe Ultrasound Wall Thickness Measurement
N. Nourrit, F. Lesage, B. Bisiaux
CEV – V&M France – Vallourec Group, Aulnoye-Aymeries [France]
458
On Line Analysis and Interpretation of Ultrasonic Images to Improve the Selectivity of the Control Installations for Steel Pipes
F. Lesage, A. Segura, B. Bisiaux
CEV – V&M France – Vallourec Group, Aulnoye-Aymeries [France]
459
The Application of Time-Frequency Transform in Mode Identification of Lamb Waves
J. Li
1
, S. Liu
2
1
Second Artillery Engineering Institute, Xi'an [China]
2
Beijing Aeronautical Manufacturing Technology Research Institute (BAMTRI) , Beijing [China]
460
Laser Ultrasonic Technique for Visualizing Ultrasonic Waves Propagating on 3-D Object
J. Takatsubo, B. Wang, H. Miyauchi
Advanced Industrial Science and Technology (AIST), Tsukuba [Japan]
461
Application of network data transmission in ultrasonic automated testing system
D. Wu, Y. Teng, Z. Zhao
Beijing Jiaotong University, Beijing [China]
462
A Modified Synthetic Aperture Focusing Technique (SAFT) by the Hilbert-Huang Transform (HHT)
C. Wang
1
, J. Tong
2
, C. Chiu
1
1
National Central University, Chungli [Taiwan, China]
2
Hungkuang University, Shalu Township, Taichung [Taiwan, China]
463
Simulation of ultrasonic fields and echo signals using cross-section photograph of test object and FDTD method
T. Kimura
1
, K. Misu
1
, M. Koike
2
1
Mitsubishi Electric Corporation, Kamakura [Japan]
2
Ryoden Shonan Electronics Corporation, Kamakura [Japan]
464
Ultrasonic Signal De-noising Using Dual Filtering Algorithm
V. Matz, M. Kreidl, R. Šmid
Czech Technical University, Prague [Czech Republic]
465
Separation of Signals Acquired with EMAT in Dual Coil Configuration
S. Štarman
1
, V. Matz
2
1
Starmans Electronics, Prague [Czech Republic]
2
Czech Technical University, Prague [Czech Republic]
466
Study on Signal Denoising in Casting Ultrasonic Testing Based on Translation Invariant
A. Qi, H. Ma, T. Liu
Xi'an University of Science and Technology, Xi'an [China]
467
The multiresolution analysis for ultrasonic non destructive evaluation
F. Bettayeb
Research center on welding and control, Algiers [Algeria]
468
Improving the material ultrasonic characterization and the signal noise ratio by the wavelet packet
F. Bettayeb
1
, S. Haciane
2
1
Research center on welding and control, Algiers [Algeria]
2
University of Science and Technology (USTHB), Algiers [Algeria]
469
Maximum nongaussianity principle for ultrasonic flaw detection
H. Lei, W. Liang, P. Que
Shanghai Jiaotong University, Shanghai [China]
470
Signal Analysis of Ultrasonic C-Scan Testing for Multi-layer Welding Structure
Z. Wang, Y. Shi, J. Liang
Beijing Institute Of Aeronautical Materials, Beijing [China]
471
Phase Reversed Image Reconstruction Method of Industrial Ultrasonic CT
Y. Chen, W. Song, K. Yuan
Tsinghua University, Beijing [China]
472
The Developments of Simulation Software for Ultrasonic Testing
H. Shan, M. Li, H. Chen
Suzhou Nuclear Power Institute, Suzhou [China]
473
Application of Ultrasonic Simulation Technology in Technical Justification of in-Service Inspection of Nuclear Power Plant
H. Chen
1
, M. Li
1
, J. Liu
2
1
Suzhou Nuclear Power Institute, Suzhou [China]
2
China Nuclear Power Technology Research Institute, Shenzhen [China]
474
Signal Processing for Guided Waves Testing Based on Magnetostrictive Effect
J. Xu
1
, X. Wu
1
, G. Shen
2
1
Huazhong University of Science and Technology, Wuhan [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
475
UMASIS, an analysis and visualization tool for developing and optimizing ultrasonic inspection techniques
J. Bloom
1
, F. Dijkstra
2
, A. Volker
1
1
TNO Science & Industry, Delft [Netherlands]
2
Applus RTD , Rotterdam [Netherlands]
476
Minimization of internal reverberation in acoustic windows used in US inspection systems by numerical simulation
M. Van der heiden, J. Bloom, A. Volker
TNO Science & Industry, Delft [Netherlands]
477
Applications of Laser-Ultrasonics and Laser-Tapping to Aerospace Composite Structures
A. Blouin, C. Neron, J. Monchalin
National Research Council of Canada (NRC), Boucherville, Quebec [Canada]
478
Applications of Laser-Ultrasonics to the Automotive Industry
A. Blouin, S. Kruger, J. Monchalin
National Research Council of Canada (NRC), Boucherville, Quebec [Canada]
479
Application of Wavelet Analysis to Signal De-noising in Ultrasonic Testing of Welding Flaws
Y. Chen, H. Ma
Xi'an University of Science and Technology, Xi'an [China]
480
Detection of Internal Rail Defects Based on the Smoothed Randon Transform in the Presence of Ultrasonic Grain Noise
M. Djeddi, P. Aknin
French National Institute for Transport and Safety Research, Arcueil [France]
481
Image processing techniques for ultrasonic inspection
H. Kieckhoefer, J. Baan, A. Mast
TNO Science & Industry, Delft [Netherlands]
482
Quantitative Defect Sizing on Components with Different Wall Thicknesses Using UT-SAFT
G. Brekow, R. Boehm, M. Kreutzbruck
Federal Institute for Materials Research and Testing (BAM), Berlin [Germany]
483
Application of the methods for processing signals from ultrasonic surface waves during the study of induction-tempered materials
Y. Ivanova
1
, T. Partalin
2
, B. Tabakova
3
1
Bulgarian Academy of Sciences, Sofia [Bulgaria]
2
Sofia University St. Kliment Ohridski, Sofia [Bulgaria]
3
Technical University Sofia, Sofia [Bulgaria]
19. SESSION:
Go to Session:
Acoustic Emission (15)
Comprehensive NDT methods (6)
Comprehensive studies and applications in NDT (49)
Computed Tomography & Digital Radiology (33)
Electromagnetic Methods (65)
Infrared Thermography (21)
Magnetic Memory (20)
Magnetic Testing (15)
NDT techniques for diverse pipelines and structures (6)
Novel applications of NDT techniques (7)
Optics (5)
Penetrant Testing (4)
Radiographic Testing & Computed Radiologic Testing (32)
Review of NDT (9)
Ultrasonic Testing (109)
Ultrasonic Testing - Guided Wave (30)
Ultrasonic Testing - Phased Array (30)
Ultrasonic Testing - Signal Processing (27)
Ultrasonic Testing - TOFD (7)
484
The Progress of TOFD Technique in China
P. Zhang
1
, G. Shen
2
, B. Hu
2
1
Tianjin Chengxinda Metal Testing Technology Co. Ltd, Tianjin [China]
2
China Special Equipment Inspection and Research Institute, Beijing [China]
485
The Application of TOFD Technique on the Large Pressure Vessel
Y. Chen
Guangdong Special Equipment Inspection Institute, Guangzhou [China]
486
IWEX: a new ultrasonic array technology for direct imaging of subsurface defects
K. Chougrani, N. Pörtzgen
Applus RTD , Rotterdam [Netherlands]
487
Depth Sizing of Surface Breaking Flaw on its Open Side by Short Path of Diffraction Technique
H. Fukutomi, S. Lin, T. Ogata
Central Research Institute of Electric Power Industry, Kanagawa [Japan]
488
Ultrasonic crack monitoring using SH waves in extreme and inaccessible environments
F. Ceglar, P. Cawley
Imperial College , London [United Kingdom]
489
Reference wavelets used for deconvolution of ultrasonic time-of-flight diffraction (ToFD) signals
F. Honarvar, A. Yaghootian
K. N. Toosi University of Technology, Tehran [Iran]
490
Application of signal processing techniques to case depth measurements by ultrasonic method
F. Honarvar, M. Zeighami
K. N. Toosi University of Technology, Tehran [Iran]
START
TOP