| Specification summary table for unicorn rotary heads | ||||
| Pipe Size Range mm | Head Speed rpm | Max no. of Channels | Testing Throughput Speed m/s | |
| URP50 | 12 - 60 | 3000 | 6 | 0.5 - 1 |
| URP100 | 25 - 115 | 2000 | 8 | 0.3 - 1 |
| URP200 | 75 - 219 | 500 - 900 | 20 | 0.25 - 0.9 |
| URP350 | 115 - 350 | 400 - 600 | 32 | 0.4 - 1.2 |
| URP500 | 115 - 508 | 300 - 450 | 36 | 0.3 - 0.9 |
The heads can be equipped for longidtudinal test only or longitudinal and wall thickness or longitudinal, transverse and thickness test. The lower testing speed given is for full longitudinal, transverse and thickness testing on the largest diameters in the range ie. the slowest head speed. Variants on these standard heads to suit specific customer requirements can also be supplied by Unicorn.