Innerspec Technologies is the World Leader in design, manufacture and commercialization of ultrasonic Electro Magnetic Acoustic Transducer (EMAT) technology for non-destructive testing of metallic parts and components.
Electro Magnetic Acoustic Transducer
'The Couplant-Free Ultrasonic Inspection for Metals'
EMAT provides all of the advantages of Ultrasonic Testing plus some unique
capabilities that make it the technique of choice for:
| Defect detection (surfaces, weld seams, volumes) in automated environments
|
| Precise thickness measurement with one-side access of hot and cold materials at production speeds
|
| Measurement of material properties (nodularity, anisotropy, grain structure) on rough surfaces without immersion tanks
|
| In-service inspections (tube & pipe, boilers, tanks, structural elements) where rough surfaces are present or when dry inspection and/or guided waves is required | | | | |
|
|
|
Home
| Article & News
| More .....
| | | |
|
| |
Ultrasonic Testing
Equipment
- Flaw detectors
- Thickness gauges
- Corrosion Thickness Gauges
- Imaging Systems
- Multi-Channel
- Phased Array Systems
Automation
- Automated flaw detection
- Scanning systems
- Laboratory systems
- Fixtures
- Manipulators
- Multi-axis control
- Portable automated Testing
Transducers (Probes)
- EMAT
Inspection Services
- Field Service
- Laboratory Services
|
EMAT Systems for In-Line Inspection
- Weld Inspection
- Volumetric Inspection of Tubes
- Volumetric Inspection of Plates/Billets/Castings
- Thickness Measurement
- Properties Measurement
|
EMAT Equipment for In-Service Inspection
- Boilers
- Pipelines
- Tanks
- ILI
|
| |
uploaded 28.04.2008
- Edit - Statistics
|
|