Calibration data set from laboratory rock sample tests
Record Control Number : 30550
Quality Validation Date : 2003-09-11
Update Date : 2003-09-25
Abstract : True tri-axial short-term strength tests have been performed on
rock samples. The samples have been taken through a 4-stage stress
history that allows the effects of stress and damage to be
individually quantified. The samples are damaged in such a way to
induce an aligned set of micro-cracks (transversely isotropic) .
A stress probe technique has been utilised to allow static modulus
values to be determined at different regions of the stress history.
Additionally ultrasonic velocity measurements have been taken in
each of the three principal directions of the sample.
The data has been processed for:
- Static modulus values.
- P-, S1-, and S2- velocity values (allowing dynamic modulus values
to be determined) .
Similar laboratory tests are planned utilising AE sensors to
determine AE event location, and magnitude with time. A subset of
the AE data is to be analysed for source mechanisms.
The data sets will be used to calibrate both the dynamic behaviour
and the static strength-reduction micro-mechanics of the AC/DC
models.
Subject Descriptors : Terrestrial science, Remote sensing, Signal processing, Software engineering
Subject Index Codes : Earth Sciences, Telecommunications, Information Processing,
Information Systems
Subject Class : Environment, IT, telecommunications
Market Applications : Environmental monitoring
Stage of Development : Scientific and/or technical knowledge (basic research)
Remarks : Results TIP
Property Rights : Copyright(s) registered
Collaboration Sought : Information exchange/Training
Sources of Support : CEC
Programmes : FP5-EAECTP C
Projects : FIKW-CT-2001-00200
Project Title : Seismic validation of 3-d thermo-mechanical models for the
prediction of the rock damage around radioactive spent fuel waste
Contact Details
Contact Name : YOUNG, R. Paul (Professor)
Position : Professor
Department : Department of Earth Sciences
Contact Organisation : University of Liverpool
Address : 4 Brownlow Street
City : Liverpool
Region : NORTH WEST (UK)
MERSEYSIDE
Postcode : L69 3GP
Country : UNITED KINGDOM
Telephone Number : +44-151-7945160
Fax Number : +44-151-7945196
Electronic Mailbox : r.p.young@liverpool.ac.uk
-------------------------------------------------------------------
Calibrated data set from laboratory rock sample tests
Record Control Number : 30556
Quality Validation Date : 2003-09-11
Update Date : 2003-09-25
Abstract : The result includes a unique data-set from laboratory tests (both
uni-axial and tri-axial) carried out on argillaceous rock samples
from the Bure en Meuse site, the potential future repository site
under investigation by ANDRA. The tests involved the collection of
ultrasonic data (both velocity and acoustic emission measurements)
as well as standard rock mechanics rock response parameters.
The data set provides an improved understanding of the behaviour of
these argillaceous rock types under different stress histories,
particularly in terms of their ultrasonic response. This is of
importance for the interpretation of data collected during in situ
tests using, for example, the tools developed in the OMNIBUS
project. In addition the experience and expertise gained from
having designed the protocol for these tests and subsequently
conducting them will provide the partner conducting these tests
with the opportunity to exploit them in terms of future consultancy
services.
Subject Descriptors : Pollution, Protection technologies, Terrestrial science, Remote sensing
Subject Index Codes : Environmental Protection, Earth Sciences, Telecommunications
Subject Class : Environment, IT, telecommunications
Market Applications : Environmental monitoring
Stage of Development : Scientific and/or technical knowledge (basic research)
Remarks : Results TIP
Property Rights : Secret know-how
Collaboration Sought : Information exchange/Training
Sources of Support : CEC
Programmes : FP5-EAECTP C
Projects : FIKW-CT-2001-00202
Project Title : Development of the tools and interpretation techniques for
ultrasonic surveys to monitor the rock barrier around radioactive
waste packages
Contact Details
Contact Name : BALLAND, Cyrille (Mr)
Position : Project Leader
Department : Department of Ground & Underground Risks
Ecole des Mines
Contact Organisation : INERIS
Address : Parc de Saurupt
City : Nancy Cedex
Region : EST
LORRAINE
Meurthe-et-Moselle
Postcode : 54042
Country : FRANCE
Telephone Number : +33-3-83584289
Fax Number : +33-3-83533849
Electronic Mailbox : cyrille.balland@mines.u-nancy.fr
-------------------------------------------------------------------
© Copyright NDT.net, info@ndt.net
| NDTnet|