| No. | Title | Author | Ref.
|
| 1 | Bulk Wave Characterization of Laminated Composites | Kline, R., Kennedy, B. | QNDE 1996, Vol. 15//B, S. 1167 -
|
| 2 | Validity of the Elastic Constant Approximations for the Ultrasonic Evaluation of Multi-Layered Inhomogeneous Composites | Ji, Y., Balasubramaniam, K., Givens, T. | QNDE 1996, Vol. 15//B, S. 1183 -
|
| 3 | Dynamic Effects in Ultrasonic Determination of Composite Moduli Using Velocity Data | Rokhlin, S. I., Huang, W. | QNDE 1996, Vol. 15//B, S. 1199 -
|
| 4 | Ultrasonic Velocities of C/AL Composites Determined by Laser Ultrasonic Method | Gan, C. M., Fei, D., Zhang, S. Y. ... | QNDE 1996, Vol. 15//B, S. 1215 -
|
| 5 | Use of Ultrasonic Lamb Waves for In-Process Porosity Inspection of the Pultrusion Process: Theoretical Velocity Calculations | Gillespie, J. W., Fecko, D. L., Steiner, K. V. | QNDE 1996, Vol. 15//B, S. 1231 -
|
| 6 | Ultrasonic NDE Techniques and the Effects of Flaws on Mechanical Performance in Multi-Directionally Reinforced Textile Composites | Hsu, D. K., Hale, R. D., Adams, D. O. | QNDE 1996, Vol. 15//B, S. 1247 -
|
| 7 | Quantitative Ultrasonic Characterization of Metal Matrix Composite Fiber/Matrix Interfacial Failure | Matikas, T. E., Gundel, D. B., Karpur, P. ... | QNDE 1996,Vol. 15//B, S. 1263 -
|
| 8 | Characterization of Composite Materials from Temporal Thermal Response | Winfree, W. P., Emeric, P. R. | QNDE 1996, Vol. 15//B, S. 1275 -
|
| 9 | Guided Waves for Composite Patch Repair of Aging Aircraft | Rajana, K. M., Rose, J. L., Barshinger, J. N. | QNDE 1996, Vol. 15//B, S. 1291 -
|
| 10 | The Use of Temperature Pulses to Detect Debonding of Honeycomb Sandwich Panels | Emery, A. F., Dauksher, W. | QNDE 1996, Vol. 15//B, S. 1305 -
|
| 11 | Measurement of Adhesion Strength of Bonds Using Nonlinear Acoustics | Arnold, W., Fassbender, S. U. | QNDE 1996, Vol. 15//B, S. 1321 -
|
| 12 | Backscatter from Specific Regions of Human Hearts Obtained from Standard Echocardiographic Views | Gussak, H. M., Finch-Johnston, A. E., Mobley, J. ... | QNDE 1996, Vol. 15//B, S. 1335 -
|
| 13 | Linear and Nonlinear Ultrasonic Properties of Fatigued 410Cb Stainless Steel | Cantrell, J. H., Na, J. K., Yost, W. T. | QNDE 1996, Vol. 15//B, S. 1347 -
|
| 14 | Nonlinear Acoustic Assessment of Precipitation-Induced Coherency Strains in Aluminum Alloy 2024 | Yost, W. T., Cantrell, J. H. | QNDE 1996, Vol. 15//B, S. 1361 -
|
| 15 | Applications of SH Mode for Measurement of Anisotropic Properties of Solids | Sachse, W., Baker, A. R., Every, A. G. ... | QNDE 1996, Vol. 15//B, S. 1375 -
|
| 16 | Structure of Magnetic Fields in High Temperature Superconductors with Columnar Defects | Ledvij, M., Benkraouda, M. | QNDE 1996, Vol. 15//B, S. 1391 -
|
| 17 | Type Discrimination of Various Welding Defects Created during Production and In-Service Use | Gray, T. A., Rehbein, D. K. | QNDE 1996, Vol. 15//B, S. 1407 -
|
| 18 | Elastic Constants Determination of the Thin Cold-Rolled Stainless Steel by Acoustic Resonance Method | Ahn, B. Y., Min, U.-S., Yoo, S. H. ... | QNDE 1996, Vol. 15//B, S. 1423 -
|
| 19 | Ultrasonic Attenuation Measurements at 300 MHz | Moreau, A., Viens, M., Jen, C. K. ... | QNDE 1996, Vol. 15//B, S. 1439 -
|
| 20 | A Critical Analysis of the Theoretical Basis of Ultrasonic Scattering Measurements | Foister, S. A. M., Anson, L. W., McKenzie, S. G. ... | QNDE 1996, Vol. 15//B, S. 1455 -
|
| 21 | A Generalized Model of the Effects of Microstructure on Ultrasonic Backscattering and Flaw Detection | Thompson, R. B. | QNDE 1996, Vol. 15//B, S. 1471 -
|
| 22 | Survey of Ultrasonic Grain Noise Characteristics in Jet Engine Titanium | Han, K. Y., Margetan, F. J., Thompson, R. B. ... | QNDE 1996, Vol. 15//B, S. 1487 -
|
| 23 | Determination of Grain-Size Distributions from Ultrasonic Attenuation | Nicoletti, D., Anderson, A. | QNDE 1996, Vol. 15//B, S. 1503 -
|
| 24 | The Statistical Distribution of Grain Noise in Ultrasonic Images | Burkel, R. H., Howard, P. J., Gilmore, R. S. | QNDE 1996, Vol. 15//B, S. 1517 -
|
| 25 | Analysis of Mechanical Damage Detection in Gas Pipeline Inspection | Creek, E. A., Burkhardt, G. L., Crouch, A. E. ... | QNDE 1996, Vol. 15//B, S. 1533 -
|
| 26 | Estimation of Grinding Burn Damage Using Barkhausen Technique | Gupta, H., Jiles, D. C., Jalics, S. ... | QNDE 1996, Vol. 15//B, S. 1547 -
|
| 27 | Photothermal and Photoacoustic Investigation of Zirconia Coating Delaminations | Salerno, A., Fenici, P., Varis, J. ... | QNDE 1996, Vol. 15//B, S. 1559 -
|
| 28 | Eddy Current Characterization of Flaws in NiCoCrAlY-Coated Nickel-Base Superalloys | Moulder, J., Larson, B., Zombo, P. | QNDE 1996, Vol. 15//B, S. 1573 -
|
| 29 | Ultrasonic Evaluation of Case Depth in Case-Carburized Steel Components | Leeper, D., Mitra, R., Fuquen, R. ... | QNDE 1996, Vol. 15//B, S. 1589 -
|
| 30 | Surface Characterization of Material Using Rayleigh Velocity Measurement in the Broad-Band Mode | Noroy, M., Tardy, F., Paradis, L. ... | QNDE 1996, Vol. 15//B, S. 1605 -
|
| 31 | Ultrasonic Predictions of Plastic Strain Ratios in Steel Sheet | Anderson, A. J., Thompson, R. B., Izworski, N. ... | QNDE 1996, Vol. 15//B, S. 1621 -
|
| 32 | Acoustoelastic Measurement of Second- and Third-Order Elastic Constants in Silicon Carbide and Alumina Particulate-Reinforced Aluminum Metal Matrix Composites | Krikorian, S., Saigal, A., Leisk, G. G. | QNDE 1996, Vol. 15//B, S. 1637 -
|
| 33 | Absolute Ultrasonic Measurements of Residual Stresses | Degtyar, A. D., Lavrentyev, A. I., Rokhlin, S. I. | QNDE 1996, Vol. 15//B, S. 1653 -
|
| 34 | Wave Propagation in Stressed Composites | Huang, W., Degtyar, A. D., Rokhlin, S. I. | QNDE 1996, Vol. 15//B, S. 1669 -
|
| 35 | Effect of Texture on Ultrasonic Backscattering Coefficient in Pure Titanium Plate | Yalda, I., Thompson, R. B., Margetan, F. J. ... | QNDE 1996, Vol. 15//B, S. 1685 -
|
| 36 | Texture Assessment in SCS-6 Fibers from Ultrasonic Dispersion Measurements | Kent, R. M., Nagy, P. B. | QNDE 1996, Vol. 15//B, S. 1701 -
|
| 37 | Characterization of Corrosion in Aluminum Alloys Using Nuclear Magnetic Resonance | Snyderman, D. M., Palmer, D. D., Conradi, M. S. | QNDE 1996, Vol. 15//B, S. 1717 -
|
| 38 | Improved Measurements of Samples Simulating Corrosion in Lap-Seams of Aluminum Aircraft | Zinke, O. H., Schmidt, W. F. | QNDE 1996, Vol. 15//B, S. 1733 -
|
| 39 | Thermal Wave Imaging of Disbonding and Corrosion on Aircraft | Hah, X., Ahmed, T., Wang, L. ... | QNDE 1996, Vol. 15//B, S. 1747 -
|
| 40 | Depth Determination of Surface-Breaking Cracks in Concrete Slabs Using a Self-Compensating Ultrasonic Technique | Achenbach, J. D., Cheng, A. | QNDE 1996, Vol. 15//B, S. 1763 -
|
| 41 | A Pulse Compression Ultrasonic Test Instrument and Its Applications | Misu, K., Nagatsuka, T., Kimura, T. ... | QNDE 1996, Vol. 15//B, S. 1779 -
|
| 42 | A Novel Inductive System for Two-Dimensional Imaging of Reinforcing Components in Concrete Structures: From Hardware to Image Enhancement | Glossop, K. J., Gaydecki, P. A., Burdekin, F. M. | QNDE 1996, Vol. 15//B, S. 1791 -
|
| 43 | Improved Assessment of Concrete Dams Using Sonic Tomography | Bond, L. J., Kepler, W. F. | QNDE 1996, Vol. 15//B, S. 1807 -
|
| 44 | A Rolling Weight Deflectometer for Quantitative Pavement Measurements | Bondurant, P. D., Johnson, R. F., Marvin, M. H. | QNDE 1996, Vol. 15//B, S. 1823 -
|
| 45 | Ultrasonic and Electromagnetic Wave Propagation and Inverse Scattering Applied to Concrete | Baermann, R., Langenberg, K. J., Bradfass, M. ... | QNDE 1996, Vol. 15//B, S. 1839 -
|
| 46 | New Work in Acoustic Leak Location in Underground Pipelines | Roberts, R., Clark, M. A., Rewerts, L. E. | QNDE 1996, Vol. 15//B, S. 1853 -
|
| 47 | Ultrasonic Inspection of an Underwater Piping System Covered with Thick Coating | Salcedo, J., Azcuaga, V. F. G., Adler, L. | QNDE 1996, Vol. 15//B, S. 1867 -
|
| 48 | A New Approach to Automated Labeling of Internal Features of Hardwood Logs Using CT Images | Li, P., Schmoldt, D. L., Abbott, A. L. | QNDE 1996, Vol. 15//B, S. 1883 -
|
| 49 | Nondestructive Evaluation of Cracks in Porous Building Materials by Use of Crawling Spot Thermal Technique | Braggiotti, A., Grinzato, E., Mazzoldi, A. ... | QNDE 1996, Vol. 15//B, S. 1895 -
|
| 50 | Ultrasonic Scan Control and Analysis Using Carla Datasets | Woodmansee, W. E., Uhl, K. M. | QNDE 1996, Vol. 15//B, S. 1909 -
|
| 51 | Ultrasonic Width and Thickness Monitoring System in a Lamination Process | Velazquez, J. J., Marcial, M. A. | QNDE 1996, Vol. 15//B, S. 1925 -
|
| 52 | Generation of Axial Shear Acoustic Resonance by Magnetostrictively Coupled EMAT | Hirao, M., Ogi, H., Minoura, K. | QNDE 1996, Vol. 15//B, S. 1939 -
|
| 53 | PACE: An Advanced Structure for Handling Multitechnique NDT Data | Vailhen, O., Lesne, J. L., Nouailhas, B. ... | QNDE 1996, Vol. 15//B, S. 1953 -
|
| 54 | Fatigue Monitoring System Progress | Cao, Q., Ling, F., Li, W. ... | QNDE 1996, Vol. 15//B, S. 1969 -
|
| 55 | Methodology for Estimating Nondestructive Evaluation Capability | Chiou, C.-P., Thompson, R. B., Jeng, S.-L. ... | QNDE 1996, Vol. 15//B, S. 1983 -
|
| 56 | Iowa Demonstration Laboratory for NDE Applications Project Review | Brasche, L., Larson, B., Utrata, D. | QNDE 1996, Vol. 15//B, S. 1999 -
|
| 57 | Interpretation of Surface Wave Signals following Multiple Specular Reflections in an Acoustic Microscope | Thompson, R. B., Johnson, J. C. | QNDE 1996, Vol. 15//B, S. 2015 -
|
| 58 | Acoustic Microscopy of Advanced Aerospace Materials | Fox, J. A., Ruddell, M. J., Matikas, T. E. ... | QNDE 1996, Vol. 15//B, S. 2031 -
|
| 59 | Recent Developments with the Dripless Bubbler Ultrasonic Scanner | Hsu, D. K., Patton, T. C. | QNDE 1996, Vol. 15//B, S. 2045 -
|
| 60 | Surface Monitoring by Combination of an Optical Sensor and an Ultrasonic Scanning System | Gindorf, A., Bamberg, J., Steinhauser, L. | QNDE 1996, Vol. 15//B, S. 2061 -
|
| 61 | Synthetic Aperture Focusing Techniques in the Near Field of a Focused Transducer | Udpa, S. S., Mina, M., Udpa, L. ... | QNDE 1996, Vol. 15//B, S. 2073 -
|
| 62 | Joint Time-Frequency Processing of Ultrasonic Signals | Jin, X. M., Malik, M. A., Saniie, J. | QNDE 1996, Vol. 15//B, S. 2089 -
|
| 63 | Integrity Monitoring of Pressurized Gas Cylinders Using the SSUE Technique | Afzal, M. A. K., Kayani, J. K., Wormley, S. J. ... | QNDE 1996, Vol. 15//B, S. 2105 -
|
| 64 | Effects of System's Limitations on the Accuracy of Measured Ultrasonic Correlated Signal | Gray, T., Jeong, P., Schmerr, L. | QNDE 1996, Vol. 15//B, S. 2117 -
|
| 65 | Development and Testing of Rotating Probe Method for Airframe Rivet Inspection | Todhunter, R., Fulton, J., Simpson, J. ... | QNDE 1996, Vol. 15//B, S. 2133 -
|
| 66 | Compensated High-Bandwidth Laser Ultrasonic Detector Based on Photo-Induced EMF in GaAs | McCahon, S. W., Dunning, G. J., Klein, M. B. ... | QNDE 1996, Vol. 15//B, S. 2149 -
|
| 67 | Optical Lock-In Vibration Detection Using Photorefractive Four-Wave Mixing | Telschow, K., Chatters, T. | QNDE 1996, Vol. 15//B, S. 2165 -
|
| 68 | Quantitative Measurement of Chrome Loss by Optical Means | Watson, M. D., Bondurant, P. D. | QNDE 1996, Vol. 15//B, S. 2181 -
|
| 69 | Noncontact Measurement of Applied Static Torque | Schmidt, W. F., Zinke, O. H. | QNDE 1996, Vol. 15//B, S. 2197 -
|
| 70 | Industrial Applications of Laser-Based Profilometry | Correa, M. A., Doyle, J. L., Bondurant, P. D. | QNDE 1996, Vol. 15//B, S. 2211 -
|
| 71 | In-Process Monitoring for Quality Assurance of Automated Composite Fabrication | Soucy, K. A. | QNDE 1996, Vol. 15//B, S. 2225 -
|
| 72 | Eddy Current Determination of Semiconductor Liquid-Solid Interface Location and Shape | Wadley, H. N. G., Dharmasena, K. P. | QNDE 1996, Vol. 15//B, S. 2241 -
|
| 73 | Remote Laster-Based Ultrasonic Inspection of Weld Joints for High Volume Industrial Applications | Klein, M. B., Mitchell, P. V., Pepper, D. M. ... | QNDE 1996, Vol. 15//B, S. 2257 -
|
| 74 | Ultrasonic Gauging for On-Line Inspection of Tubes | Frankel, J., Abbate, A., Reed, R. W. | QNDE 1996, Vol. 15//B, S. 2273 -
|
| 75 | Determination of a New Ultrasonic Indicator to Follow the Concrete Setting in Real Time | Corneloup, G., Garnier, V. | QNDE 1996, Vol. 15//B, S. 2289 -
|
| 76 | The Evolution of a Nuclear Fuel Welding and Ultrasonic Inspection Machine for Improved Quality and Process Control | Landry, J. D., Kiernan, M. T. | QNDE 1996, Vol. 15//B, S. 2305 -
|
| 77 | Analysis of Compressibility Origins in Monolithic Ceramic Suspensions Using X-Ray Imaging Techniques | Gray, J. N., Huss, S. P., Schilling, C. H. | QNDE 1996, Vol. 15//B, S. 2323 -
|
| 78 | Data Fusion for Chemical Process Monitoring, Control and Optimization | Eaton, M., Ricker, N. L. | QNDE 1996, Vol. 15//A, S. 25 -
|
| 79 | Modeling of Ultrasonic Signals from Weak Inclusions | Margetan, F. J., Chiou, C.-P., Thompson, R. B. | QNDE 1996, Vol. 15//A, S. 49 -
|
| 80 | Ultrasonic Modeling of Real-Life NDT Situations: Applications and Further Developments | Klaholz, S., Langenberg, K. J., Kostka, J. ... | QNDE 1996, Vol. 15//A, S. 57 -
|
| 81 | Numerical Simulation of Pulsed Pressure Waves in Attenuative and Dispersive Media | Ludwig, R., Wismer, M. G. | QNDE 1996, Vol. 15//A, S. 73 -
|
| 82 | Distance Amplitude Correction Factors for Immersion Ultrasonic Measurements through Curved Surfaces | Garton, M., Gray, T., Zombo, P. | QNDE 1996, Vol. 15//A, S. 89 -
|
| 83 | Elastic Wave Scattering by an Interface Crack in Layered Materials | Yin, J.-H., Kitahara, M. | QNDE 1996, Vol. 15//A, S. 105 -
|
| 84 | Numerical Model of Elastic Wave Interactions with a Diffusion Bond | Zhou, J., Saffari, N. | QNDE 1996, Vol. 15//A, S. 113 -
|
| 85 | Coherent and Incoherent Scattering Mechanisms in Air-Filled Permeable Materials | Nagy, P. B. | QNDE 1996, Vol. 15//A, S. 129 -
|
| 86 | A Computationally Efficient Modeling Code for SH-Waves in Austenitic Welds Using an Explicit Space-Time Green-Function | Kroening, M., Spies, M. | QNDE 1996, Vol. 15//A, S. 145 -
|
| 87 | Green's Function for Lamb's Problem and Rayleigh Wave Propagation in General Transversely Isotropic Materials | Kroning, M., Spies, M. | QNDE 1996, Vol. 15//A, S. 161 -
|
| 88 | Geometry and Diffraction Effects in Acoustic Beam Reflection Studies from a Fluid-Loaded Plate | Safaeinili, A., Lobkis, O. I., Chimenti, D. E. | QNDE 1996, Vol. 15//A, S. 177 -
|
| 89 | The Existence of Low Loss Lamb Modes in Highly Attenuative Media | Cawley, P., Chan, C.-W. | QNDE 1996, Vol. 15//A, S. 193 -
|
| 90 | Lamb Wave Scattering from Rivets | Hinders, M. K. | QNDE 1996, Vol. 15//A, S. 209 -
|
| 91 | Guided Wave Mode Propagation Influence for a Shear Horizontal Wave Source in an Anisotropic Viscoelastic Layer | Menon, S. M., Pelts, S. P., Rose, J. L. | QNDE 1996, Vol. 15//A, S. 223 -
|
| 92 | Leaky Lamb Wave along VCR Magnetic Tapes | Yokota, K., Hirao, M., Fukuoka, H. | QNDE 1996, Vol. 15//A, S. 239 -
|
| 93 | Lamb Wave Propagation in Thermally Damaged Composites | Smith, B. T., Seale, M. D. | QNDE 1996, Vol. 15//A, S. 261 -
|
| 94 | Axisymmetric Waves in Layered Anisotropic Fibers and Composites | Nagy, P. B., Nayfeh, A. H. | QNDE 1996, Vol. 15//A, S. 275 -
|
| 95 | Aperture Integral Ultrasonic Pulse Transmission Model | Roberts, R. A. | QNDE 1996, Vol. 15//A, S. 291 -
|
| 96 | Ultrasonic Wave Propagation through Nozzles and Pipes with Claddings around Their Inner Walls | Thompson, R. B., Minachi, A. | QNDE 1996, Vol. 15//A, S. 307 -
|
| 97 | Lamb Waves Propagation in Aluminum Honeycomb Structures | Lim, M. K., Guo, N. | QNDE 1996, Vol. 15//A, S. 323 -
|
| 98 | Recent Developments in Modeling Eddy-Current Probe-Flaw Interactions | Woo, L. W., Murphy, R. K., Sabbagh, E. H. ... | QNDE 1996, Vol. 15//A, S. 331 -
|
| 99 | Forward and Inverse Processing in Electromagnetic NDE Using SQUIDs | Donaldson, G. B., Cochran, A., McNab, A. ... | QNDE 1996, Vol. 15//A, S. 347 -
|
| 100 | Edge Crack Detection: A Theoretical and Experimental Study | Nakagawa, N., Chao, J., Moulder, J. C. ... | QNDE 1996, Vol. 15//A, S. 361 -
|
| 101 | Wavelet Expansions in Volume Integral Method of Eddy-Current Modeling | Basart, J. P., Wang, B., Moulder, J. C. | QNDE 1996, Vol. 15//A, S. 377 -
|
| 102 | Optimal Multidimensional Multifrequency Eddy Current Mixing Techniques | Fisher, J. L., Bartels, K. A. | QNDE 1996, Vol. 15//A, S. 393 -
|
| 103 | Thickness and Conductivity of Metallic Layers from Pulsed Eddy Current Measurements | Rose, J. H., Tai, C.-C., Moulder, J. C. | QNDE 1996, Vol. 15//A, S. 409 -
|
| 104 | Effect of Phase Delay on Low Frequency Operation of Flux Focusing Eddy Current Probe | Fulton, J., Wincheski, B. | QNDE 1996, Vol. 15//A, S. 417 -
|
| 105 | Underwater X-Ray Tomography Using Compton Backscatter Imaging | Chow, J., Draper, C., Levenberry, L. ... | QNDE 1996, Vol. 15//A, S. 433 -
|
| 106 | A Practical Algorithm for Reconstruction from X-Ray Backscatter Data | Poranski, C. F., Ham, Y. S., Greenawald, E. C. | QNDE 1996, Vol. 15//A, S. 449 -
|
| 107 | Heavy Metal Contamination Detection Using X-Rays | Gray, J. N., Jensen, T., Robinson, D. ... | QNDE 1996, Vol. 15//A, S. 465 -
|
| 108 | Dual-Energy Computed Tomography for Ceramics and Composite Materials | Dinten, J. M., Robert, C., Rizo, P. | QNDE 1996, Vol. 15//A, S. 481 -
|
| 109 | Mathematical Modelling of Transient Thermography and Defect Sizing | Almond, D. P., Saintey, M. B. | QNDE 1996, Vol. 15//A, S. 503 -
|
| 110 | Early-Time Pulse-Echo Thermal Wave Imaging | Kuo, P. K., Favro, L. D., Thomas, R. L. ... | QNDE 1996, Vol. 15//A, S. 519 -
|
| 111 | Thermal Ellipsometry: A Tool Applied for In-Depth Resolved Characterization of Fibre Orientation in Composites | Krapez, J.-C. | QNDE 1996, Vol. 15//A, S. 533 -
|
| 112 | Simulations on the Accuracy of Laser-Flash Data Analysis Methods | Fenici, P., Volcan, A., Fabbri, L. ... | QNDE 1996, Vol. 15//A, S. 549 -
|
| 113 | 3D Finite Element Methods for Modeling MFL Inspection of Pipelines | Lord, W., Si, J. T., Sun, Y. S. ... | QNDE 1996, Vol. 15//A, S. 561 -
|
| 114 | Characterization of Surfaces and Coatings Using Laser-Generated Ultrasonic Surface Waves | Knight, B. E., Schroeder, S. C., Yee, F. ... | QNDE 1996, Vol. 15//A, S. 585 -
|
| 115 | Shear Wave Wedge for Laser Ultrasonics | Balasubramaniam, K., Shah, V., Singh, J. ... | QNDE 1996, Vol. 15//A, S. 601 -
|
| 116 | Injection Locked Laser Sensor for Ultrasonic Sensing | Burger, C. P., Smith, J. A. | QNDE 1996, Vol. 15//A, S. 615 -
|
| 117 | Heterodyne Detection of Ultrasound from Rough Surfaces Using a Double Phase Conjugate Mirror | Drolet, D., Blouin, A., Monchalin, J.-P. ... | QNDE 1996, Vol. 15//A, S. 631 -
|
| 118 | Fiberized Sagnac Interferometer for Ultrasound Measurement | Krishnaswamy, S., Fomitchov, P., Achenbach, J. D. | QNDE 1996, Vol. 15//A, S. 645 -
|
| 119 | Optical Techniques to Examine the Scattering of Rayleigh Surface Waves | Jacobs, L. J., Bruttomesso, D. A. | QNDE 1996, Vol. 15//A, S. 651 -
|
| 120 | Phase Stepping Shearography for Testing Commercial Aircraft Structures: An Application Review of Advanced Image Processing Techniques for Shearography | Scherling, D., Bisle, W. J., Tober, G. | QNDE 1996, Vol. 15//A, S. 665 -
|
| 121 | Detection/Location of Small Flaws in Composite Structures Using Microwaves | Farina, D. J., Flam, R. P., Liu, J. M. | QNDE 1996, Vol. 15//A, S. 679 -
|
| 122 | Microwave Sensors for Imaging Moisture and Flaws in Advanced Composites | King, R., Werner, M. | QNDE 1996, Vol. 15//A, S. 693 -
|
| 123 | Air-Gap Detection in Dielectric Materials by a Step-Frequency Microwave Technique | Liu, J. M. | QNDE 1996, Vol. 15//A, S. 705 -
|
| 124 | Electromagnetic Modeling of the Interaction of Cracks in Metallic Surfaces with Open-Ended Waveguides Using an Equivalent Magnetic Current | Ganchev, S., Abiri, H., Zoughi, R. ... | QNDE 1996, Vol. 15//A, S. 719 -
|
| 125 | Wavelet Transform Signal Processing Applied to Ultrasonics | Frankel, J., Abbate, A., Das, P. | QNDE 1996, Vol. 15//A, S. 741 -
|
| 126 | Improvement of Time Reversal Processing in Titanium Inspections | Fink, M., Miette, V., Wu, F. | QNDE 1996, Vol. 15//A, S. 757 -
|
| 127 | Optimum Filter Based Techniques for Data Fusion | Mina, M., Udpa, S. S., Udpa, L. ... | QNDE 1996, Vol. 15//A, S. 773 -
|
| 128 | Testing for Nongaussian Fluctuations in Grain Noise | Donohue, K. D., Neal, S. P. | QNDE 1996, Vol. 15//A, S. 789 -
|
| 129 | Fuzzy Inference Systems for Invariant Pattern Recognition in MFL NDE | Udpa, S. S., Udpa, L., Lord, W. ... | QNDE 1996, Vol. 15//A, S. 805 -
|
| 130 | Registration Issues in the Fusion of Eddy Current and Ultrasound NDE Data Using Q-Transforms | Udpa, L., Udpa, S. S., Xue, T. ... | QNDE 1996, Vol. 15//A, S. 813 -
|
| 131 | Edge Detection on Eddy Current Image to Increase Defect Characterization | La, R., Attaoui, P., Lengelle, R. ... | QNDE 1996, Vol. 15//A, S. 829 -
|
| 132 | Conductivity Imaging in Plates Using Current Injection Tomography | Rousakov, S. V., Staton, D. J., Wikswo, J. P. | QNDE 1996, Vol. 15//A, S. 845 -
|
| 133 | Computed Tomography Using Laser-Based Ultrasonics | Achenbach, J. D., Huang, J., Krishnaswamy, S. ... | QNDE 1996, Vol. 15//A, S. 861 -
|
| 134 | Development of a New Method for the Inspection of a 3D Volume of Ultrasonic Data | Guerault, F., Corneloup, G., Roy, O. ... | QNDE 1996, Vol. 15//A, S. 875 -
|
| 135 | Virtual Reality for Nondestructive Evaluation Applications | Udpa, S., Mandayam, S., Lord, W. ... | QNDE 1996, Vol. 15//A, S. 897 -
|
| 136 | A Novel Image Processing Algorithm for Enhancing the Probability of Detection of Flaws in X-Ray Images | Udpa, L., Elshafiey, I., Gray, J. N. ... | QNDE 1996, Vol. 15//A, S. 903 -
|
| 137 | Improvement to Defect Detection by Ultrasonic Data Processing: The DTVG Method | Moysan, J., Corneloup, G., Francois, D. | QNDE 1996, Vol. 15//A, S. 917 -
|
| 138 | Strategies for Characterizing Transducers and Measurement Systems | Thompson, D. O., Thompson, R. B., Schmerr, L. W. | QNDE 1996, Vol. 15//A, S. 931 -
|
| 139 | Metal Diffusion Bonded Transducers for Resonant Ultrasound Spectroscopy (RUS) | Migliori, A., Darling, T. W., Dixon, R. D. | QNDE 1996, Vol. 15//A, S. 947 -
|
| 140 | Wideband Nonuniformly Excited Focused Transducers - Theory and Experiments | De Vadder, D., Lhemery, A., Gengembre, N. | QNDE 1996, Vol. 15//A, S. 963 -
|
| 141 | Observation of Shear Wave Modes in the Echoes of the Longitudinal Wave Transducer | Lee, J. K., Kim, Y. H., Kim, H. C. | QNDE 1996, Vol. 15//A, S. 987 -
|
| 142 | Acoustic Waves Generated by a Transient Point Source in an Anisotropic Medium: Comparison between Theory and Experiment | Mourad, A., Audoin, B., Deschamps, M. | QNDE 1996, Vol. 15//A, S. 1003 -
|
| 143 | Broadband Fields Radiated in a Solid by Water-Coupled Transducers: A Comparison of Approximate Models, Numerical Approaches and Experiments | Lhemery, A., Calmon, P., Nadal, J. | QNDE 1996, Vol. 15//A, S. 1019 -
|
| 144 | Design and Optimization of a Multifunctional Phased Array Search Unit | Kroning, M., Gebhardt, W., Dalichow, M. H. ... | QNDE 1996, Vol. 15//A, S. 1035 -
|
| 145 | Air-Coupled Ultrasound and Leaky Lamb Waves in Composites | Lobkis, O. I., Safaeinili, A., Chimenti, D. E. | QNDE 1996, Vol. 15//A, S. 1059 -
|
| 146 | Air-Coupled Ultrasonic Bulk Waves to Measure Elastic Constants in Composite Materials | Hutchins, D. A., Hosten, B., Schindel, D. W. | QNDE 1996, Vol. 15//A, S. 1075 -
|
| 147 | A New ECT Probe with Rotating Direction Eddy Current | Koyama, K., Hoshikawa, H. | QNDE 1996, Vol. 15//A, S. 1091 -
|
| 148 | Computer Assisted Eddy Current Probe Design | Nakagawa, N., Prasad, A. N. S., Raulerson, D. ... | QNDE 1996, Vol. 15//A, S. 1105 -
|
| 149 | High Sensitivity AC Field Measurement Using Rhombic Inducer | Mostafavi, R. F., Mirshekar-Syahkal, D. | QNDE 1996, Vol. 15//A, S. 1121 -
|
| 150 | Magnetoresistive Eddy-Current Sensor for Detecting Deeply Buried Flaws | Avrin, W. F. | QNDE 1996, Vol. 15//A, S. 1145 -
|
| 151 | Magneto-Optic/Eddy Current Imaging of Subsurface Corrosion and Fatigue Cracks in Aging Aircraft | Skaugset, R. L., Thorne, D. K., Shih, W. C. L. ... | QNDE 1996, Vol. 15//A, S. 1159 -
|
| 152 | Low Frequency Guided Plate Wave Propagation in Fiber Reinforced Composites | Bar-Cohen, Y., Lih, S.-S., Mal, A. K. | QNDE 1996, Vol. 15//B, S. 1175 -
|
| 153 | Application of Shear Waves for Composite Laminate Characterization | Hsu, D. K., Fischer, B. A. | QNDE 1996, Vol. 15//B, S. 1191 -
|
| 154 | Acoustic Emission Analysis of SCS-6 Fiber Fracture in Titanium Matrix Composites | Wadley, H. N. G., Sypeck, D. J. | QNDE 1996, Vol. 15//B, S. 1207 -
|
| 155 | Characterization of Static- and Fatigue-Loaded Carbon Composites by X-Ray CT | Brand, H. R., Martz, H. E., Groves, S. E. ... | QNDE 1996, Vol. 15//B, S. 1223 -
|
| 156 | The Effect of Porosity Density and Configuration in Composite Materials on the Ultrasonic Waveform | Ellsworth, S., Vaccaro, C., Pettit, D. ... | QNDE 1996, Vol. 15//B, S. 1239 -
|
| 157 | Eddy Current Detection of Fatigue Microcrack Distributions in Al-SiC Composites | Meshii, M., Lawson, L., Moulder, J. C. ... | QNDE 1996, Vol. 15//B, S. 1255 -
|
| 158 | Thermography for Honeycomb Panel Inspection | Thompson, J. G. | QNDE 1996, Vol. 15//B, S. 1271 -
|
| 159 | Influence of the Frequency Behavior of Arall and Glare on the Ultrasonic C-Scan Inspection | Modderman, T. M. | QNDE 1996, Vol. 15//B, S. 1283 -
|
| 160 | Evaluation of Adhesion Integrity in Graphite Epoxy Bonded Structures Using Ultrasonic Reflection Factor Analysis | Balasubramaniam, K., Sullivan, R. W., Bennett, G. | QNDE 1996, Vol. 15//B, S. 1299 -
|
| 161 | Ultrasonic Evaluation of Titanium Alloy Diffusion Bonding | Perocchi, L. C., Gigliotti, M. F. X., Gilmore, R. S. ... | QNDE 1996, Vol. 15//B, S. 1313 -
|
| 162 | Ultrasonic Evaluation of Quality Attributes in Live Beef Animals Using Real-Time B-Mode Ultrasound Imaging | Wilson, D., Izquirdo, M., Rouse, G. ... | QNDE 1996, Vol. 15//B, S. 1329 -
|
| 163 | Determination of Elastic Parameters of Pharmaceutical Materials Using a Fiber Interferometer | Raatikainen, P., Oksanen, M., Luukkala, M. ... | QNDE 1996, Vol. 15//B, S. 1341 -
|
| 164 | Plastic Strain Ratio and Texture Coefficients in Orthotropic Sheets of Cubic Metals | Ao, Q., Man, C.-S. | QNDE 1996, Vol. 15//B, S. 1353 -
|
| 165 | A Nondestructive Observation of the Mechanism of Plastic Deformation in Orthogonal Cutting | Ruud, C. O., Park, Y. W., Cohen, P. H. | QNDE 1996, Vol. 15//B, S. 1367 -
|
| 166 | Crack Size Detection Capability of Acoustic Emission | Crump, T. N., Fowler, T. J., Barnes, C. A. | QNDE 1996, Vol. 15//B, S. 1383 -
|
| 167 | Material Properties of Aged and Unaged Inconel 718 as Determined from Nondestructive and Destructive Tests | Kameda, J., Rehbein, D. K., Buck, O. ... | QNDE 1996, Vol. 15//B, S. 1399 -
|
| 168 | Determination of Elastic Constants by Line-Focus V(Z) Measurements of Multiple SAW Modes | Achenbach, J. D., Li, W. | QNDE 1996, Vol. 15//B, S. 1415 -
|
| 169 | Materials Characterization by a Time-Resolved and Polarization-Sensitive Ultrasonic Technique | Hsu, N. N., Xiang, D., Blessing, G. V. | QNDE 1996, Vol. 15//B, S. 1431 -
|
| 170 | Thermal Effects in the Fracture of Rubber-Modified Polystyrene | Wu, Z., Telenkov, S. A., Favro, L. D. ... | QNDE 1996, Vol. 15//B, S. 1447 -
|
| 171 | Variance of the Ultrasonic Signal from a Defect beneath a Rough Surface | Rose, J. H., Bilgen, M. | QNDE 1996, Vol. 15//B, S. 1463 -
|
| 172 | An Experimental Investigation of Ultrasonic 'Grain Noise' in Titanium-6AL-4V | McKenzie, S. G., Foister, S. A. M., Chivers, R. C. | QNDE 1996, Vol. 15//B, S. 1479 -
|
| 173 | Ultrasonic Noise and the Volume of the Ultrasonic Pulse | Gilmore, R. S., Howard, P. J. | QNDE 1996, Vol. 15//B, S. 1495 -
|
| 174 | Predicting Gated-Peak Grain Noise Distributions for Ultrasonic Inspections of Metals | Yalda, I., Margetan, F. J., Thompson, R. B. | QNDE 1996, Vol. 15//B, S. 1509 -
|
| 175 | Ultrasonic Attenuation Measurements in Jet-Engine Titanium Alloys | Yalda, I., Margetan, F. J., Thompson, R. B. ... | QNDE 1996, Vol. 15//B, S. 1525 -
|
| 176 | Metal Loss Characterization in 55-Gallon Drum Steel by the Magnetic Flux Leakage Method | Riechers, D., Hockey, R., Duncan, D. | QNDE 1996, Vol. 15//B, S. 1539 -
|
| 177 | Time Resolved Infrared Radiometry for Subsurface Interface Imaging | Spicer, J. W. M., Osiander, R., Murphy, J. C. | QNDE 1996, Vol. 15//B, S. 1551 -
|
| 178 | Subsurface Defect Detection in Ceramic Materials Using Optical Gating Techniques | Duncan, M., Battle, P. R., Mahon, R. ... | QNDE 1996, Vol. 15//B, S. 1565 -
|
| 179 | Eddy Current Measurement of Thicknesses in Multiple-Layered Film | Sun, Y. S., Cooley, D., Udpa, S. S. | QNDE 1996, Vol. 15//B, S. 1581 -
|
| 180 | Surface Elastic Wave Measurements for Determination of Steel "Hardness Gradients | 1996, Vol. 15//B, S. 1597 - | QNDE 1996, Vol. 15//B, S. 1597 -
|
| 181 | Ultrasonic NDE of Sprayed Ceramic Coatings | Blessing, G. V., Slotwinski, J. A. | QNDE 1996, Vol. 15//B, S. 1613 -
|
| 182 | Using Rayleigh Wave Dispersion to Characterize Residual Stresses | Jiang, L., Kline, R. | QNDE 1996, Vol. 15//B, S. 1629 -
|
| 183 | Effect of Shear Modes Interference in Anisotropic Materials | Lavrentyev, A. I., Degtyar, A. D., Rokhlin, S. I. | QNDE 1996, Vol. 15//B, S. 1645 -
|
| 184 | Absolute Determination of Elastic Constants and Stresses from Ultrasonic Group Velocity Data | Rokhlin, S. I., Degtyar, A. D. | QNDE 1996, Vol. 15//B, S. 1661 -
|
| 185 | Determination of Angular Parallaxes between the Geometric Coordinate System and the Material Symmetry Coordinate System of Anisotropic Materials | Baste, S., Aristegui, C. | QNDE 1996, Vol. 15//B, S. 1677 -
|
| 186 | Effect of Wave Types on Ultrasonic Texture Identification | Min, S., Lu, W., Hughes, D. | QNDE 1996, Vol. 15//B, S. 1693 -
|
| 187 | Nondestructive Ultrasonic Characterization of the Orientation Distribution of Short-Fiber Composites | Ledbetter, H., Dunn, M. L. | QNDE 1996, Vol. 15//B, S. 1709 -
|
| 188 | Quantitative Measurement of Metal Loss Due to Corrosion in Aluminum Aircraft Skin | Dayal, V., Patton, T. C., Hinzie, B. L. ... | QNDE 1996, Vol. 15//B, S. 1725 -
|
| 189 | Nondestructive Evaluation of Corrosion through Insulation | Austin, R., Carriveau, G. W. | QNDE 1996, Vol. 15//B, S. 1741 -
|
| 190 | Eddy-Current Detection of Pitting Corrosion in Aircraft Lap-Splices | Moulder, J. C., Satveli, R., Rose, J. H. | QNDE 1996, Vol. 15//B, S. 1755 -
|
| 191 | Application of Spread-Spectrum Ultrasonic Evaluation to Concrete Structures | Kayani, J. K., Russell, S. F., Wormley, S. J. ... | QNDE 1996, Vol. 15//B, S. 1771 -
|
| 192 | Defect Detection in Concrete Bridge Decks Using Radar | Bhandarkar, V., Chen, H. L., Sami, Z. ... | QNDE 1996, Vol. 15//B, S. 1787 -
|
| 193 | Ultrasonic NDT Prototype for the Inspection of Ducted Post Stressing Tendons in Concrete Beams | Gaydecki, P. A., Duncan, P. J., Burdekin, F. M. | QNDE 1996, Vol. 15//B, S. 1799 -
|
| 194 | Assessment of Industrial Floor Slabs Using Nondestructive Testing Methods | Biggs, D. T., Rogers, H. D., Kanonik, M. C. ... | QNDE 1996, Vol. 15//B, S. 1815 -
|
| 195 | A Coring Method for the Nondestructive Evaluation of Effective Prestress Force in Prestressed Concrete Structures | Wang, J., Pessiki, S. | QNDE 1996, Vol. 15//B, S. 1831 -
|
| 196 | Long Range Bridge Girder Evaluation Using Lamb Waves | Parashis, A., White, K. R., Carrica, V. ... | QNDE 1996, Vol. 15//B, S. 1847 -
|
| 197 | The Inspection of Chemical Plant Pipework Using Lamb Waves: Defect Sensitivity and Field Experience | Lowe, M., Alleyne, D., Cawley, P. | QNDE 1996, Vol. 15//B, S. 1859 -
|
| 198 | On-Site Ultrasonic Inspection of Highway Culverts | Frankel, J., Schroeder, S. C., Abbate, A. | QNDE 1996, Vol. 15//B, S. 1875 -
|
| 199 | Nondestructive Evaluation of Green Dimension Lumber Using Stress Wave and Transverse Vibration Techniques | Gangarao, H. V. S., Bidigalu, G. M., Ross, R. J. ... | QNDE 1996, Vol. 15//B, S. 1891 -
|
| 200 | High Performance Ultrasonic Inspection of Tubes | Giraud, J. P., De Vareilles, O., Lasserre, F. | QNDE 1996, Vol. 15//B, S. 1903 -
|
| 201 | Adaptation of a Marine Echo-Sounder to Support UST Remediation Activities at Hanford Nuclear Reservation | Clark, M. A., Marmaras, C., Martin, D. M. | QNDE 1996, Vol. 15//B, S. 1917 -
|
| 202 | Application of Dynamic Adaptive Focusing System to Ultrasonic Nondestructive Testing | Roy, O., Cattiaux, G., Acounis, H. ... | QNDE 1996, Vol. 15//B, S. 1931 -
|
| 203 | Nuclear Waste Drum Characterization with Mobile Tomographic Assay and NDE | Entwistle, D., Bernardi, R. T., Swinford, J. | QNDE 1996, Vol. 15//B, S. 1945 -
|
| 204 | A Thermal Imaging System for Crack Growth Quantification in Thermo-Mechanical Fatigue Specimens | Mueller, A., White, G., Torrington, G. | QNDE 1996, Vol. 15//B, S. 1961 -
|
| 205 | Raising the Reliability of NDE by Combination and Standardisation of NDT-Data Using the Trappist System | Johannsen, K., Heine, S., Schumm, A. ... | QNDE 1996, Vol. 15//B, S. 1975 -
|
| 206 | Probability of Detection for Applied Ultrasonic Inspection | Tucker, W. T., Sturges, D. J., Gilmore, R. S. ... | QNDE 1996, Vol. 15//B, S. 1991 -
|
| 207 | A New Technique for Surface Acoustic Wave Speed Measurement in Laterally Inhomogeneous Materials | Kundu, T., Maslov, K. I., Ghosh, T. | QNDE 1996, Vol. 15//B, S. 2007 -
|
| 208 | Development of an Apertured-Confocal Acoustic Microscope | Lulay, K. E. | QNDE 1996, Vol. 15//B, S. 2023 -
|
| 209 | A Digital Signal Processing for Measuring Leaky Surface Wave Velocity with C-Scan Acoustic Microscope | Sato, T., Fujii, I., Okade, M. ... | QNDE 1996, Vol. 15//B, S. 2039 -
|
| 210 | A Guided Wave Resonance Matching Technique for in Situ Monitoring of Powder Injection Molded Products | Yi, R., Menon, S. M., German, R. M. ... | QNDE 1996, Vol. 15//B, S. 2053 -
|
| 211 | Measurement of Viscosity in Liquids Using Reflection Coefficient Phase Difference Method | Costley, R. D., Balasubramaniam, K., Singh, J. ... | QNDE 1996, Vol. 15//B, S. 2067 -
|
| 212 | Impact of Quantization Noise on the Quality of Ultrasonic Signal Deconvolution | Fortunko, C. M., Renken, M. C. | QNDE 1996, Vol. 15//B, S. 2081 -
|
| 213 | Choice of Coded Waveform and Correlation Filter for Self-Noise Suppression in Ultrasonic Correlation Systems | Russell, S. F., Kayani, J. K. | QNDE 1996, Vol. 15//B, S. 2097 -
|
| 214 | Nondestructive Testing Potential of a Magnetoacoustic Storage Correlator (MASC) | Oksanen, M., Ermolov, V., Luukkala, M. | QNDE 1996, Vol. 15//B, S. 2113 -
|
| 215 | Two Dimensional Multi-Frequency Eddy Current Data Fusion | Udpa, S. S., Yim, J., Udpa, L. ... | QNDE 1996, Vol. 15//B, S. 2125 -
|
| 216 | Eddy Current Inspection of Threaded Fasteners | Green, R. E., Schlegel, J., Friant, C. L. | QNDE 1996, Vol. 15//B, S. 2141 -
|
| 217 | An Application of Holographic Interferometry to Evaluate the Dynamics and Material Characteristics of Cast Compliant Structures | Fein, H. | QNDE 1996, Vol. 15//B, S. 2157 -
|
| 218 | Automated Laser Scatter Detection of Near-Surface Defects and Machining Damage in Ceramic Components | Ellingson, W. A., Steckenrider, J. S. | QNDE 1996, Vol. 15//B, S. 2173 -
|
| 219 | Optimization of Neural Network Parameters for Defect Characterization | Yeoh, C. H., Chao, M., Mandayam, S. ... | QNDE 1996, Vol. 15//B, S. 2189 -
|
| 220 | Induction Coil Shape and Size Considerations in Magnetic Field Measurement with Spatially Fast Varying Distribution 1996, Vol. 15//B, S. 2203 - | Toosi, B., Sadeghi, S. H. H. | QNDE 1996, Vol. 15//B, S. 2203 -
|
| 221 | Minimum-Norm Least-Squares Inverse for Magnetic Flux Leakage Image Reconstruction | Bruno, A. C. | QNDE 1996, Vol. 15//B, S. 2219 -
|
| 222 | A Prototype Apparatus for Determining Changes in the Electrical Conductivity of Production Run Carbon Fibers | Dulcie, L. L. | QNDE 1996, Vol. 15//B, S. 2233 -
|
| 223 | Magnetic Flux Leakage Inspection of Moving Steel Sheets | Shin, Y.-K. | QNDE 1996, Vol. 15//B, S. 2249 -
|
| 224 | Resonance Inspection for Quality Control | Rhodes, G. W., Schwar, J. J. | QNDE 1996, Vol. 15//B, S. 2265 -
|
| 225 | Wall Thickness Measurements in Hot Steel Pipe Using Non-Contact Ultrasound | Rohani, M. S., Edwards, C., Palmer, S. B. ... | QNDE 1996, Vol. 15//B, S. 2281 -
|
| 226 | Acoustic Waveguide Cure Curves for Materials Ranging from Fast Cure Resins to Slow Cure Concrete | Sanjana, Z. N., Harrold, R. T., Brynsvold, R. | QNDE 1996, Vol. 15//B, S. 2297 -
|
| 227 | A Process Sensor for Locating the Liquid-Solid Boundary through the Mold of a Casting | Siewert, T. A., Dube, W. P., Paran, J. ... | QNDE 1996, Vol. 15//B, S. 2315 -
|
| 228 | Novel X-Ray Imaging Method for Evaluating Defect Evolution in Ceramic Tapes | Gray, J. N., Maranville, C. W., Schilling, C. H. | QNDE 1996, Vol. 15//B, S. 2331 -
|
| 229 | Chemical Non-Destructive Evaluation at the Center for Process Analytical Chemistry | Koch, J. E., Kowalski, B. R. | QNDE 1996, Vol. 15//A, S. 1 -
|
| 230 | Optical Sensors for Direct Measurements in Chemical Processes | Burgess, L. W. | QNDE 1996, Vol. 15//A, S. 9 -
|
| 231 | The Use of Spectral Methods in Predicting the Reflection and Transmission of Ultrasonic Signals through Flaws | Emery, A. F., Dauksher, W. | QNDE 1996, Vol. 15//A, S. 33 -
|
| 232 | Elastic Wave Diffraction at Cracks in Anisotropic Materials | Temple, J. A. G., Lewis, P. A., Wickham, G. R. | QNDE 1996, Vol. 15//A, S. 41 -
|
| 233 | Mechanical Reciprocity Principles and Ultrasonic Measurement Models | Sedov, A., Schmerr, L. W. | QNDE 1996, Vol. 15//A, S. 65 -
|
| 234 | Theoretical Predictions and Experimental Measurements of Echo Responses from Tilted Flat-Bottomed Holes | Weight, J. P., Lhemery, A. | QNDE 1996, Vol. 15//A, S. 81 -
|
| 235 | Defect Sizing Using Distance-Gain-Size Diagrams for Flat-Bottomed Holes in a Solid: Theoretical Analysis and Experimental Verification | Hussein, S. A., Weight, J. P. | QNDE 1996, Vol. 15//A, S. 97 -
|
| 236 | Spring and Asymptotic Boundary Condition Models for Study of Scattering by Thin Cylindrical Interphases | Rokhlin, S. I., Huang, W. | QNDE 1996, Vol. 15//A, S. 121 -
|
| 237 | Modeling and Parameter Estimation of Ultrasonic Back- Scattered Echoes | Jin, X. M., Demirli, R., Saniie, J. | QNDE 1996, Vol. 15//A, S. 137 -
|
| 238 | Mathematical Modelling of the Rayleigh Wave Reception by the System with Elastic Waveguide | Pelts, S. P., Shikchman, V. M. | QNDE 1996, Vol. 15//A, S. 153 -
|
| 239 | Dispersion of Guided Circumferential Waves in a Circular Annulus | Berthelot, Y., Qu, J., Li, Z. | QNDE 1996, Vol. 15//A, S. 169 -
|
| 240 | Lamb Wave Propagation across a Lap Joint | Guo, D., Chang, Z., Mal, A. K. | QNDE 1996, Vol. 15//A, S. 185 -
|
| 241 | Scattering Analysis and Simulation for Lamb Wave Ultrasonic Testing | Yamano, M., Hirose, S. | QNDE 1996, Vol. 15//A, S. 201 -
|
| 242 | Guided Wave Behavior Analysis in Multi-Layered Inhomogeneous Anisotropic Plates | Sullivan, R., Ji, Y., Balasubramaniam, K. | QNDE 1996, Vol. 15//A, S. 217 -
|
| 243 | Lamb Wave Mode Sensitivity to Detect Various Material Defects in Multilayered Composite Plates | Matikas, T. E., Karpur, P., Nicolaou, P. D. ... | QNDE 1996, Vol. 15//A, S. 231 -
|
| 244 | Utility of Lamb Waves for Near Surface Crack Detection | Cho, Y., Rajana, K. M., Rose, J. L. | QNDE 1996, Vol. 15//A, S. 247 -
|
| 245 | Lamb Wave Modes Propagating along Arbitrary Directions in an Orthotropic Plate | Zhang, S. Y., Cheng, J. C. | QNDE 1996, Vol. 15//A, S. 253 -
|
| 246 | Perturbation and Finite Difference Solutions for Wave Propagation in Composites with Periodic Stiffness Variations | Kline, R. A., Rasmussen, M. L., Bert, C. W. ... | QNDE 1996, Vol. 15//A, S. 267 -
|
| 247 | Efficient Modeling of Finite Acoustic Beam Excitation and Detection of Interface and Bulk Waves on Planar and Cylindrical Fluid-Solid | Zeroug, S. | QNDE 1996, Vol. 15//A, S. 283 -
|
| 248 | Finite Element Modeling of Transient Wave Phenomena at Solid/Fluid Interfaces | Udpa, S., Lord, W., Udpa, L. ... | QNDE 1996, Vol. 15//A, S. 299 -
|
| 249 | Absorbing Boundary Conditions with Zero Reflection Angles for Compressional and Shear Incident Waves | Saffari, N., Zhou, J. | QNDE 1996, Vol. 15//A, S. 315 -
|
| 250 | Extended Magnetic Potential Method for Quasi-Static Electromagnetism and Eddy Current Phenomena | Chao, J., Nakagawa, N. | QNDE 1996, Vol. 15//A, S. 339 -
|
| 251 | Eddy Current Flow Near an Edge: A Comparison between Stratton-Chu and Magnetic Potential Formulations | Moulder, J. C., Lehther, D., Nakagawa, N. ... | QNDE 1996, Vol. 15//A, S. 355 -
|
| 252 | Analytical Solutions to the Problem of Eddy Current Probes Consisting of Long Parallel Conductors | Mertes, C., Lesage, O., Ptchelintsev, A. ... | QNDE 1996, Vol. 15//A, S. 369 -
|
| 253 | Three Dimensional Simulation of Remote Field Eddy Current Nondestructive Testing Phenomena | Qu, M. X., Chen, M. J., Sun, Y. S. ... | QNDE 1996, Vol. 15//A, S. 385 -
|
| 254 | Depth-Selective SQUID Eddy Current Techniques for Second Layer Flaw Detection | Wikswo, J. P., Ma, Y. P. | QNDE 1996, Vol. 15//A, S. 401 -
|
| 255 | Optimization Tool for X-Ray Radiography NDE | Gray, J. N., Elshafiey, I. | QNDE 1996, Vol. 15//A, S. 425 -
|
| 256 | A Model of X-Ray Film Response | Gray, J. N., Aljundi, T., Wallingford, R. ... | QNDE 1996, Vol. 15//A, S. 441 -
|
| 257 | Temporal Response of Terbium Glass Scintillator Used for X-Ray Tomography and Radiography | Winfree, W. P., West, M. S. | QNDE 1996, Vol. 15//A, S. 457 -
|
| 258 | Segmentation and Density-Evaluation of Fiber-Reinforced Materials by Dual-Energy Computerized Tomography | Rizo, P., Hassler, U., Garnero, L. | QNDE 1996, Vol. 15//A, S. 473 -
|
| 259 | Application of 3D X-Ray CT Data Sets to Finite Element Analysis | Brand, H. R., Martz, H. E., Hollerbach, K. ... | QNDE 1996, Vol. 15//A, S. 489 -
|
| 260 | X-Ray Computed Tomography Application Research | Yancey, R. N., Neel, S. T. | QNDE 1996, Vol. 15//A, S. 497 -
|
| 261 | Applications of Lockin-Thermography Methods | Karpen, W., Rantala, J., Zenzinger, G. ... | QNDE 1996, Vol. 15//A, S. 511 -
|
| 262 | Precise Thermal NDE for Quantifying Structural Damage | Durbin, P. F., Del Grande, N. K. | QNDE 1996, Vol. 15//A, S. 525 -
|
| 263 | Time-Resolved Microwave Thermoreflectometry for Infrastructure Inspection | Chang, Y., Osiander, R., Hildebrand, R. ... | QNDE 1996, Vol. 15//A, S. 541 -
|
| 264 | Linearized MFL Model for Embedded Flaw Detection in Rails | Udpa, S. S., Udpa, L., Athavale, A. S. ... | QNDE 1996, Vol. 15//A, S. 553 -
|
| 265 | Magnetic Particle Inspection Simulation Model | Udpa, S. S., Udpa, L., Zhang, Z. ... | QNDE 1996, Vol. 15//A, S. 569 -
|
| 266 | Laser Ultrasonic Thermoelastic/Ablation Generation with Laser Interferometric Detection in Graphite/Polymer Composites | Mehl, J. B., Caron, J. N., Steiner, K. V. | QNDE 1996, Vol. 15//A, S. 577 -
|
| 267 | Narrow Band Laser Ultrasonics NDE | Burger, C. P., Duffer, C. E. | QNDE 1996, Vol. 15//A, S. 593 -
|
| 268 | Laser Ultrasonic Detection of the Solidification Front during Casting | Telschow, K. L., Walter, J. B. | QNDE 1996, Vol. 15//A, S. 607 -
|
| 269 | A Laser Interferometric Method for Small- and Finite-Amplitude Ultrasonic Waves' Detection in Transparent Medi | Quentin, G., Jia, X., Adler, L. | QNDE 1996, Vol. 15//A, S. 623 -
|
| 270 | Specifications of an Ultrasonic Receiver Based on Two-Wave Mixing in Photorefractive Gallium Arsenide Implemented in a Laser-Ultrasonic System | Neron, C., Blouin, A., Monchalin, J.-P. ... | QNDE 1996, Vol. 15//A, S. 637 -
|
| 271 | A Fiber Optic Ultrasound Sensor for Monitoring the Cure of Epoxy | Krishnaswamy, S., Dorighi, J., Achenbach, J. D. | QNDE 1996, Vol. 15//A, S. 657 -
|
| 272 | A Compact Digital Phase-Stepping Shearography System | Wu, S., Bard, B. A., Tittmann, B. R. | QNDE 1996, Vol. 15//A, S. 673 -
|
| 273 | Preliminary Results of Microwave Non-Contact Detection and Depth Determination of Disbonds in Low Permitivity and Low Loss Thick Sandwich Composites | Zoughi, R., Ganchev, S., Carriveau, G. W. ... | QNDE 1996, Vol. 15//A, S. 686 -
|
| 274 | A Microwave Transducer for Detecting Conductive Surfaces beneath Protective Coatings | Heil, G. G., Domalewski, J. J., Hoyt, J. K. ... | QNDE 1996, Vol. 15//A, S. 701 -
|
| 275 | Effects of Lift-Off on Microwave NDE Using an Open-Ended Rectangular Waveguide | Matteson, M. A., Liu, J. M. | QNDE 1996, Vol. 15//A, S. 713 -
|
| 276 | Near-Field Analysis of Rectangular Waveguide Probes Used for Imaging | Ganchev, S., Abiri, H., Zoughi, R. ... | QNDE 1996, Vol. 15//A, S. 727 -
|
| 277 | An Application of Wavelet Signal Processing to Ultrasonic Nondestructive Evaluation | DeFacio, B., Van Nevel, A., Neal, S. P. | QNDE 1996, Vol. 15//A, S. 733 -
|
| 278 | Echo Extraction from an Ultrasonic Signal Using Continuous Wavelet Transform | Sallard, J., Roy, O., Moubarik, S. E. | QNDE 1996, Vol. 15//A, S. 749 -
|
| 279 | Singular Value Decomposition of Wigner Distribution for Time-Frequency Representation of Ultrasonic Echoes | Malik, M. A., Jin, X. M., Saniie, J. | QNDE 1996, Vol. 15//A, S. 765 -
|
| 280 | Quantitative Evaluation of Defects by Fuzzy Reasoning Based on Principal Component Analysis | Yabe, Y., Mandai, T., Kitahara, M. ... | QNDE 1996, Vol. 15//A, S. 781 -
|
| 281 | Crack Parameter Characterization by a Neural Network | Guo, Q. C., Achenbach, J. D., Kitahara, M. ... | QNDE 1996, Vol. 15//A, S. 797 -
|
| 282 | Introduction of the Signature Classification Development System | Lin, J. S., Brown, L. M. | QNDE 1996, Vol. 15//A, S. 821 -
|
| 283 | Eddy Current Image Restoration Using the Groshong Parametric Model | Maury, H., Philippe, J.-M., Villard, D. ... | QNDE 1996, Vol. 15//A, S. 837 -
|
| 284 | High Resolution Image Reconstruction of Polymer Composite Materials Using Neural Networks | Mottram, J. T., Hutchins, D. A., Hines, E. L. ... | QNDE 1996, Vol. 15//A, S. 853 -
|
| 285 | Ultrasonic Imaging of Anomalies in Truck Tires | Rogers, R., Achenbach, J. D., Peterson, M. ... | QNDE 1996, Vol. 15//A, S. 869 -
|
| 286 | A New Technique for Distinguishing Internal Voids from Solid Inclusions | Kundu, T., Maslov, K. I., Lobkis, O. I. | QNDE 1996, Vol. 15//A, S. 883 -
|
| 287 | Magneto-Optic Image Classification Using Neural Networks | Fulton, J. P., Nath, S., Wincheski, B. | QNDE 1996, Vol. 15//A, S. 891 -
|
| 288 | Imaging Flaws under Insulation Using a SQUID Magnetometer | Zimmerman, J. E., Barbosa, C. H., Ribeiro, P. C. ... | QNDE 1996, Vol. 15//A, S. 911 -
|
| 289 | Imaging of Creep Damaged CrMo Steel Piping Using Magnetic Parameter Variations | Jiles, D. C., Negley, M. A. | QNDE 1996, Vol. 15//A, S. 925 -
|
| 290 | Determination of the Absolute Sensitivity Limit of a Piezoelectric Displacement Transducer | Fortunko, C. M., Boltz, E. S. | QNDE 1996, Vol. 15//A, S. 939 -
|
| 291 | The Effect of Dust and Surface Roughness on the Efficiency of Solid Coupled Wheel Probes | Cawley, P., Drinkwater, B. | QNDE 1996, Vol. 15//A, S. 955 -
|
| 292 | A New Ultrasonic Transducer Combining Three Modes: High Axial Resolution, High Transverse Resolution and Standard Modes | Lhemery, A., De Vadder, D., Gengembre, N. | QNDE 1996, Vol. 15//A, S. 979 -
|
| 293 | Transient Analysis of a Line-Focus Transducer Probing a Liquid/Solid Interface | Fick, S. E., Xiang, D., Blessing, G. V. ... | QNDE 1996, Vol. 15//A, S. 995 -
|
| 294 | Modeling the Ultrasonic Radiation of Shear Wave Angle Beam Transducers | Schmerr, L. W., Lerch, T. P., Sedov, A. | QNDE 1996, Vol. 15//A, S. 1011 -
|
| 295 | Interrogating a Thin Layer of Heterogeneity with Confocal Transducers | Rebinsky, D. A., Harris, J. G., Wickham, G. | QNDE 1996, Vol. 15//A, S. 1027 -
|
| 296 | The Response of an Air-Coupled Ultrasonic Transducer for Various Backplates and Apertures | Hutchins, D. A., Bashford, A. G., Schindel, D. W. | QNDE 1996, Vol. 15//A, S. 1043 -
|
| 297 | Non-Contact Ultrasonic Tomography Imaging Using Air-Coupled Capacitance Transducers | Hutchins, D. A., Wright, W. M. D., Schindel, D. W. | QNDE 1996, Vol. 15//A, S. 1051 -
|
| 298 | Quantitative Materials Characterization of Elastic Plates Using Air-Coupled Leaky Lamb Waves | Safaeinili, A., Chimenti, D. E., Lobkis, O. I. | QNDE 1996, Vol. 15//A, S. 1067 -
|
| 299 | Air-Coupled Ultrasonic Transducers for the Detection of Defects in Plates | Farlow, R., Cawley, P., Hayward, G. ... | QNDE 1996, Vol. 15//A, S. 1083 -
|
| 300 | Passive Pulsed Eddy Current Inspection of Sheet Metal | Ferris, R., Riechers, D., Kelley, R. ... | QNDE 1996, Vol. 15//A, S. 1099 -
|
| 301 | Application of Self-Nulling Eddy Current Probe and Spin-Off Sensor Technologies to Airline Industries and Beyond | Namkung, M. | QNDE 1996, Vol. 15//A, S. 1113 -
|
| 302 | The Emergence of Extended Field Technology in the Air Force | Price, L. S., Keppler, E. E., Nuxoll, G. ... | QNDE 1996, Vol. 15//A, S. 1129 -
|
| 303 | Inspection of Metallic Plates Using a Novel Remote Field Eddy Current NDT Probe | Lord, W., Udpa, S. S., Cooley, D. ... | QNDE 1996, Vol. 15//A, S. 1137 -
|
| 304 | Advances in the Theory and Practice of SQUID NDE | Carr, C., Donaldson, G. B., McKirdy, D. M. ... | QNDE 1996, Vol. 15//A, S. 1151 - |