TOC- MAY 01 1996: Russian journal of nondestructive testing


Related departments:
1. Publications for UT Literature incl. Books
2. An UT bibliographical List
3. List to all TOCs beginning with the 26th week of 1996, with an explanation: "What is a TOC?".

Subject: UnCover Reveal - Russian journal of nondestructive testing


JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 353
AU Builo, S.I.
TI Statistical Models for Qualitative Evaluation of the Distortion of the
   Amplitude Distribution of Acoustic Emission Pulses and for Increasing the
   Reliability of the Acoustic Emission Method.
SI 1061-8309(19960501)32:5L.353:SMQE;1-
>>                UnCover #:  251,080,211,250               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 331
AU Gurvich, A.K.
AU Entigen, I.Z.
TI Error of Determination of the Position of a Conventional Defective Area
   in Ultrasonic Inspection of Welded Joints.
SI 1061-8309(19960501)32:5L.331:EDPC;1-
>>                UnCover #:  251,080,211,192               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 337
AU Lange, Yu. V.
AU Voropaev, S.I.
AU Nefedov, S.N.
TI Spectra of Pulsed Signals of Transducers of a Low-Frequency Acoustic
   Flaw Detectors.
SI 1061-8309(19960501)32:5L.337:SPST;1-
>>                UnCover #:  251,080,211,222               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 348
AU Builo, S.I.
TI Probability-Information Aspects of Evaluation of the Reliability of
   Results of Nondestructive Inspection and Diagnostics of the Strength of
   Solids.
SI 1061-8309(19960501)32:5L.348:PAET;1-
>>                UnCover #:  251,080,211,231               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 361
AU Komarov, V.A.
AU Il'yasov, R.S.
AU Lomaeva, V.P.
TI Dependence of the Efficiency of Inhomogeneous Magnetostrictive
   Electromagnetic-Acoustic Conversion on the Macroscopic Properties of the
   Medium.
SI 1061-8309(19960501)32:5L.361:DEIM;1-
>>                UnCover #:  251,080,212,003               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 368
AU Strelkov, V.I.
AU Zagidulin, R.V.
TI SAT Borehole Acoustic Televiewer.
SI 1061-8309(19960501)32:5L.368:SBAT;1-
>>                UnCover #:  251,080,212,007               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 378
AU Kogan, L. Kh.
AU Pashagin, O.A.
AU Polenova, V.N.
TI Eddy-Current Monitoring of the Depth and Hardness of Surface-Hardened
   Layers of Manufactured Articles Using Superimposed Transducers.
SI 1061-8309(19960501)32:5L.378:EMHO;1-
>>                UnCover #:  251,080,212,014               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 383
AU Sidorenko, A.S.
TI A Computerized Eddy-Current System for Monitoring the Wall Thickness of
   Turbine Blades Made of Heat-Resistant Alloys.
SI 1061-8309(19960501)32:5L.383:CESM;1-
>>                UnCover #:  251,080,212,018               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 390
AU Fastriskii, V.S.
AU Vingris, L.T.
AU Mazversitis, I.T.
TI Analysis of the Feasibility of Eddy-Current Monitoring of Hardened
   Layers of Feromagnetic Materials.
SI 1061-8309(19960501)32:5L.390:AFM;1- 
>>                UnCover #:  251,080,212,022               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 393
AU Ul'yanov, A.I.
AU Zakharov, V.A.
AU Arsent'eva, N.B.
TI A Method of Coercive Force Measurement with Surface-Mounting Magnetic
   Devices.
SI 1061-8309(19960501)32:5L.393:MCFW;1-
>>                UnCover #:  251,080,212,027               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 399
AU Rigmant, M.B.
AU Gorkunov, E.S.
AU Chernova, G.S.
TI Instrument for Measuring the Content of Ferritic Phase Ferritometer
   FM-3IFM.
SI 1061-8309(19960501)32:5L.399:IMCF;1-
>>                UnCover #:  251,080,212,032               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 404
AU Chugunov, A.A.
AU Shlepnev, I.O.
AU Mareev, K.A.
TI Eddy-Current Flaw Detection in Elements of Sectional Blanks for Making
   Superconducting Leads with the Aid of a Computerized System of Signal
   Processing.
SI 1061-8309(19960501)32:5L.404:EFDS;1-
>>                UnCover #:  251,080,212,035               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 411
AU Sazhina, E. Yu.
TI Optimization of the Service Characteristics of Holding Electromagnets.
SI 1061-8309(19960501)32:5L.411:OSC;1- 
>>                UnCover #:  251,080,212,040               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 418
AU Novikov, V.F.
AU Kostryukova, N.K.
AU Rybnikova, O.I.
TI Change in the Magnetostriction of Certain Steels During the Initial
   Stages of Plastic Deformation.
SI 1061-8309(19960501)32:5L.418:CMCS;1-
>>                UnCover #:  251,080,212,042               
  
JT Russian journal of nondestructive testing.      
DA MAY 01 1996 v 32 n 5
PG 423
AU Sharando, V.I.
AU Novikov, S.A.
TI Study of Galvanic Coatings by the Thermoelectric and
   Magnetic-Separation Methods with Different Application and Heat-Treatment
   Conditions.
SI 1061-8309(19960501)32:5L.423:SGCT;1-
>>                UnCover #:  251,080,212,045           -- --------------------------------------------------------------------------------------
The REVEAL Alert service is provided by the UnCover Company.  If you    
need further information or assistance, please phone us at              
800.787.7979 (outside the US at 303.758.3030), or send e-mail to        
uncover@carl.org.  Thank you for using REVEAL.                          

|NDTnet ||Top|