Back: |List to all TOCs| |NDTnet|

TOC - September 2000 : NDT plus

A Manually selection by use of the Keyword alert of 'non-destructive testing', 'nondestructive testing' and 'eddy current'
                       
    
JT Polymer engineering and science.
DA JUL 01 2000 v 40 n 7
PG 1628   
AU Ferreira, M.   
AU Lam, T.M.   
AU Delvael, Y.   
TI Nondestructive Testing of Polyaramide Cables by Longitudinal Wave   
   Propagation: Study of the Dynamic Modulus.   
SU SI 0032-3888(20000701)40:7L.1628:NTP;1-   
AV Article availability and price:                     
$  19.25 Total  =  10.00 Service +   5.25 Copyright +  4.00 Fax Surch.         
>>                 UnCover #:  251,129,091,206          
  
JT Surface & coatings technology.
DA AUG 21 2000 v 130 n 2 / 3
PG 233   
AU Fu, L.   
AU Khor, K.A.   
AU Teo, T.N.   
TI Non-destructive evaluation of plasma sprayed functionally graded thermal   
   barrier coatings.   
SI 0257-8972(20000821)130:2:3L.233:NEPS;1-   
AV Article availability and price:                     
$  34.00 Total  =  10.00 Service +  20.00 Copyright +  4.00 Fax Surch.         
>>                 UnCover #:  251,129,138,065          
  
JT Cement and concrete research.
DA MAR 01 2000 v 30 n 3
PG 491   
AU Hall, C.   
AU Colston, S. L.   
AU Barnes, P.   
TI Non-destructive tomographic energy-dispersive diffraction imaging of the   
   interior of bulk concrete.   
SI 0008-8846(20000301)30:3L.491:NTED;1-   
AV Article availability and price:                     
$  34.00 Total  =  10.00 Service +  20.00 Copyright +  4.00 Fax Surch.         
>>                 UnCover #:  251,129,151,059          
  
JT Review of scientific instruments.
DA AUG 01 2000 v 71 n 8
PG 3161   
AU Tai, Cheng-Chi   
TI Characterization of coatings on magnetic metal using the swept-frequency   
   eddy current method.   
SI 0034-6748(20000801)71:8L.3161:CCMM;1-   
AV Article availability and price:                     
$  29.00 Total  =  10.00 Service +  15.00 Copyright +  4.00 Fax Surch.         
>>                 UnCover #:  251,129,229,091          
  
JT Surface coatings australia.
DA MAY 01 2000 v 37 n 5
PG 20   
TI Non-destructive measurement of coating adhesion.   
SI 0815-709X(20000501)37:5L.20:NMCA;1-   
AV Article availability and price:                     
 Publisher forbids delivery of this title.                  
>>                 UnCover #:  251,130,027,113          
  
JT Optics letters.
DA AUG 15 2000 v 25 n 16
PG 1189   
AU Ying, Jinpin   
AU Liu, Feng   
AU Alfano, R.R.   
TI Nondestructive evaluation of incipient corrosion in a metal beneath paint by
   second-harmonic tomography.   
SI 0146-9592(20000815)25:16L.1189:NEIC;1-   
AV Article availability and price:                     
$  24.00 Total  =  10.00 Service +  10.00 Copyright +  4.00 Fax Surch.         
>>                 UnCover #:  251,129,243,229          
  
              
------------------------------------------------------------------------------
The REVEAL Alert service is provided by the UnCover Company.  If you    
need further information or assistance, please phone us at              
800.787.7979 (outside the US at 303.758.3030), or send e-mail to        
uncover@carl.org.  Thank you for using REVEAL.                          

|Top|
|List to all TOCs|
|NDTnet |
©copyright NDT.net info@ndt.net