JT Journal of composites for construction.
DA AUG 01 1998 v 2 n 3
PG 126
AU Littles Jr., Jerrol W.
AU Jacobs, Laurence J.
AU Zureick, Abdul-Hamid
TI Ultrasonic Techniques to Characterize Pultruded Composite Members.
AV Article availability and price:
Publisher forbids delivery of this title.
>> UnCover #: 251,098,175,210
JT Sensors and actuators. part a, physical.
DA AUG 15 1998 v 69 n 2
PG 139
AU Hietanen, J.
TI Closed-form formulation for sensitivity of capacitive ultrasonic transducers
using V-grooved backplates.
SI 0924-4247(19980815)69:2L.139:CFSC;1-
AV Article availability and price:
$ 33.00 Total = 10.00 Service + 19.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,098,204,121
JT Composites science and technology.
DA 1998 v 58 n 5
PG 741
AU Audoin, B.
AU Bescond, C.
AU Guilbaud, S.
TI Measurement of stiffness coefficients at elevated temperatures by means of
laser-generated ultrasonic waves.
SI 0266-3538(1998)58:5L.741:MSCE;1-
AV Article availability and price:
$ 33.00 Total = 10.00 Service + 19.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,098,206,245
JT Light metal age.
DA FEB 01 1998 v 56 n 1 / 2
PG 136
AU Hertwich, G.
AU Langgartner
TI Automatic Ultrasonic Testing of Billet and Forging Stock.
SI 0024-3345(19980201)56:1:2L.136:AUTB;1-
AV Article availability and price:
Publisher forbids delivery of this title.
>> UnCover #: 251,098,225,068
JT Journal of food engineering.
DA 1998 v 35 n 3
PG 323
AU Ghaedian, R.
AU Coupland, J.N.
AU McClements, D.J.
TI Ultrasonic Determination of Fish Composition.
SI 0260-8774(1998)35:3L.323:UDFC;1-
AV Article availability and price:
$ 33.00 Total = 10.00 Service + 19.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,041,237
JT Composites. part a, applied science and manufa
DA 1998 v 29 n 7
PG 743
AU Bechtold, G.
AU Gaffney, K.M.
AU Friedrich, K.
TI Fibre orientation in an injection moulded specimen by ultrasonic
backscattering.
SI 1359-835X(1998)29:7L.743:FOIM;1-
AV Article availability and price:
$ 33.00 Total = 10.00 Service + 19.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,123,045
JT Applied physics letters.
DA AUG 10 1998 v 73 n 6
PG 741
AU Degertekin, F. Levent
AU Atalar, Abdullah
AU Khuri-Yakub, Butrus T.
TI Micromachinable ultrasonic leaky wave air transducers.
SI 0003-6951(19980810)73:6L.741:MULA;1-
AV Article availability and price:
$ 29.00 Total = 10.00 Service + 15.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,124,164
JT Ieee transactions on ultrasonics, ferroelectrics
DA JUL 01 1998 v 45 n 4
PG 1006
AU Xiang, D.
AU Hsu,N.N.
AU Blessing, G.V.
TI Statistical Error Analysis of Time and Polarization Resolved Ultrasonic
Measurements.
SI 0885-3010(19980701)45:4L.1006:SEAT;1-
AV Article availability and price:
$ 24.00 Total = 10.00 Service + 10.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,128,052
JT Ieee transactions on ultrasonics, ferroelectrics
DA JUL 01 1998 v 45 n 4
PG 1071
AU Saitoh, S.
AU Kobayashi, T.
AU Yamashita, Y.
TI A 20 MHz Single-Element Ultrasonic Probe Using
0.91Pb(Zn1/3Nb2/3)O3-0.09PbTiO3 Single Crystal.
SI 0885-3010(19980701)45:4L.1071:2MSU;1-
AV Article availability and price:
$ 24.00 Total = 10.00 Service + 10.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,128,069
JT Ieee transactions on ultrasonics, ferroelectrics
DA JUL 01 1998 v 45 n 4
PG 980
AU Lockwood, G.R.
AU Talman, J.R.
AU Brunke, S.S.
TI Real-Time 3-D Ultrasound Imaging Using Sparse Synthetic Aperture
Beamforming.
SI 0885-3010(19980701)45:4L.980:R3UI;1-
AV Article availability and price:
$ 24.00 Total = 10.00 Service + 10.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,128,042
JT Aerospace engineering
DA APR 01 1998 v 18 n 4
PG 14
TI Ultrasound and electromagnetic fields are used in nondestructive inspection
devices.
SU A hand-held nondestructive inspection device offers alternative solutions
for damage detection on aircraft.
SI 0736-2536(19980401)18:4L.14:UEFA;1-
AV Article availability and price:
$ 17.75 Total = 10.00 Service + 3.75 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,099,178,247
JT Journal of manufacturing science and engineering
DA AUG 01 1998 v 120 n 3
PG 600
AU Zhang, S.B.
AU Zhang, Y.M.
AU Kovacevic, R.
TI Noncontact Ultrasonic Sensing for Seam Tracking in Arc Welding Processes.
SI 1087-1357(19980801)120:3L.600:NUSS;1-
AV Article availability and price:
Publisher forbids delivery of this title.
>> UnCover #: 251,100,006,106
JT Sensors and actuators. part a, physical.
DA JUN 30 1998 v 69 n 1
PG 68
AU Gaete-Garreton, L.
AU Hernandez, Y. Vargas
AU Gallego Juarez, J. A.
TI A simple non-linear technique for secondary calibration of ultrasonic
probes.
SI 0924-4247(19980630)69:1L.68:SNTS;1-
AV Article availability and price:
$ 33.00 Total = 10.00 Service + 19.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,100,030,175
JT Journal of microelectromechanical systems.
DA SEP 01 1998 v 7 n 3
PG 295
AU Jin, X.
AU Ladabaum, I.
AU Khuri-Yakub, B.T.
TI The Microfabrication of Capacitive Ultrasonic Transducers.
SI 1057-7157(19980901)7:3L.295:MCUT;1-
AV Article availability and price:
$ 24.00 Total = 10.00 Service + 10.00 Copyright + 4.00 Fax Surch.
>> UnCover #: 251,100,045,088
--------------------------------------------------------------
|Top| |