Subject:
Reveal Alert: ultrasonic ( and ultrasound for selected cases)
JT Composites engineering.
DA 1995 v 5 n 6
PG 675
AU Balasubramaniam, Krishnan
AU Ji, Yuyin
AU Gardner, Steven
TI A study on the influence of fiber-matrix interphase properties on ultrasonic
wave behavior using effective elastic property models.
SI 0961-9526(1995)5:6L.675:SIIAV Article availability and price:
$ 27.50 Total = 8.50 Service + 15.00 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,041,080
JT Composites engineering.
DA 1995 v 5 n 6
PG 697
AU Karpur, Prasanna
AU Matikas, Theodore E.
AU Krishnamurthy, S.
TI Ultrasonic characterization of the fiber-matrix interphase/interface for
mechanics of continuous fiber reinforced metal matrix and ceramic matrix
composites.
SI 0961-9526(1995)5:6L.697:UCIAV Article availability and price:
$ 27.50 Total = 8.50 Service + 15.00 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,041,089
JT Composites engineering.
DA 1995 v 5 n 6
PG 713
AU Rokhlin, S.I.
AU Chu, Y.C.
AU Huang, W.
TI Determination of fiber-matrix interphase elastic moduli from ultrasonic
phase velocity and attenuation data.
SI 0961-9526(1995)5:6L.713:DFIE;1-
AV Article availability and price:
$ 27.50 Total = 8.50 Service + 15.00 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,041,095
JT Composites engineering.
DA 1995 v 5 n 6
PG 735
AU Bashyam, Manohar
TI Ultrasonic technique to measure stiffness coefficients of CMC and its
implications on characterizing material degradation.
SI 0961-9526(1995)5:6L.735:UTMS;1-
AV Article availability and price:
$ 27.50 Total = 8.50 Service + 15.00 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,041,099
JT International journal of thermophysics.
DA JUL 01 1996 v 17 n 4
PG 851
AU Daridon, J. L.
AU Lagourette, B.
AU Labes, P.
TI Compressibilities of Ternary Mixtures Cl-nCl6-CO2 Under Pressure from
Ultrasonic Measurements of Sound Speed.
SI 0195-928X(19960701)17:4L.851:CTMC;1-
AV Article availability and price:
$ 22.00 Total = 8.50 Service + 9.50 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,042,060
JT Journal of physics d: applied physics.
DA JUL 14 1996 v 29 n 7
PG 2015
AU Masi, L.
AU Borchi, E.
AU de Gennaro, S.
TI Porosity behaviour of ultrasonic velocities in polycrystalline Y-V-C-O.
SI 0022-3727(19960714)29:7L.2015:PBUV;1-
AV Article availability and price:
$ 32.25 Total = 8.50 Service + 19.75 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,043,231
JT Polymer engineering and science.
DA JUL 01 1996 v 36 n 13
PG 1832
AU Maffezzoli, A.
AU Luprano, V.A.
AU Nicolais, L.
TI Ultrasonic Wave Attentuation During Water Sorption in Poly(2-Hydroxyethyl
Methacrylate) Hydrogels.
SI 0032-3888(19960701)36:13L.1832:UWAD;1-
AV Article availability and price:
$ 17.75 Total = 8.50 Service + 5.25 Copyright + 4.00 Fax Surch.
>> Profile # UnCover #: 251,068,083,095
--
The REVEAL Alert service is provided by the UnCover Company. If you
need further information or assistance, please phone us at