UTILISATION DES TECHNIQUES ÉMISSION ACOUSTIQUE ET ACOUSTO-ULTRASONS POUR L'ÉVALUATION DE L'ÉTAT D'ENDOMMAGEMENT D'UNE AILE D'AVION EN BOIS
USE OF ACOUSTIC EMISSION AND ACOUSTO-ULTRASONIC TECHNIQUES FOR DAMAGE EVALUATION ON A FULL SCALE WOOD AIRPLANE WINGS

N. Giammei1, A. Proust2 3, D. Marlot13, J. Lenain14, J. Lanvin3 2, L. Brancheriau4 , J. Klinka4
1Euro Physical Acoustics4, Paris [France]
2Euro Physical Acoustics SA4, Sucy-en-Brie [France]
3FCBA2, n.n [France]
4AVIATION CIVILE, n.n [France]
Acoustic Emission (AE), acoustic emission sensor, Inspection, Ultrasonic Testing (UT), shear waves, Visual and Optical Testing (VT/OT), shearography, spectroscopy, spectroscopy, spectroscopy, spectroscopy, spectroscopy, spectroscopy, spectroscopy, spectroscopy, aerospace, wood, elastic properties, crack detection
Click here to enter or to change Keywords
34 views since published or 2010-01-01, click for more details
Emission acoustique2009-01
   

ToDo: Make the search accent-insensitive. Automatically expand the search to find synonyms, plural and spelling variants of search terms.

© NDT.net       Advertising with NDT.net.