Re: Mass Deposition Sensor for Coatings
Posted by: Kyle Reed , E-mail: kreed@microcoating.com, on October 14, 1999 at 14:31:08 :In Reply to: Re: Mass Deposition Sensor for Coatings posted by : Hermann Wüstenberg on October 14, 1999 at 14:00:44:
: If the ambience condition are allowing the use of PVDF foils as a piezoelectric transducer material, their application would give a much higher sensitivity for the change in masses deposited at one of the contacting electrodes.
The temperature of the deposition would be 200 C. Do you know the temperature limit of PVDF foils?
Thank you for the reply