Posted by: faran hussain , E-mail: Address, on May 09, 2008 at 09:57 :Helium Leak Test & Ammonia Leak Tests are two different Tests for sensitive leakage detection. We are thinking of using a mixture of both gases to save time. As recommended soaking time in case of Ammonia is 08 hours and that four Helium is 01 hour. So by mixing the two gases we can attempt Helium Leak test during soaking time of Ammonia. If some one has any expiernec or any apprehensions kindly please share.