Home Forum Technical Discussions

hydrophilic remover

Posted by: diego on May 09, 2008 at 18:05:

hi, I just want to ask regarding the effectiveness of hydrophilic remover, according to military manual once that the part after you remove from hydrophilc remover the emulsification stop but the level 3 said once you remove the part from hydrophilic remover the action never stop, the hydrophilic remover action is dillution not diffusion like lipophilic emusifier, which one is correct?
tnx!