: please provide visual acceptance criteria for porosity in TIG welding
------------ End Original Message ------------Aceeptance Limit for PT/MT in AWS is defined as
CJP Groove welds in butt joints transverse to the direction of computes tensile stress shall have no visible piping porosity.
For all other groove welds and fillet welds, the sum of visible piping porosity 1mm or greater in dia. shall not exceed 10mm in any linear inch of weld and shall not exceed 20mm in any 12in. length of weld.