Mr. Gonulal,
the acceptance criteria are not the same. In A-578 level B there is an additional requirement for interaction of smaller discontinuities. (See ASTM A-578 item 8.2)
regards,----------- Start Original Message -----------
: Dear Specialists,
: ASME SA 435 and SA 578 code requires straigth beam examination of carbon steel plates greater than 12mm. SA 435 and SA 578 Level B hvae the same acceptance criteria.
: If a plate has been inspected in acc. with SA 578 Level B, and the code requires SA 435 inspection. Is there any Code interpretetion or experience with ASME Code work?
------------ End Original Message ------------