Posted by: mustafa GONULAL(PID_3636), E-mail: Address, on June 05, 2008 at 08:28 :
In Reply to: Re: ASME SA 435 vs SA 578 posted by : Manfred Richter
, E-mail: Address, on June 04, 2008 at 18:48 :
----------- Start Original Message -----------
: Mr. Gonulal,
: the acceptance criteria are not the same. In A-578 level B there is an additional requirement for interaction of smaller discontinuities. (See ASTM A-578 item 8.2)
: regards,
: : Dear Specialists,
: : ASME SA 435 and SA 578 code requires straigth beam examination of carbon steel plates greater than 12mm. SA 435 and SA 578 Level B hvae the same acceptance criteria.
: : If a plate has been inspected in acc. with SA 578 Level B, and the code requires SA 435 inspection. Is there any Code interpretetion or experience with ASME Code work?
------------ End Original Message ------------Thanks for response Mr. Richter,
Then we can say that SA578 Level B is more restricted than SA435. So, if the plate is ispected in acc. with SA 578 B, does it need to be checked by SA 435?