That is normally a straightforward measurement for an ultrasonic thickness gage. For best results, use a precision gage with a single element high frequency delay line tranducer (10 or 20 MHz), as opposed to a gage designed for corrosion survey, which will typically not be quite as accurate. I'm attaching a link to an application note on ultrasonic gaging of coiled sheet steel that you may find relevant.

----------- Start Original Message -----------
: Hi, Im seeking the best option for the thickness meaturment of the the sheet metals. could you please any one point me to the variuse type of thickness meaturment methods?
: in this way, I can study them and find the best one for my case
: Best Regards
: Mehdi
------------ End Original Message ------------




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help