Posted by: bobsudharmin(PID_3396), E-mail: Address, on July 28, 2008 at 15:15 :
In Reply to: EN 10160 interpretation posted by : yasin karavacıoğlu , E-mail: Address, on July 18, 2008 at 14:01 :
Isn't the statement clear enough? Defects of size less than 100mm2 is not to be considered. The criteria would be ACCEPT if it does not exceed 15 in nos.
best regards,
bobsudharmin
----------- Start Original Message -----------
: Dear Expert;
: We work on UT test for plate.
: For EN 10160 class S1;
: standard say permisible defect size and number of defects are following :
: Area
: Defect mm² Max. number of defects
: Within 1 m²
: 100 - 1000 15
: My question is if there is 15 defects in this range and also there is some defect that's sizes is lower than 100mm². At this condition this plate is acceptable or not ?
: Thank you
------------ End Original Message ------------
- Re: EN 10160 interpretation Y.Karavacioglu 07:57 Aug-01-2008 (1)
- Re: EN 10160 interpretation bob sudharmin
16:14 Aug-01-2008 (0)
Attention! Please click the button only once. This may take a moment to process
Forum
Technical Discussions
Help