[ NDT-net Forum ]
[ Follow Ups ] [ Post Followup ] [ Help ]
Re: one-sided inspection of multi-layered composite sandwich structure
Posted by: Gary Georgeson , E-mail: gary.e.georgeson@boeing.com, on March 21, 2000 at 18:08 :In Reply to: one-sided inspection of multi-layered composite sandwich structure posted by : Gary Georgeson on March 21, 2000 at 17:49:
: Is anyone aware of any NDE/NDI development in the area of
: one-sided inspection of multi-layered composite sandwich
: structure? Is any research being done? What instruments
: or technologies are being used?: I'm interested in anything that is being done right now
: in this area.: My phone number is 206-662-2161. Or, you can email me back
at gary.e.georgeson@boeing.com: Gary Georgeson, Ph.D
: Sr. Specialist Engineer
: Composites NDE Focal
: Boeing, Seattle
- Re: one-sided inspection of multi-layered composite sandwich structure Ian Munns 12:01 4/03/2000 (3)
- Re: one-sided inspection of multi-layered composite sandwich structure Wolfgang Bisle 14:13 4/25/2000 (2)
- Re: one-sided inspection of multi-layered composite sandwich structure John Newman, Laser Technology Inc. 18:12 5/28/2002 (0)
- Re: one-sided inspection of multi-layered composite sandwich structure Randy Plis 14:37 4/25/2000 (0)