Forum
Technical Discussions
Re: Corrosion Metre
Posted by: Simon Amallraja , E-mail: Address, on August 06, 2008 at 19:26 :In Reply to: Corrosion Metre posted by : Goutam Basu
, E-mail: Address, on August 06, 2008 at 10:03 :
----------- Start Original Message -----------
: Is there any instrument available as CORROSION METRE for checking corrosion in storage tanks etc. If anybody aware please send me the detail.
------------ End Original Message ------------You can use an Ultrasonic Thickness Gage with A Scan display and B Scan mapping facility for your application. There are many manufacturers in the World with above combination.
Contact us, if you need any further details.
Simon
Attention! Please click the button only once. This may take a moment to process
Forum
Technical Discussions
Help