Re: one-sided inspection of multi-layered composite sandwich structure
Posted by: J. Mark Davis(PID_553), E-mail: mkdavis@mindspring.com, on March 23, 2000 at 09:06 :
In Reply to: one-sided inspection of multi-layered composite sandwich structure posted by : Gary Georgeson on March 21, 2000 at 17:49:
Dear Gary,
I have used some time of flight techniques on a vessel in South America. Not
necessarily research, but I was sizing cracks from the head of the vessel
that were 3 feet long and about 75 % through wall. Not a difficult task.
I have train some of the UT personnel at Boeing at your facility in Creeping
waves, Tip Diffraction, etc. I am on the road and I will let you know the
name of the person that I remember.
Sincerely,
J. Mark Davis
---------------
: Is anyone aware of any NDE/NDI development in the area of
: one-sided inspection of multi-layered composite sandwich
: structure? Is any research being done? What instruments
: or technologies are being used?: I'm interested in anything that is being done right now
: in this area.: My phone number is 206-662-2161. Or, you can email me back.
: Gary Georgeson, Ph.D
: Sr. Specialist Engineer
: Composites NDE Focal
: Boeing, Seattle