Re: NDT Inspection of Prestressing Tendon Systems in Pressurized Concrete Containments

Posted by: Gary Woodside , E-mail: gary@gwoodside.fsnet.co.uk, on March 29, 2000 at 10:33 :

In Reply to: NDT Inspection of Prestressing Tendon Systems in Pressurized Concrete Containments posted by : John McCanna on March 28, 2000 at 16:56:

In the UK a 7.5m long 6mm dia videoscope is used for looking at the tendons of prestressed bridge supports in preperation for increasing the weight limit.

Tendons were failing through corrosion as incorrect grouting procedures were leaving the tendons exposed.

Regards

Gary

I am looking for an inspection process to determine cracking, corrosion, etc., of grouted prestressed tendons. The tendons consist of 19 x 0.62 inch diameter strands with access to the ends only.

: Thank you




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL: Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Link Title: is important! Information on my Home Page
Optional Image URL: http://www....gif


Attention! Please click the button only once. This may take a moment to process


[ NDT-net Forum ] [ Help ]