Re: Sizing of ToFD Indications
Posted by: Nigel Armstrong(PID_728), E-mail: Address, on August 29, 2008 at 10:48 :
In Reply to: Sizing of ToFD Indications posted by : Nilesh Pathare , E-mail: Address, on August 29, 2008 at 08:25 :
Nilesh
The proven truth is that TOFD has a much higher Probability Of Detection (POD) than other volumetric methods, e.g. RT or pulse-echo UT. It will easily detect defects which even very high quality RT may not be able to find. As the method relies only on a discontinuities presence (and not its volume or reflectivity) to produce a diffracted signal it is obviously capable of detecting flaws with very little through wall extent (TWE). However ECA derived acceptance criteria should allow for this enhanced detection capability with much greater lengths of low TWE flaws being acceptable than flaws of greater TWE. However it would be inadvisable to use the same acceptance criteria for RT and TOFD!!!
A discernible separation between upper and lower defect tip diffaction signals is needed to accurately size the flaw's TWE. A flaw of very little TWE, such as a threadlike defect or cold lap (lack of inter-run fusion orientatated parallel to the test surface), both practically undetectable by radiography, may not provide clear separation between upper and lower tip diffracted signals and therefore accurate height measurement is unlikely. Additionally, for near-surface flaws the upper tip diffracted signal may be masked by the lateral wave and the poorly-trained technician is often measuring the time duration of the wavetrain of the lower tip diffracted response.
I recommend you read Charlesworth and Temple's excellent book "Enginnering Applications of Ultrasonic TOFD" to gain an appreciation of the benefits and limitations of TOFD.
Hope this helps.
Nigel
----------- Start Original Message -----------
: Dear Members,
: Sizing of Indications found by AUT ToFD is challenging since we are replacing RT with this AUT. In my experience I observed many recordable indications in ToFD images and No indications in RT films for the same location. Thickness of job is 31mm and DWSI shot for RT.
: If we make sizing of defects by taking first white phase and last black phase of ToFd indication it gives more height than actual. So can anyone highlight me with his previous experience regarding the sizing technique.
: Regards,
: Nil
------------ End Original Message ------------
- Re: Sizing of ToFD Indications Nilesh Pathare 09:26 Sep-01-2008 (0)
- Re: Sizing of ToFD Indications mj 09:12 Aug-30-2008 (2)
- Re: Sizing of ToFD Indications Jan Verkooijen
![]()
12:36 Aug-31-2008 (1)
- Re: Sizing of ToFD Indications Ed Ginzel
![]()
01:42 Sep-02-2008 (0)
Attention! Please click the button only once. This may take a moment to process
Forum
Technical Discussions
Help