Re: one-sided inspection of multi-layered composite sandwich structure
Posted by: Galina Pavlenko , E-mail: pgv@votum.md, on March 30, 2000 at 11:41 :In Reply to: one-sided inspection of multi-layered composite sandwich structure posted by : Gary Georgeson on March 21, 2000 at 17:49:
Dear Mr.Georgeson,
Votum JSC (Moldova) designs and manufactures a new portable bond tester "BT-C".
The BT-C is intended for one-sided inspection of various composites and honeycombs.
The BT-C is excellent in detecting of delaminations, disbonds, unbonds, porosities and internal structures violations.
It offers mechanical impedance & resonance testing and C-image reconstructing of structure violations.
Detailed information about BT-C you can find in Internet: www.votum.mdPlease let me know if You require any further information.
Best regards,
Galina Pavlenko
Votum JSC