Re: coercive force

Posted by: Michel Couture Profile (PID_2805), E-mail: Address, on September 05, 2008 at 17:24 :

In Reply to: coercive force posted by : XiangYan , E-mail: Address, on September 05, 2008 at 16:51 :

In one word, YES! The lower the L/D Ratio (Length to Diameter), greater is the Coercive Force required to demagnetise the item. But shape is not the only factor. You also have to take into account such properties as heat treatment and alloying.

Cheerio's
Michel

----------- Start Original Message -----------
: is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?
------------ End Original Message ------------




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help