The coercive force depends on so many micro structural factors that is very unlikely to have the same values for two identically shaped and alloyed samples.
----------- Start Original Message -----------
: is the coercive force depend on the shape ? Provided two samples are made of the same material but different shape, you measure their coercive force could you end up with different results ?