Dear Martin,

I am working on ultrasonic spectral analysis for microstructural characterization. The list of the publications on this subject are as follows:

(1)Anish Kumar et al., "Influence of grain size on ultrasonic specral parameters in AISI type 316 stainless steel" Scripta Materialia, 40(3), 1999, pp. 333-340.
(2)Anish Kumar, T. Jayakumar and Baldev Raj "Ultrasonic specral analysis for microstructural characterizaition of austenitic and ferritic steels" To appear in Philosophical Magazine A, in next issue.
(3)Brown, A.F., "Material Testing by ultrasonic spectroscopy", Ultrasonics, 11,1973, pp 203.
(4) Gericke O.R.,"Ultrasonic Spectroscopy", Research technique in NDT, Ed. R.S. Sharpe, Vol.1, 1970, Acadamic Press, London. pp 31-61.
(5)Fitting, D.W. and Adler, L., 1981, Ultrasonic Spectral Analysis for NDE, Plenum Press, New York.(Book)

For any further information please feel free to contact me at anish@igcar.ernet.in

Anish Kumar
Indira Gandhi Centre for Atomic Research,
Kalpakkam, India.


Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL: Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Link Title: is important! Information on my Home Page
Optional Image URL: http://www....gif


Attention! Please click the button only once. This may take a moment to process


[ NDT-net Forum ] [ Help ]