[ NDT-net Forum ]
[ Follow Ups ] [ Post Followup ] [ Help ]
Re: Epoxy-filled EDM Notches for MT
Posted by: Dent McIntyre(PID_125), E-mail: mcintyrj@pgg.mcdermott.com, on April 05, 2000 at 18:28 :
In Reply to: Epoxy-filled EDM Notches for MT posted by : Phil Herman Jr. on April 03, 2000 at 20:45:
: PH Tool manufactures NDT Reference Standards and Test Blocks. We have a need for epoxy-filling of narrow (0.001" to 0.005" wide) EDM notches in Mag Particle standards in order to prevent mechanical holding of the indicating medium. We are searching for an epoxy that does NOT naturally flouresce under a blacklight. Does anyone have a suggestion for such an epoxy?
Why are you stuck on Epoxy? Why not fill it with solder or brazing rod?
- Re: Epoxy-filled EDM Notches for MT Phil Herman Jr. 22:11 4/05/2000 (0)