Dear Forum:
I am working on ultrasonic spectral analysis for the detection of hydrogen damages (HIC and/or SOHIC) and I haven“t found too much literatura on this subject. Can somebody help me giving me names or leads of literature on this issue? Also, if someone has some experience, I would appreciate any comment or suggestion on how to help me with this.
Thanks in advance
Eng. Raśl Navarrete
Universidad Central de Venezuela.