The reason it shows up on the film dark is from scatter between the "B" itself and the film.
----------- Start Original Message -----------
: Hi,
: How does a letter B appears black in RT film, when it is placed at the back of film ?
: I find some procedures mentioning,
: "If a dark image "B" appears on a lighter background then this is not a cause for rejection"
: thanks for replies,
:
: Suresh
------------ End Original Message ------------