What is the reference sensitivity required for 0° probe, when testing the fusion zone (and weld) of Full Penetration Joints from main member side?

Whether Lamination test sensitivity (2nd back wall echo at 80% etc) is acceptable or we need to make a DAC using SDH? Consider the following codes:

Case 1: According to ABS Guide
Case 2: According to AWS D1.1
Case 3: According to API RP 2X




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help