In Reply to: Elastic Modulus posted by : Anish Kumar on April 05, 2000 at 08:19: Re: Elastic Modulus
Posted by: mahmoodnajafi on April 24, 2000 at 09:10:
: I am working on microstructural characterization in metallic materials, such as ferritic steels, Inconel 625 superalloy etc., using ultrasonic measurements. Quite often, I need the elastic modulus values of various types of precipitates for uderstanding the change in ultraosnic velocity with precipitation, such as M23C6, Cr2N, and Fe2Mo (Laves phase) in steels and gamma prime, gamma double prime, delta and Ni2Mo type of precipitates in Superalloys. Is there some publication or record where I can get these values, or if some body can supply these values i will be very much thankful to him.: Thanking You.
: Anish Kumar