Posted by: NEELA , E-mail: Address, on October 30, 2008 at 06:13 :In Reply to: Re: UT for below 8mm thk posted by : JK , E-mail: Address, on October 29, 2008 at 18:09 :
Dear J.K.
Please mention the code ,It will help forum member to discuss further
Thanks
----------- Start Original Message -----------
: Hi,
: Though there are some codes which allow UT to be carried out above 6 mm.
: Using a 4Mhz transducer(8x9 mm) preferebly 70,80 degree krautkrammer probes & increasing the skip to 1-2 skip .
: The best way to do is take a mock-up peice of the thickness of the weld you are going to test . A notch on the root and on the crown of the weld would be used as reference.
: Anything more on this please contact me
: Regards
: J.K
------------ End Original Message ------------