Home Forum Technical Discussions     

Re: UT for below 8mm thk

Posted by: chris s Profile (PID_3032), E-mail: Address, on November 04, 2008 at 18:08 :

In Reply to: UT for below 8mm thk posted by : gowri santhosh Profile , E-mail: Address, on October 25, 2008 at 14:03 :

----------- Start Original Message -----------
: hi, this is santhosh
: please tell me about UT for below 8mm thickness with reference code. thanks for reply.
------------ End Original Message ------------

I would suggest that you contact a level III who is knowledgeable in regards to phased array, make appropriate mock-ups and test your techs accordingly


Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help