Posted by: S.V.Swamy(PID_839), E-mail: Address, on November 25, 2008 at 10:21 :
In Reply to: Re: ASTM A578 posted by : Theo Micottis , E-mail: Address, on November 24, 2008 at 22:27 :
Theo,
That test was meant to know whether you can catch the mistake! Don't assume that the given procedure is correct. As a level III, you are supposed to correct and contest another level III if needed.
I did not respond earlier because I don't have ready access to the specification but my analysis was same as Nigel's (and I acknowledged that separately to him a few hours ago). I felt inspired to comment on this from a Trainer's perspective.
Best wishes for the future.
Swamy
NDT Guru (Trainer)----------- Start Original Message -----------
: Thank you very much Nigel. In reality this was my task in the exam for the third level UT. They gave me this standard for the unbond test and I really didn't think they gave me a wrong specification or at least with some deviations.I read S7.1 and I was quite sure of my choice. Well I failed my exam it will be better next time.You have been very useful.
: Thank you very much
: THEO
------------ End Original Message ------------
- Re: ASTM A578 Theo Micottis 19:22 Nov-25-2008 (0)
- Re: ASTM A578 Michel Couture
17:54 Nov-25-2008 (0)