Posted by: Shibu T James , E-mail: Address, on December 04, 2008 at 11:58 :Up to what thickness (minimum & maximum) we can perform normal beam U T scanning (thickness check) on stainless steel pipe? Please mention the code also.
Regards,
Shibu T James
- Re: UT scanning Tom Nelligan
![]()