1)why cant we use angled longitudinal beam for inspection as it has higehr velocity? can we able to produce angled longitudinal beam?
2) in TOFD we use angled Longitudianl beam? so i think we can get angled longitudinal beam.
3)mode conversion start in material or wedge?????????
- Re: mode conversion Ed Ginzel
![]()