[ NDT-net Forum ]
[ Follow Ups ] [ Post Followup ] [ Help ]
Re: Railway
Posted by: David Hermanutz , E-mail: panaptyndtvic@bigpond.com, on June 15, 2000 at 17:14 :In Reply to: Railway posted by : Ignacio Fraile on June 13, 2000 at 21:19:
: Esteemed colleagues:
: I’m looking for information about methods and/or standards related to the U T inspection of Railwaysrails
: I’ll welcome any recommendation or advice.
: Kind regards.: Ignacio Fraile
for a start tryhttp://www.cnde.iastate.edu/ncce/UT_CC/Sec.6.1/Sec.6.1.html
The rail industry is quite a huge concern with a lot of manufacturing testing going on throughout the world. There are currently systems worth close to a million dollars and $600 dollar D-meters. Please give us a little more detail as to what end of the industry you are involved in...
- Re: Railway Mike Bentley 13:03 8/03/2000 (0)
- Re: Railway Mike Bentley 13:01 8/03/2000 (0)
- Re: Railway Mike Bentley 12:58 8/03/2000 (0)