Posted by: MEHDY , E-mail: Address, on December 24, 2008 at 22:50 :In Reply to: Re: Aws d1.1 UT Indication rate posted by : Ed T. , E-mail: Address, on December 21, 2008 at 04:14 :
----------- Start Original Message -----------
: : may you tell how to define "b" of a-b-c=d of UT indication rate in AWS D1.1? Thanks.
: b is your dB level at reference. In other words when you set your 0.060" diameter hole in the IIW block to say 80% FSH and your dB level is 50dB, then 50 becomes b.
------------ End Original Message ------------