Posted by: Justin Lehmann Profile (PID_3162), E-mail: Address, on January 06, 2009 at 23:31 :

In Reply to: Re: PT dwell time variations in reference to temperature extremes posted by : Michel Couture Profile , E-mail: Address, on December 27, 2008 at 19:59 :

Jim,

Take a look at ASTM E-1417. It states "The component,
penetrant, and ambient temperatures shall all be in the range from 40 to 125°F [4 to 52°C] unless otherwise specified." It goes on, "The dwell time, unless otherwise specified, shall be a minimum of 10 min. For temperatures between 40 and 50°F [4.4 and 10°C], dwell time shall be a minimum of 20 min."
The ASTM does not address temperatures outside of these ranges.

Justin Lehmann
Manager - Training and Consulting Services
Quality Testing Services, Inc
2305 Millpark Dr
St. Louis, MO 63043
314-770-0607
314-770-0103 fax
314-575-7485 cell
jcl@qualitytesting.net

----------- Start Original Message -----------
: Hi Jim,
: I totally agree with Swamy. Even more I do remember 20 years ago when I got into NDT and dealing mostly with Military Standard that we (in the Canadian Air Force) used MIL-I-6868 to select the penetrant and developer that was compatible with the job we had to do. I do know if it still exist today or if it has been superseded by another code. But, in the end, if you consult the manufacturer's spec. for a product and stay within the temperature range of the code your working to, you shouldn't have any problem. Remember keep it simple and don't try to reinvent the wheel. Many people have spent countless hours to come up with with is already establish and it work.
: Cheerio's
: Michel
: : What is vague about them? And the manufacturers provide enough literature, if needed. If the temperature is too low, viscosity will be too high and penetration will not take place properly. If the temperature is too high, the penetrant will dry out and will again not penetrate. If in doubt, use test coupons at the same temperature and see whether you are able to pick up the needed indications.
: : Swamy
: : NDT Guru
: : Hyderabad, India
: : : Does anybody have....... or know where i can find.... a table outlining penetrant and developer dwell times with regards to temperature? I know certain codes and standards provide guidelines but I'm looking for something less vague.
------------ End Original Message ------------




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help