AEA Sonomatic BV has been working in this area for over
a decade now and has build up a vast reference in this
application. Procedures were validated with clients and
Authorised Inspection bodies such as Stoomwezen (1992)
and TueV Nord (1999). Procedures are based upon research
of established research institutes and our own research
and practical experiences.
An article describing this in some more detail can be found
on this site under:
www.ndt.net/article/ecndt98/chemical/105/105.htm
a product descriptor can be found under
http://www.aeat.co.uk/energy/prdsrv/inspect/fldser/hha.htm
Please do not hesitate to contact me
if you require any more information.Jan Verkooijen