PT Marker
Posted by: Andrea Steen(PID_428), E-mail: andrea.m.steen@allison.com, on June 27, 2000 at 20:52 :
Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulpher? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.
Andrea Steen
NDT Engineer/Level III
Rolls-Royce Corporation
- Re: PT Marker Andrea Steen 16:17 6/28/2000 (3)
- Re: PT Marker Dent McIntyre 16:29 6/28/2000 (2)
- Re: PT Marker Thomas Murphy 23:10 7/25/2000 (1)
- Re: PT Marker dave ronson 17:16 11/06/2000 (0)